Bridgman growth of twin-free ZnSe single crystals
Source abstract
Abstract
Abstract In order to grow a large twin-free ZnSe single crystal, we have adopted a closed double-crucible to prevent the deviation from the stoichiometric compositions of the melt during Bridgman growth and determined the optimum growth conditions. They contain a special temperature program, an over-heating temperature of 76 K from the melting point of 1797 K, and the temperature gradient at the growth interface of 30 K cm −1 and a growth rate of 3.6 mm h −1 determined in previous paper. Under these growth conditions, we have successfully grown twin-free high-quality ZnSe single crystals using a polycrystalline seed. Chemical etching on the cleaved (110) plane has shown that the average value of etch pit density (EPD) is about 2.0×10 5 cm −2 . The rocking curves of 4-crystal X-ray diffraction have shown the 19 arcsec in full-width at half-maximum (FWHM). The photoluminescence (PL) spectra at 4.2 K have shown the resolved intensive free exciton, bound exciton emission lines and the weak DAP emission bands. The FWHM of I 1 d emission was less than 0.5 meV. However, the deep-level emission bands were hardly observed. Above all, the results suggest that the ZnSe single crystals grown by the present method are of a very high quality.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Chalcogenide Semiconductor Thin Films · Quantum Dots Synthesis And Properties · Perovskite Materials and Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (21)
Show source-provided references
1. Guha · Appl. Phys. Lett. · 1993 · 63 · 310710.1063/1.110218 ↗
2. Yodo · J. Cryst. Growth · 1988 · 92 · 19610.1016/0022-0248(88)90450-2 ↗
3. Ohno · J. Cryst. Growth · 1998 · 184/185 · 550
4. Cantwell · J. Appl. Phys. · 1992 · 71 · 293110.1063/1.351026 ↗
5. Terashima · J. Crystal Growth · 1990 · 102 · 38710.1016/0022-0248(90)90395-2 ↗
6. Tsujimoto · Jpn. J. Appl. Phys. · 1966 · 5 · 63610.1143/JJAP.5.636 ↗
7. Kimura · J. Crystal Growth · 1973 · 20 · 28310.1016/0022-0248(73)90092-4 ↗
8. Fukuda · J. Crystal Growth · 1996 · 161 · 4510.1016/0022-0248(95)00610-9 ↗
9. Kikuma · J. Crystal Growth · 1985 · 71 · 13610.1016/0022-0248(85)90053-3 ↗
10. Kulakov · Soviet Phys. Solid State · 1976 · 18 · 526
11. Rudolph · Jpn. J. Appl. Phys. · 1994 · 33 · 199110.1143/JJAP.33.1991 ↗
12. Wang · J. Crystal Growth · 2000 · 214/215 · 87510.1016/S0022-0248(00)00219-0 ↗
13. Rudolph · Mater. Sci. Eng. R · 1995 · 15 · 8510.1016/0927-796X(95)00182-4 ↗
14. Omino · J. Crystal Growth · 1992 · 117 · 8010.1016/0022-0248(92)90720-4 ↗
15. Kikuma · Jpn. J. Appl. Phys. · 1991 · 30 · 271810.1143/JJAP.30.2718 ↗
16. Tiller · Acta Metallurg. · 1953 · 1 · 42810.1016/0001-6160(53)90126-6 ↗
17. Holton · J. Crystal Growth · 1969 · 6 · 9710.1016/0022-0248(69)90099-2 ↗
18. Kikuma · J. Crystal Growth · 1978 · 44 · 46710.1016/0022-0248(78)90012-X ↗
19. Yoshida · J. Crystal Growth · 1992 · 117 · 7510.1016/0022-0248(92)90719-Y ↗
20. Shone · J. Crystal Growth · 1988 · 86 · 13210.1016/0022-0248(90)90710-3 ↗
21. Korostelin · J. Crystal Growth · 1999 · 197 · 44910.1016/S0022-0248(98)00742-8 ↗