journal article·2020-11

Tuning of CeO2-MnO2 nano composite in Al-Zn alloy matrix for effective activation

S.R. Archana, P.S. Arun, B.R. Sreelekshmi, S.M.A. Shibli

Publisher page

Abstract

Abstract Efficient Al + 5 wt% Zn sacrificial anode was prepared and its activity was further enhanced by tuning CeO2-MnO2 nano composite in the alloy matrix. The nano composite was prepared by thermal decomposition method and was characterised by XRD and HRTEM. Al + 5 wt% Zn were fabricated by the incorporation of the composite in the alloy matrix. The composite acted as lattice expander in the Al-Zn alloy and increased dissolution of Zn. Very high galvanic efficiency of 92% was achieved by tuning the amount of the composite in the Al-Zn alloy anode. Its uniform corrosion behaviour was evaluated by potentiodynamic polarization, electrochemical impedance spectroscopy, cyclic polarisation and post consumption microscopic evaluation. A significant lowering in impedance value was achieved by increasing the amount of nano composite in the alloy due to the increased penetration of the oxide film by chloride ions. The composite and Zn in the alloy synergistically activated the Al alloy which facilitated uniform corrosion suppressing pitting corrosion.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: ZnO doping and properties · Catalytic Processes in Materials Science · Semiconductor materials and devices

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (44)

Show source-provided references
1. Ab initio and thermodynamic modelling of alloying effects on activity of sacrificial aluminium anodes10.1016/j.corsci.2011.01.046 ↗
2. Corrosion of an Al–Zn–In alloy in chloride media10.1016/S0010-938X(02)00042-2 ↗
3. Breakdown of ultrathin anodic valve metal oxide films in metal-insulatormetal-contacts compared with metal-insulator-electrolyte contacts10.1016/S0040-6090(02)00453-4 ↗
4. A study on the corrosion behavior of aluminum alloys in seawater10.1016/j.matdes.2007.01.021 ↗
5. Corrosion mechanism of Al, Al–Zn and Al–Zn–Sn alloys in 3 wt.% NaCl solution10.1016/j.corsci.2014.07.018 ↗
6. Passivity breakdown, pit initiation and propagation of pits in metallic materials – review10.1016/j.corsci.2014.10.006 ↗
7. Corrosion analysis of Al–Zn–In–Mg–Ti–Mn sacrificial anode alloy10.1016/j.jallcom.2010.02.174 ↗
8. Electrodeposition of gallium and zinc onto aluminium. Influence of the electrodeposited metals on the activation process10.1016/j.tsf.2007.04.016 ↗
9. Mechanism of activation of aluminum by low melting point elements: part 1-effect of zinc on activation of aluminum in metastable pitting10.5006/1.3284817 ↗
10. Development of high performance aluminium alloy sacrificial anodes reinforced with metal oxides10.1016/j.matlet.2006.10.062 ↗
11. influence of alloying elements and microstructure on aluminium sacrificial anode performance: case of Al-Zn10.1023/A:1003684219989 ↗
12. The activation of aluminium by activator elements10.1016/0010-938X(93)90149-B ↗
13. Effect of gallium ions on the electrochemical behaviour of Al, Al-Sn, Al-Zn and Al-Zn-Sn alloys in chloride solutions10.1016/S0010-938X(00)00100-1 ↗
14. Electrochemical behaviour of Al-Zn-Ga and Al-In-Ga alloys in chloride media10.1016/j.matchemphys.2012.06.036 ↗
15. The synergistic interaction between indium and zinc in the activation of aluminium in aqueous electrolytes10.1016/0010-938X(94)90155-4 ↗
16. Anodic dissolution of Al sacrificial anodes in NaCl solution containing Ce10.1016/j.corsci.2011.01.001 ↗
17. Development of nano cerium oxide incorporated aluminium alloy sacrificial anode for marine applications10.1016/j.corsci.2008.06.017 ↗
18. Development of MnO2-incorporated high performance aluminium alloy matrix sacrificial anodes10.1007/s10800-008-9659-3 ↗
19. T. Pojanavaraphan, Aluminium alloy for sacrificial anode. WO2017034486 A1, 2017.
20. In situ corrosion analysis of Al-Zn-In-Mg-Ti-Ce sacrificial anode alloy10.1016/j.matchar.2012.01.003 ↗
21. Fundamentals and catalytic applications of CeO2-based materials10.1021/acs.chemrev.5b00603 ↗
22. Synergistic effect of CeO2 modified TiO2 photocatalyst on the enhancement of visible light photocatalytic performance10.1016/j.jallcom.2017.04.138 ↗
23. Complete oxidation of methane on NiO nanoclusters supported on CeO2 nanorods through synergistic effect10.1021/acssuschemeng.8b00234 ↗
24. Synthesis, characterization and application of nano CeO2–Fe2O3 mixed oxide electrocatalyst for hydrogen evolution reaction10.1016/j.ijhydene.2016.11.092 ↗
25. Enhanced electrocatalytic activity of a hierarchical CeO2 @MnO2 core-shell composite for oxygen reduction reaction10.1016/j.ceramint.2018.09.111 ↗
26. Design and preparation of MnO2/CeO2−MnO2 double-shelled binary oxide hollow spheres and their application in CO oxidation10.1021/acsami.6b00002 ↗
27. Rational design of template-free MnOx-CeO2 hollow nanotube as de-NOx catalyst at low temperature10.1016/j.apsusc.2017.09.131 ↗
28. Pt-Au/MOx-CeO2 (M = Mn, Fe, Ti) Catalysts for the Co-oxidation of CO and H2 at room temperature10.3390/molecules22030351 ↗
29. Highly porous and tunable electrocatalysts for the hydrogen and oxygen evolution reaction10.1002/adfm.201402078 ↗
30. Regulating proton-coupled electron transfer for efficient water splitting by manganese oxides at neutral pH10.1038/ncomms5256 ↗
31. Temperature effects on structural properties in the synthesis of nanocrystalline Zr0.5Ce0.5O2 solid solution: a study by XRD and HRTEM10.1016/j.jallcom.2009.10.249 ↗
32. Synthesis, structural and optical properties of Mn-doped ceria nanoparticles: a promising catalytic material10.1007/s40195-016-0387-0 ↗
33. Revealing the relationship between grain size and corrosion rate of metals10.1016/j.scriptamat.2010.08.035 ↗
34. Galvanic corrosion characteristics of aluminum alloyed with group IV metals
35. Relationship between microstructure, microhardness and corrosion sensitivity of an AA2024-T3 friction stir welded joint10.1016/j.corsci.2011.05.049 ↗
36. Corrosion behavior and mechanical properties of Al-Zn-Mg aluminum alloy weld10.1016/j.corsci.2017.05.007 ↗
37. Mechanism of activation of aluminum by low-melting point elements: Part 2 effect of zinc on activation of aluminum in pitting corrosion10.5006/1.3283964 ↗
38. Electrochemical corrosion study of Mg–Al–Zn–Mn alloy in aqueous ethylene glycol containing chloride ions10.1016/j.jmrt.2016.04.003 ↗
39. Enhancing the insulating and dielectric properties of barrier anodic Al2O3 on high purity aluminium
40. The role of chloride ions pH in the corrosion and pitting of Al-Si alloys10.1023/A:1012039804089 ↗
41. Electrochemical behaviour of aluminium alloys containing indium and tin in NaCl solution10.1016/j.matchemphys.2010.02.040 ↗
42. Determining the appropriate scan rate to perform cyclic polarization test on the steel bars in concrete10.1016/j.electacta.2009.10.004 ↗
43. Study of Al alloy corrosion in neutral NaCl by the pitting scan technique10.1016/j.matchemphys.2010.02.022 ↗
44. The pit transition potential in the repassivation of aluminium alloys10.1002/sia.5270 ↗