Optimization of sintering conditions on the Bi-2223 formation and grain size
Source abstract
Abstract
Phases equilibrium between Bi-2201, Bi-2212 and Bi-2223 phases has been established depending on the sintering time and the sintering temperature. Starting with calcined powder (820°C/24 h), optimization of sintering conditions (temperature, time and intermediate milling) has been achieved. Three sintering steps are necessary to obtain high Bi-2223 phase content. The sintering conditions can be described as follows: 100 h at 850°C, first intermediate milling, 25 h at 850°C, second intermediate milling and 25 h at 835°C. The final Bi-2223 phase content reaches 93% with a resulting grain size between 2 and 3 μm.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Physics of Superconductivity and Magnetism · X-ray Diffraction in Crystallography · Superconducting Materials and Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (10)
Show source-provided references
1. Heine · Appl. Phys. Lett. · 1989 · 55 · 244110.1063/1.102295 ↗
2. Seino · Jpn. J. Appl. Phys. · 1989 · 28 · L7810.1143/JJAP.28.L78 ↗
3. Tampieri · J. Mater. Sci. · 1999 · 34 · 617710.1023/A:1004786324179 ↗
4. Maeda · Jpn. J. Appl. Phys. · 1988 · 27 · L20910.1143/JJAP.27.L209 ↗
5. Rouessac · Physica C · 1997 · 282–287 · 51110.1016/S0921-4534(97)00374-2 ↗
6. J. Mater.
7. Garnier · Supercond. Sci. Technol. · 2000 · 13 · 60210.1088/0953-2048/13/5/333 ↗
8. Schmahl · Supercond. Sci. Technol. · 1998 · 11 · 126910.1088/0953-2048/11/11/013 ↗
9. Strobel · J. Less-Common Met. · 1990 · 164–165 · 51910.1016/0022-5088(90)90255-I ↗
10. Chen · J. Am. Ceram. Soc. · 1992 · 75 · 115010.1111/j.1151-2916.1992.tb05552.x ↗