Characteristics of F doped PZT ceramics using different fluorine sources
Source abstract
Abstract
Abstract In this study, some structural and electrical properties of a PZT base composition Pb 0.89 (Ba, Sr) 0.11 (Zr 0.52 Ti 0.48 )O 3 co-doped with 1 mol% manganese and 2 mol% fluorine have been studied. Two different fluorine sources were used: lead fluoride PbF 2 and manganese fluoride MnF 2 . These fluoride salts are added to the co-precipitated precursors powder. Mn dopant was added to the solution as manganese acetate (MnAc) before co-precipitation, when PbF 2 was used. The structural analysis of the sintered ceramics revealed that MnF 2 doping makes the volume of the cubic unit cell ( V c ) and the grain size decrease, whereas (MnAc, PbF 2 ) co-doping makes the apparent density increase and keeps the average grain size and V c unchanged. Both types of doping reagents largely enhance the piezoelectric activity (high d 33 and k 33 coefficients, well saturated Polarization–Electric field loops) but MnF 2 induces both combinatory soft and hard characteristics compared to (MnAc, PbF 2 ) co-doping. Impedance spectroscopy showed that both types of doping reagents strongly reduce the electrical conductivity with the same conducting species, i.e. the same defect chemistry, confirmed by optical absorption data. Finally, this study shows that in the semi-wet process used, PbF 2 is added homogeneously to the co-precipitated powder. Whatever the fluorine source, only the coexistence of Mn and F dopants is necessary to improve the piezoelectric response.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Ferroelectric and Piezoelectric Materials · Acoustic Wave Resonator Technologies · Microwave Dielectric Ceramics Synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (20)
Show source-provided references
1. Berlincourt · J. Acoust. Soc. Am. · 1992 · 91 · 303410.1121/1.402938 ↗
2. Guiffard · J. Appl. Phys. · 1999 · 86 · 574710.1063/1.371588 ↗
3. Boucher · J. Appl. Phys. · 2002 · 92 · 543710.1063/1.1499526 ↗
4. Guiffard · Ferroelectrics · 2004 · 313 · 13510.1080/00150190490903856 ↗
5. Eyraud · Ferroelectrics · 2002 · 265 · 30310.1080/00150190208260631 ↗
6. Boucher · Jpn. J. Appl. Phys. · 2004 · 43 · 537810.1143/JJAP.43.5378 ↗
7. Gao · Jpn. J. Appl. Phys. · 2001 · 40 · 68710.1143/JJAP.40.687 ↗
8. Zhang · Mater. Lett. · 2005 · 59 · 347110.1016/j.matlet.2005.06.016 ↗
9. L. Eyraud, P. Eyraud, F. Eyraud, D. Audigier, M. Boisrayon, U.S. Patent 5,683,613, November (1997).
10. Guiffard · Mater. Res. Bull. · 1998 · 33 · 175910.1016/S0025-5408(98)00189-5 ↗
11. Sinclair · Int. Ceram. · 2000 · 2 · 33
12. Izaki · Jpn. J. Appl. Phys. · 1992 · 31 · 304510.1143/JJAP.31.3045 ↗
13. Chiang · Ceram. Bull. · 1981 · 60 · 484
14. Ohtaka · J. Am. Ceram. Soc. · 1995 · 78 · 80510.1111/j.1151-2916.1995.tb08251.x ↗
15. Carl · Ferroelectrics · 1978 · 17 · 47310.1080/00150197808236770 ↗
16. Kamiya · Jpn. J. Appl. Phys. · 1992 · 31 · 305810.1143/JJAP.31.3058 ↗
17. Zuo · Mater. Lett. · 2002 · 54 · 18510.1016/S0167-577X(01)00561-4 ↗
18. Raymond · J. Phys. Chem. Solids · 1996 · 57 · 150710.1016/0022-3697(96)00020-0 ↗
19. Guiffard · J. Eur. Ceram. Soc. · 2005 · 25 · 248710.1016/j.jeurceramsoc.2005.03.087 ↗
20. Ang · Phys. Rev. B · 2000 · 62 · 22810.1103/PhysRevB.62.228 ↗