Effect of post-annealing treatments on the properties of Zn1−xCdxO films on glass substrates
Source abstract
Abstract
Abstract Ternary Zn 1− x Cd x O (0≤ x ≤0.53) alloy crystalline films with highly (0 0 2)-preferred orientations have been prepared on glass substrates by using the dc reactive magnetron sputtering method and exposed to annealing treatments in O 2 ambient. The crystal quality of the annealed Zn 1− x Cd x O films improves much. As a case of the sample with x =0.53, the diffraction peaks in intensity attain maximum values at the annealing temperature of 500 °C. But for the samples with x ≥0.53, the CdO phase separation and re-evaporation from the films are very serious. So for the Zn 1− x Cd x O films with higher Cd content, to prevent the segregation of CdO, the annealing temperature should be less than 400 °C, and the annealing time should be less than 1 h.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: ZnO doping and properties · Copper-based nanomaterials and applications · Gas Sensing Nanomaterials and Sensors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (20)
Show source-provided references
1. Makino · Appl. Phys. Lett. · 2001 · 78 · 123710.1063/1.1350632 ↗
2. Narayan · J. Appl. Phys. · 1998 · 84 · 259710.1063/1.368440 ↗
3. Ohtomo · Mater. Sci. Eng. · 1998 · B56 · 26310.1016/S0921-5107(98)00218-9 ↗
4. Kim · Thin Solid Films · 2000 · 377–378 · 79810.1016/S0040-6090(00)01290-6 ↗
5. Suramanyam · Opt. Mater. · 1999 · 13 · 23910.1016/S0925-3467(99)00070-1 ↗
6. Yan · Phys. Rev. Lett. · 2001 · 86 · 572310.1103/PhysRevLett.86.5723 ↗
7. Ohtomo · Appl. Phys. Lett. · 1998 · 72 · 246610.1063/1.121384 ↗
8. Ma · Chin. Phys. Lett. · 2003 · 20 · 94210.1088/0256-307X/20/6/347 ↗
9. Jin · Solid State Commun. · 2001 · 119 · 40910.1016/S0038-1098(01)00244-7 ↗
10. Zhao · J. Cryst. Growth · 2002 · 234 · 42710.1016/S0022-0248(01)01698-0 ↗
11. Choi · Thin Solid Films · 1996 · 289 · 15310.1016/S0040-6090(96)08923-7 ↗
12. Vigil · Thin Solid Films · 2000 · 361–362 · 5310.1016/S0040-6090(99)01061-5 ↗
13. Tabet-Derraz · Solar Energy Mater. Solar Cells · 2002 · 73 · 24910.1016/S0927-0248(01)00134-9 ↗
14. Sakurai · J. Cryst. Growth · 2002 · 237–239 · 51410.1016/S0022-0248(01)01954-6 ↗
15. Makino · Appl. Phys. Lett. · 2001 · 78 · 123710.1063/1.1350632 ↗
16. Yin · J. Cryst. Growth · 2000 · 220 · 28110.1016/S0022-0248(00)00861-7 ↗
17. Carballeda-Galicia · Thin Solid Films · 2000 · 371 · 10510.1016/S0040-6090(00)00987-1 ↗
18. Vigil · Mater. Chem. Phys. · 2001 · 68 · 24910.1016/S0254-0584(00)00358-8 ↗
19. Srikant · J. Appl. Phys. · 1997 · 81 · 635710.1063/1.364393 ↗
20. Ueda · J. Appl. Phys. · 1998 · 84 · 617410.1063/1.368933 ↗