Microstructural transformation and thermo-mechanical improvement of quinary Bi–Sn–In–Ga–Zn solder bumps on a flexible PET substrate
Source abstract
Abstract
Abstract Novel Bi–Sn–In–Ga–Zn powders were fabricated using a gas atomization process. The addition of 5.0 wt% Zn to a Bi–Sn–In–Ga alloy system resulted in the formation of a pure Zn state as a precipitate, which was mostly dispersed along the grain boundaries during solidification. From this reason, the refined microstructure, which was effective for easy adsorption of outer thermal energy and high surface free energy, could provide a lower onset melting temperature of 58.9 °C and narrower melting range of 6.9 °C compared to those of the quaternary solder powders used as a reference (61.6 and 7.6 °C, respectively). The hardness of the quinary solder was also significantly increased (by 34.7%) by the addition of Zn. As a result, the quinary solder pastes reflowed at a low melting temperature of 110 °C, which is well suited to the formation of solder joints on a flexible polyethylene terephthalate (PET) substrate.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · 3D IC and TSV technologies · Injection Molding Process and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (61)
Show source-provided references
1. Electromigration in 3D–IC scale Cu/Sn/Cu solder joints10.1016/j.jallcom.2016.03.134 ↗
2. Influence of laminate type on tin whisker growth in tin-rich lead-free solder alloys10.1016/j.mseb.2012.03.039 ↗
3. Utilizing the thermodynamic nanoparticle size effects for low temperature Pb-free solder10.1016/j.mseb.2011.12.019 ↗
4. Properties and reliability of solder microbump joints between Si chips and a flexible substrate10.1007/s11664-015-3781-x ↗
5. Materials science
6. Preparation of property-controlled Bi-based solder powders by a ball-milling process10.3390/met6040074 ↗
7. Substrates for flexible electronics: A practical investigation on the electrical, film flexibility, optical, temperature, and solvent resistance properties10.1002/polb.22227 ↗
8. Thermo-mechanical evolution of ternary Bi–Sn–In solder micropowders and nanoparticles reflowed on a flexible PET substrate10.1016/j.apsusc.2016.12.050 ↗
9. Microstructure and mechanical properties of as-reflowed Sn58Bi composite solder pastes10.1016/j.jmatprotec.2016.07.040 ↗
10. Effect of In on microstructure, thermodynamic characteristic and mechanical properties of Sn–Bi based lead-free solder10.1016/j.jallcom.2015.01.219 ↗
11. Effective suppression of interfacial intermetallic compound growth between Sn–58wt.% Bi solders and Cu substrates by minor Ga addition10.1016/j.jallcom.2013.10.035 ↗
12. Low-frequency damping properties of eutectic Sn–Bi and In–Sn solders10.1016/j.scriptamat.2010.12.035 ↗
13. Correlation between microstructure and mechanical properties of Sn–Bi–X solders10.1016/j.msea.2015.11.038 ↗
14. Solder wetting behavior enhancement via laser-textured surface microcosmic topography10.1016/j.apsusc.2016.01.167 ↗
15. Structure and properties of lead-free solders bearing micro and nano particles10.1016/j.mser.2014.06.001 ↗
16. Thermal property, wettability and interfacial characterization of novel Sn–Zn–Bi–In alloys as low-temperature lead-free solders10.1016/j.matdes.2015.06.148 ↗
17. Microstructural evolution and joint strength of Sn–58Bi/Cu joints through minor Zn alloying substrate during isothermal aging10.1016/j.jallcom.2016.07.084 ↗
18. Effects of minor Cu and Zn additions on the thermal, microstructure and tensile properties of Sn–Bi-based solder alloys10.1016/j.jallcom.2014.06.015 ↗
19. The effect of adding Zn into the Sn–Ag–Cu solder on the intermetallic growth rate
20. R. Mayappan, Wetting and intermetallic study between Sn–3.5Ag–1.0Cu–xZn lead-free solders and copper substrate (x=0, 0.1, 0.4, 0.7), 501 (2012) 150-154.
21. Effects of Zn addition on microstructure and tensile properties of Sn–1Ag–0.5 Cu alloy10.1016/j.msea.2009.10.048 ↗
22. New, lead-free solders10.1007/BF02653349 ↗
23. Puttlitz · 2004
24. Ti addition to enhance corrosion resistance of Sn–Zn solder alloy by tailoring microstructure10.1016/j.jallcom.2015.04.168 ↗
25. Oxidation resistant effects of Ag2S in Sn–Ag–Al solder: A mechanism for higher electrical conductivity and less whisker growth10.1016/j.corsci.2015.12.021 ↗
26. Bimodal NdNiAl and NdFeB hybrid catalytic and magnetic nanoparticles laminated on Fe foam: catalytic conversion of CO+3H2 to CH410.1039/C7RA00940B ↗
27. Fabrication of pre-alloyed Al–Li powders with high Li content via thermal dehydrogenation of LiH and rapid solidification process10.1016/j.matdes.2016.01.009 ↗
28. Rate-dependent indentation hardness of a power-law creep solder alloy10.1063/1.1537513 ↗
29. Impurity and alloying effects on interfacial reaction layers in Pb-free soldering10.1016/j.mser.2009.12.001 ↗
30. Synthesis and thermal properties of low melting temperature tin/indium (Sn/In) lead-free nanosolders and their melting behavior in a vapor flux10.1016/j.jallcom.2014.11.173 ↗
31. Microstructural modifications and properties of low-Ag-content Sn–Ag–Cu solder joints induced by Zn alloying10.1016/j.jallcom.2015.09.033 ↗
32. Shackelford · 2016
33. Grain refinement of electronic solders: The potential of combining solute with nucleant particles10.1016/j.jallcom.2017.04.268 ↗
34. Effect of silver and indium addition on mechanical properties and indentation creep behavior of rapidly solidified Bi–Sn based lead-free solder alloys10.1016/j.msea.2012.09.038 ↗
35. Effect of Al on the electrochemical corrosion behaviour of Pb free Sn–8.5Zn–0.5Ag–XAl–0.5Ga solder in 3.5% NaCl solution10.1016/j.apsusc.2005.08.020 ↗
36. Effects of aging treatment on mechanical properties and microstructure of Sn–8.5Zn–0.5Ag–0.01Al–0.1Ga solder10.1016/j.msea.2006.11.144 ↗
37. The crystal structure of a metastable binary phase related to β-Ga: β′-Ga (In)10.1016/0022-4596(79)90129-4 ↗
38. Direct writing of flexible electronics through room temperature liquid metal ink10.1371/journal.pone.0045485 ↗
39. Thermodynamic studies of gallium–indium liquid alloys by solid state electrochemistry with oxide electrolytes10.1021/je60070a016 ↗
40. Pressure-induced structural change in liquid GaIn eutectic alloy10.1038/s41598-017-01233-1 ↗
41. Effects of a third element on microstructure and mechanical properties of eutectic Sn–Bi solder10.5104/jiepeng.2.98 ↗
42. Interfacial reactions between molten Sn–Bi–X solders and Cu substrates for liquid solder interconnects10.1016/j.actamat.2006.02.030 ↗
43. Studies of the Ag–In phase diagram and surface tension measurements10.1007/s11664-001-0138-4 ↗
44. Early stage growth characteristics of Ag3Sn intermetallic compounds during solid–solid and solid–liquid reactions in the Ag–Sn interlayer system: Experiments and simulations10.1016/j.jallcom.2014.08.082 ↗
45. The role of Zn precipitates and Cl− anions in pitting corrosion of Sn–Zn solder alloys10.1016/j.corsci.2014.12.014 ↗
46. Effect of exposure to alkaline solution on Sn–9Zn solder joints10.1016/j.jmatprotec.2014.12.018 ↗
47. Corrosion measurement of Sn–Zn lead-free solders in 6M KOH solution10.1016/j.measurement.2013.10.002 ↗
48. The effects of gallium additions on microstructures and thermal and mechanical properties of Sn–9Zn solder alloys10.1155/2014/606814 ↗
49. The effect of undercooling on the microstructure and tensile properties of hypoeutectic Sn–6.5Zn–xCu Pb-free solders10.1016/j.matdes.2015.05.016 ↗
50. Enhancement of creep resistance and thermal behavior of eutectic Sn–Cu lead-free solder alloy by Ag and In-additions10.1016/j.matdes.2012.04.007 ↗
51. The influence of Ni and Zn additions on microstructure and phase transformations in Sn–0.7Cu/Cu solder joints10.1016/j.actamat.2014.10.003 ↗
52. Thermal and mechanical properties of Sn–Zn–Bi lead-free solder alloys10.1016/j.jallcom.2009.04.108 ↗
53. Tensile deformation behavior and melting property of nano-sized ZnO particles reinforced Sn–3.0Ag–0.5Cu lead-free solder10.1016/j.msea.2014.09.028 ↗
54. Effect of Al addition to bulk microstructure, IMC formation, wetting and mechanical properties of low-Ag SAC solder
55. Smallman · 1999
56. An improved technique for determining hardness and elastic modulus using load and displacement sensing indentation experiments10.1557/JMR.1992.1564 ↗
57. The tensile impact properties of aged Sn–3Ag–0.5Cu/Cu solder joints10.1016/j.microrel.2015.10.002 ↗
58. Comparison of the fracture toughness of Cu6Sn5 intermetallic compound as measured by nanoindentation and other methods10.1016/j.matlet.2015.10.019 ↗
59. In situ observations on creep fatigue fracture behavior of Sn–4Ag/Cu solder joints10.1016/j.actamat.2011.06.010 ↗
60. On the initial stages of phase formation at the solid Cu/liquid Sn-based solder interface10.1016/j.actamat.2016.07.021 ↗
61. Interface reaction between an electroless Ni–Co–P metallization and Sn–3.5Ag lead-free solder with improved joint reliability10.1016/j.actamat.2014.02.026 ↗