journal article·2005-04

Preparation of La0.5Sr0.5CoO3 powders and thin film from a new aqueous solution–gel precursor

J. Pagnaer, A. Hardy, D. Mondelaers, G. Vanhoyland, J. D’Haen, M.K. Van Bael, H. Van den Rul, J. Mullens, L.C. Van Poucke

Materials Science and Engineering: B· Volume 118· Issue 1-3
Publisher page

Abstract

Abstract This paper reports on the spin deposition of LSCO thin films on a SiO 2 /Si substrate by a new aqueous solution–gel route. Stable and monometallic precursor solutions are prepared from common and inexpensive oxides or hydroxides. The aqueous La 3+ precursor is synthesized by reaction of La 2 O 3 with citric acid. In order to prepare an aqueous Sr 2+ precursor Sr(OH) 2 is complexed by EDTA. The new peroxo citrato Co 2+ precursor is synthesized by reaction of Co(OH) 2 with hydrogen peroxide in an aqueous solution of citric acid. Mixing the individual precursors in stoichiometric quantities results in a clear and stable aqueous LSCO precursor solution. Evaporation of water transforms this solution in an amorphous gel that is homogeneous down to nanometer scale. In situ high temperature X-ray diffraction analysis of the gel reveals that phase pure LSCO powder is formed at 550 °C without detection of any intermediate crystalline phase. Spin deposition and crystallization at 625 °C in pure O 2 of this aqueous precursor solution resulted in a phase pure conductive LSCO thin film. The sheet resistance of this thin film amounted to 235 Ω/sq. Since the thickness of the film is 120 nm, the specific resistivity was calculated to be 2.8 mΩ cm at room temperature.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Ferroelectric and Piezoelectric Materials · Magnetic and transport properties of perovskites and related materials · Electronic and Structural Properties of Oxides

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (19)

Show source-provided references
1. Liu · J. Mater. Sci. · 1997 · 32 · 20310.1023/A:1018508123039 ↗
2. Chen · Solid State Ionics · 1997 · 98 · 710.1016/S0167-2738(97)00097-0 ↗
3. Goodenough · J. Appl. Phys. · 1963 · 36 · 103110.1063/1.1714087 ↗
4. Javoric · Int. Ferroelectr. · 2000 · 30 · 30910.1080/10584580008222280 ↗
5. Aggarwal · J. Appl. Phys. · 1998 · 83 · 161710.1063/1.366874 ↗
6. Cheung · J. Appl. Phys. Lett. · 1993 · 62 · 204510.1063/1.109474 ↗
7. Ramesh · Mater. Sci. Eng. R · 2001 · 32 · 19110.1016/S0927-796X(00)00032-2 ↗
8. van Doorn · J. Mater. Chem. · 1998 · 8 · 210910.1039/a800500a ↗
9. Narendar · Catal. Today · 1997 · 35 · 24710.1016/S0920-5861(96)00160-5 ↗
10. Hardy · J. Sol–gel Sci. Technol. · 2003 · 26 · 110310.1023/A:1020762824990 ↗
11. Hardy · J. Eur. Ceram. Soc. · 2004 · 24 · 90510.1016/S0955-2219(03)00420-5 ↗
12. Storms · Key Eng. Mater · 2004 · 264 · 34710.4028/www.scientific.net/KEM.264-268.347 ↗
13. Van Werde · J. Mater. Chem. · 2001 · 11 · 119210.1039/b100209k ↗
14. Van Bael · Int. Ferroelectr. · 2002 · 45 · 20510.1080/10584580215366 ↗
15. Nelis · J. Eur. Ceram. Soc. · 2001 · 21 · 204710.1016/S0955-2219(01)00169-8 ↗
16. Pagnaer · J. Eur. Ceram. Soc. · 2004 · 24 · 91910.1016/S0955-2219(03)00392-3 ↗
17. Hardy · Thermochim. Acta · 2003 · 397 · 14310.1016/S0040-6031(02)00272-1 ↗
18. Closset · Powder Diffr. · 1996 · 1110.1017/S0885715600008873 ↗
19. Wu · J. Phys. D: Appl. Phys. · 2001 · 34 · 158710.1088/0022-3727/34/11/305 ↗