XANES and XRR study on phase evolution of TiO2 films developed using HiPIMS
Source abstract
Abstract
High power impulse magnetron sputtering (HiPIMS) is one of the recent advanced techniques for the development of high quality TiO 2 thin films. Due to the formation of high energetic ions in the discharge, HiPIMS can produce various crystalline phases of TiO 2 (anatase and rutile) with low roughness as compared to conventional direct current magnetron sputtering (DCMS). This work emphasizes on the effect of oxygen partial pressure in the evolution of phases and oxidation states of TiO 2 films deposited using HiPIMS along with a comparative study against DCMS grown films under similar oxygen environment. TiO 2 thin films were prepared with DCMS and HiPIMS, as a function of oxygen content in the sputter gas flow. Thickness, density and roughness were calculated using XRR fitting and analysis. It was observed that HiPIMS deposited films were smoother and denser than DCMS grown films. Crystallite sizes of HiPIMS deposited films were significantly lower than DCMS. Phase growth analyses were performed using X-ray diffraction (XRD), Raman and XANES (X-ray absorption near-edge spectroscopy of the Ti L 2,3 and O K-edges) spectroscopy. In HiPIMS grown films, the increase in O 2 partial pressure changed the phase from rutile to mixed and then to anatase phase whereas only rutile and mixed phases were detected in DCMS grown film under similar oxygen environment. HiPIMS developed films were smooth, uniform free from cracks as observed in FESEM and Atomic Force microscope (AFM) morphological images. Lognormal crystallite size distribution values decreased with increasing O 2 partial pressure. Crystal field splitting values of (Δ o) between ∼1.9 and 2.2 eV indicate crystalline phase formation by XANES Ti L 2,3-edge analysis. These findings point to better crystalline growth TiO 2 thin films as compared to DC-MS. HiPIMS grown films shows phase transformation of rutile into mix phase and anatase with increase in oxygen partial pressure.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · ZnO doping and properties · Electronic and Structural Properties of Oxides
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (86)
Show source-provided references
1. Origin of the pre-peak features in the oxygen K-edge x-ray absorption spectra of LaFeO 3 and LaMnO 3 studied by Ga substitution of the transition metal ion
2. Insights into TiO 2 polymorphs: highly selective synthesis, phase transition, and their polymorph-dependent properties10.1039/C7RA11515F ↗
3. New understanding of the difference of photocatalytic activity among anatase, rutile and brookite TiO210.1039/C4CP02201G ↗
4. Influence of annealing on optical and photovoltaic properties of nanostructured TiO2films10.1088/1757-899X/168/1/012054 ↗
5. Impact of rutile and anatase phase on the photocatalytic decomposition of lactic acid10.1016/j.apcatb.2019.04.042 ↗
6. Controlled formation of anatase and rutile TiO 2 thin films by reactive magnetron sputtering10.1063/1.4931925 ↗
7. Dye-sensitized anodic TiO2 nanotubes10.1016/j.elecom.2005.08.013 ↗
8. R. Singh, M. Gupta, D. M. Phase, and S. K. Mukherjee, “Phase growth analysis of sputtered TiO2 thin films at low oxygen partial pressures using XANES and XRR.”.
9. Understanding the physical properties of thin TiO2 films treated in different thermal atmospheric conditions
10. Structure and corrosion properties of thin TiO 2 films obtained by magnetron sputtering10.1016/j.vacuum.2019.03.026 ↗
11. Improvement of facile hydrothermal TiO2 rutile nanorod-flower using second HiPIMS deposition for DSSC performance enhancement
12. UV-Shielding TiO2 thin film deposition on flexible and heat-labile substrate using an open-air hybrid CVD/Plasma method10.1016/j.vacuum.2021.110424 ↗
13. TiO2 photocatalysis for the degradation of pollutants in gas phase: From morphological design to plasmonic enhancement10.1016/j.jphotochemrev.2015.07.001 ↗
14. Temperature-Responsive Multilayer Films Based on Block Copolymer-Coated Silica Nanoparticles for Long-Term Release of Favipiravir10.1021/acsanm.1c03334 ↗
15. Temperature-Responsive Multilayer Films of Micelle-Based Composites for Controlled Release of a Third-Generation EGFR Inhibitor10.1021/acsapm.9b01051 ↗
16. Electrostatically Assembled Multilayered Films of Biopolymer Enhanced Nanocapsules for on-Demand Drug Release10.1021/acsabm.9b00381 ↗
17. Tailoring crystalline structure of titanium oxide films for optical applications using non-biased filtered cathodic vacuum arc deposition at room temperature10.3390/coatings11020233 ↗
18. Why is anatase a better photocatalyst than rutile? - Model studies on epitaxial TiO2 films
19. Controlled formation of anatase and rutile TiO2 thin films by reactive magnetron sputtering10.1063/1.4931925 ↗
20. Electronic and optical properties of three phases of titanium dioxide: Rutile, anatase, and brookite10.1103/PhysRevB.51.13023 ↗
21. Influence of the oxygen partial pressure on the growth and optical properties of RF-sputtered anatase TiO2 thin films10.1016/j.rinp.2017.08.018 ↗
22. Oxygen partial pressure induced effects on the microstructure and the luminescence properties of pulsed laser deposited TiO 2 thin films10.1063/1.4973721 ↗
23. Properties of sputtered TiO2 thin films as a function of deposition and annealing parameters10.1016/j.physb.2015.01.037 ↗
24. Surface and photocatalytic properties of TiO2 thin films prepared by non-aqueous surfactant assisted sol-gel method10.1016/j.jece.2020.104267 ↗
25. Chemical Vapor Deposition of Photocatalytically Active Pure Brookite TiO2 Thin Films10.1021/acs.chemmater.7b04944 ↗
26. Electronic-beam evaporation processed titanium oxide as an electron selective contact for silicon solar cells10.1016/j.cap.2021.10.005 ↗
27. Thickness dependence of the growth of magnetron-sputtered TiO 2 films studied by Raman and optical transmittance spectroscopy10.1063/1.4811682 ↗
28. Pulsed laser deposition of thin films of TiO2 for Li-ion batteries10.1016/j.apsadv.2021.100090 ↗
29. L. A. Martínez-Chávez, E. M. Rivera-Muñoz, R. R. Velázquez-Castillo, L. Escobar-Alarcón, and K. Esquivel, “Au-Ag/TiO2 Thin Films Preparation by Laser Ablation and Sputtering Plasmas for Its Potential Use as Photoanodes in Electrochemical Advanced Oxidation Processes (EAOP),” Catalysts , vol. 11, no. 11. 2021, 10.3390/catal11111406.10.3390/catal11111406 ↗
30. Antibacterial, magnetic and dielectric properties of nano-structured V doped TiO2 thin films deposited by dip coating technique10.1016/j.matchemphys.2021.124659 ↗
31. TiO2 thin films by ultrasonic spray pyrolysis as photocatalytic material for air purification10.1098/rsos.181578 ↗
32. Photoluminescence and photocatalytic activity of spin coated Ag+ doped anatase TiO2 thin films
33. Magnetron sputtering technique for analyzing the influence of RF sputtering power on microstructural surface morphology of aluminum thin films deposited on SiO2/Si substrates10.1007/s00339-021-04892-0 ↗
34. HiPIMS deposition of TiOx in an industrial-scale apparatus: Effects of target size and deposition geometry on hysteresis10.1016/j.surfcoat.2013.08.053 ↗
35. Low-energy ion irradiation in HiPIMS to enable anatase TiO2 selective growth10.1088/1361-6463/aac080 ↗
36. Rutile TiO2 thin films grown by reactive high power impulse magnetron sputtering10.1016/j.tsf.2013.07.058 ↗
37. Synthesis of Anatase (Core)/Rutile (Shell) Nanostructured TiO2 Thin Films by Magnetron Sputtering Methods for Dye-Sensitized Solar Cell Applications10.1021/acsaem.9b01910 ↗
38. Blocking layers for nanocomposite photoanodes in dye sensitized solar cells: Comparison of atomic layer deposition and TiCl4 treatment10.1016/j.tsf.2015.11.054 ↗
39. Ti2p and O1s X-ray absorption of TiO2 polymorphs10.1016/S0038-1098(97)00300-1 ↗
40. Oxygen K-edge X-ray Absorption Spectra10.1021/acs.chemrev.9b00439 ↗
41. L2,3 x-ray-absorption edges of d0 compounds: K+, Ca2+, Sc3+, Ti4+Oh (octahedral) symmetry10.1103/PhysRevB.41.928 ↗
42. Phase growth analysis of sputtered TiO2 thin films at low oxygen partial pressures using XANES and XRR10.1088/2053-1591/ab4e3f ↗
43. Photocatalytic activity and stability of TiO2 and WO3 thin films10.1016/j.matchar.2012.04.021 ↗
44. Stability of TiO2-coated ZnO photocatalytic thin films for photodegradation of methylene blue10.1116/6.0000306 ↗
45. Stability of the photocatalytic activity of TiO2deposited by reactive sputtering10.1590/1980-5373-mr-2021-0051 ↗
46. Development of fast heating electron beam annealing setup for ultra high vacuum chamber10.1063/1.4865458 ↗
47. Development of soft X-ray polarized light beamline on Indus-2 synchrotron radiation source10.1063/1.4872719 ↗
48. Surface Studies of Solids by Total Reflection of X-Rays10.1103/PhysRev.95.359 ↗
49. Inert gas effects on the deposition rate of TiO2 during reactive HiPIMS10.1016/j.surfcoat.2014.02.009 ↗
50. Target material pathways model for high power pulsed magnetron sputtering10.1116/1.1865133 ↗
51. Measurement of the plasma potential in a magnetron discharge and the prediction of the electron drift speeds10.1088/0963-0252/10/3/314 ↗
52. Plasma potential mapping of high power impulse magnetron sputtering discharges10.1063/1.3700242 ↗
53. The physical reason for the apparently low deposition rate during high-power pulsed magnetron sputtering10.1016/j.vacuum.2007.10.011 ↗
54. Deposition rates of high power impulse magnetron sputtering: Physics and economics10.1116/1.3299267 ↗
55. Guiding the deposition flux in an ionized magnetron discharge10.1016/j.tsf.2006.07.183 ↗
56. Cross-field ion transport during high power impulse magnetron sputtering10.1088/0963-0252/17/3/035021 ↗
57. Effects of oxygen partial pressure on packing density and laser damage threshold of TiO2 thin films10.1063/1.2779243 ↗
58. Synthesis and doping of TiO2 thin films via a new type of laser plasma source
59. Effect of peak power in reactive high power impulse magnetron sputtering of titanium dioxide10.1016/j.surfcoat.2011.04.071 ↗
60. The Scherrer Formula for X-Ray Particle Size Determination10.1103/PhysRev.56.978 ↗
61. Contamination of TiO2 thin films spin coated on rutile and fused silica substrates10.1016/j.surfcoat.2018.09.009 ↗
62. Thickness dependence of structural, optical and morphological properties of sol-gel derived TiO2 thin film10.1088/2053-1591/aae4d0 ↗
63. Development of MgO:TiO2 thin films for gas sensor applications10.1016/j.ceramint.2018.11.079 ↗
64. Calibration of the Raman spectrum to the oxygen stoichiometry of nanophase TiO210.1063/1.104274 ↗
65. Effects of Oxygen Modification on the Structural and Magnetic Properties of Highly Epitaxial La0.7Sr0.3MnO3 (LSMO) thin films10.1038/s41598-020-60343-5 ↗
66. ImageJ2: ImageJ for the next generation of scientific image data10.1186/s12859-017-1934-z ↗
67. Effect of oxygen addition on microstructure and mechanical properties of quaternary TNTZ superelastic thin films obtained by magnetron sputtering10.1016/j.matchemphys.2018.06.066 ↗
68. Influence the oxygen flow rate on the film thickness, structural, optical and photoluminescence behavior of DC sputtered NiOx thin films10.1016/j.physb.2019.05.012 ↗
69. Influence of O2 flow rate on the characteristics of TiO2 thin films deposited by RF reactive sputtering10.1016/j.matpr.2020.07.405 ↗
70. Effect of oxygen partial pressure in deposition ambient on the properties of RF magnetron sputter deposited Gd_2O_3 thin films10.1364/AO.56.006114 ↗
71. High doping efficiency Al-doped ZnO films prepared by co-injection spatial atomic layer deposition10.1016/j.jallcom.2021.161025 ↗
72. Gwyddion: an open-source software for SPM data analysis10.2478/s11534-011-0096-2 ↗
73. XANES observations of the inhibition and promotion of anatase and rutile phases in silver containing films10.1039/c3ja50354b ↗
74. The role of interstitial sites in the Ti3d defect state in the band gap of titania10.1126/science.1159846 ↗
75. Study of the L23 edges in the 3d transition metals and their oxides by electron-energy-loss spectroscopy with comparisons to theory10.1103/PhysRevB.26.614 ↗
76. Polaronic satellites in x-ray-absorption spectra10.1103/PhysRevB.41.12366 ↗
77. A Ti L-edge X-ray absorption study of Ti-silicate glasses10.1007/s002690100208 ↗
78. L2,3 x-ray-absorption edges of d0 compounds: K+, Ca2+, Sc3+, and Ti4+ in Oh (octahedral) symmetry10.1103/PhysRevB.41.928 ↗
79. 2p x-ray absorption of 3d transition-metal compounds: An atomic multiplet description including the crystal field10.1103/PhysRevB.42.5459 ↗
80. Electron energy-loss spectroscopy (EELS) and the electronic structure of titanium dioxide10.1016/0038-1098(87)90792-7 ↗
81. Role of local geometry in the spin and orbital structure of transition metal compounds10.1134/S1063776116030079 ↗
82. Ti 2p x-ray absorption in titanium dioxides (TiO2): The influence of the cation site environment
83. Electronic structure of titania aerogels from soft x-ray absorption spectroscopy10.1103/PhysRevB.69.245102 ↗
84. Oxygen 1s X-ray-absorption edges of transition-metal oxides10.1103/PhysRevB.40.5715 ↗
85. Electron energy loss and X-ray absorption spectroscopy of rutile and anatase: a test of\rstructural sensitivity10.1088/0953-8984/1/4/012 ↗
86. Electronic structure modification and Fermi level shifting in niobium-doped anatase titanium dioxide thin films: a comparative study of NEXAFS, work function and stiffening of phonons10.1039/C5CP07287E ↗