journal article·2008-01

Energy level diagram for lanthanide-doped lanthanum orthovanadate

Andreas H. Krumpel, Erik van der Kolk, Pieter Dorenbos, Philippe Boutinaud, Enrico Cavalli, Marco Bettinelli

Materials Science and Engineering: B· Volume 146· Issue 1-3
Publisher page

Abstract

Abstract Based on temperature dependent photoconductivity, excitation, and emission measurements we have established the absolute location of 4f energy levels of Pr 3+ , Eu 2+ and Tb 3+ doped in LaVO 4 . In combination with an empirical model describing a systematic and material independent variation of the 4f ground states of tri- and divalent lanthanides this information was used to predict the corresponding absolute energy level positions of all the other lanthanides in the same compound. The results of our work are presented in a complete energy level diagram for LaVO 4 :Ln (Ln = La, Ce, Pr, …, Lu).
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Luminescence Properties of Advanced Materials · Glass properties and applications · Crystal Structures and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (12)

Show source-provided references
1. Zhang · J. Cryst. Growth · 2004 · 260 · 46010.1016/j.jcrysgro.2003.08.067 ↗
2. Liu · Appl. Phys. Lett. · 2006 · 88
3. Yu · Appl. Phys. A: Mater. Sci. Proc. · 2005 · 80
4. Boutinaud · Chem. Phys. Lett. · 2005 · 418
5. Boutinaud · Spectr. Lett. · 2007 · 4010.1080/00387010701247019 ↗
6. Dorenbos · J. Phys.: Condens. Matter · 2003 · 15
7. Dorenbos · J. Luminsc. · 2004 · 108
8. Dorenbos · Appl. Phys. Lett. · 2006 · 8910.1063/1.2336716 ↗
9. van der Kolk · Chem. Mater. · 2006 · 18 · 345810.1021/cm060775s ↗
10. van der Kolk · Appl. Phys. Lett. · 2003 · 83 · 174010.1063/1.1603337 ↗
11. Polosan · Phys. Status Solidi C · 2007 · 410.1002/pssc.200673749 ↗
12. PC measurements were done in a similar way as reported earlier [10]: the electrical contacts evaporated on two opposing faces of the same crystal were made of gold with a thickness of 30nm or rather 6nm where transparency was needed. The contact configuration was in such a way that the light was hitting the transparent part of the top contact therefore producing free charge carriers across the entire crystal. The excitation source was a 450W xenon lamp (FL-1039) and the photocurrent was detected with an electrometer (EM, model 6517A, Keithley). The stabilized voltage supply of this electrometer was also used for applying 1000V across the opposing electrodes. Again the spectra were corrected for the background (including dark current) and the xenon-lamp spectrum.