journal article·2003-09

Mechanical tensile promotion and superconducting properties of highly Pb-content HTc-BPSCCO superconductor

Morsy M.A. Sekkina, Khaled M. Elsabawy

Publisher page

Abstract

Abstract The samples of the general formula (Bi0.8Pb0.2+x)2Sr2Ca2Cu3O10, where 0.0≤x≤0.3 mol% were prepared by the conventional high temperature solid state reaction technique. The extra lead (x) was added as very fine powder of pure Pb-metal with particle size ≤50 μm. The superconducting measurements for HTc-2223-phase proved that, best Tc=109 K is for the sample with x=0.2 (Pb-content=0.4 mol%) while the lowest Tc=98 K is for the sample with x=0.3 mol%. The evaluated crystalline lattice structure of the prepared samples mainly belongs to the superconductive tetragonal phase (2223), besides secondary (2201) and (2212) phases in minor. The c-axis lattice parameter exhibits length elongation as x (Pb-content) increases from x=0.1 to 0.3. The maximum mechanical tensile strength values at 295 K were promoted and found to be 37.5, 38.6 and 41.4 MPa as Pb-content increases from x=0.1 to 0.3, respectively.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Physics of Superconductivity and Magnetism · Superconducting Materials and Applications · Magnetic Properties and Applications

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (30)

Show source-provided references
1. Wong · J. Am. Ceram. Soc. · 1994 · 77 · 283310.1111/j.1151-2916.1994.tb04512.x ↗
2. Bobrov · 1989 · 247
3. Alford · Supercond. Sci. Technol. · 1990 · 3 · 110.1088/0953-2048/3/1/002 ↗
4. Chan · Supercond. Sci. Technol. · 1991 · 413 · 20
5. Miyase · Supercond. Sci. Technol. · 1995 · 8 · 62610.1088/0953-2048/8/8/005 ↗
6. Niu · Jpn. J. Appl. Phys. · 1988 · 27 · L144210.1143/JJAP.27.L1442 ↗
7. Morris · Phys. Rev. · 1989 · B39 · 661210.1103/PhysRevB.39.6612 ↗
8. Zhao · Physica C · 1989 · 159 · 63910.1016/0921-4534(89)91297-5 ↗
9. Presland · Physica C · 1990 · 176 · 9510.1016/0921-4534(91)90700-9 ↗
10. Kao · Physca C · 1993 · 177 · 376
11. Miehe · Physica C · 1990 · 171 · 33910.1016/0921-4534(90)90150-D ↗
12. Tarascon · Phys. Rev. · 1988 · B38 · 885
13. Chudnovsky · Phys. Rev. Lett. · 1990 · 65 · 306010.1103/PhysRevLett.65.3060 ↗
14. Hazen · Phys. Rev. Lett. · 1988 · 60 · 117410.1103/PhysRevLett.60.1174 ↗
15. Zandbergen · Physica C · 1988 · 156 · 32510.1016/0921-4534(88)90756-3 ↗
16. Petrick · Phys. Rev. · 1990 · B42 · 38710.1103/PhysRevB.42.387 ↗
17. Han · Supercond. Sci. Technol. · 1997 · 10 · 37110.1088/0953-2048/10/6/001 ↗
18. Welp · Nature (London) · 1996 · 276 · 44
19. Primo · Solid State Ionics · 1993 · 63–65 · 87210.1016/0167-2738(93)90209-L ↗
20. Zhengping · J. Supercond. · 1990 · 42110.1007/BF00617470 ↗
21. Tomita · Supercond. Sci. Technol. · 2000 · 13 · 72210.1088/0953-2048/13/6/318 ↗
22. Hong · J. Am. Ceram. Soc. · 1991 · 74 · 14510.1111/j.1151-2916.1991.tb04341.x ↗
23. Pandey · Physica C · 1995 · 241 · 27910.1016/0921-4534(94)02383-2 ↗
24. Sastry · Physica C · 1994 · 235–240 · 50310.1016/0921-4534(94)91475-3 ↗
25. Tomita · Supercond. Sci. Technol. · 2001 · 15 · 932
26. Wu · Jpn. J. Appl. Phys. · 1998 · 37 · L43810.1143/JJAP.37.L438 ↗
27. Ikeda · Jpn. J. Appl. Phys. · 1998 · 27 · L206710.1143/JJAP.27.L2067 ↗
28. Ikeda · Physica C · 1991 · 190 · 1810.1016/S0921-4534(05)80186-8 ↗
29. Sung · Physica C · 1995 · 252 · 15510.1016/0921-4534(95)00341-X ↗
30. Azzouz · Physica C · 2001 · 356 · 8310.1016/S0921-4534(01)00124-1 ↗