journal article·2017-11

Impact of nano zinc oxide on the friction – Wear property of electroless nickel-phosphorus sea shell composite coatings

M.S. Jagatheeshwaran, A. Elayaperumal, S. Arulvel

Publisher page

Abstract

Abstract High friction force of NiP/SSP (Nickel-phosphorus/Sea shell particle) composite coating limits their use in low friction applications, hence to overcome this, nano ZnO is incorporated with different weight percentage. NiP with weight fraction (3.0 g/l) of (SSP) and various weight fractions (0.10 g/l, 0.25 g/l, 0.50 g/l, 0.75 g/l and 1.0 g/l) of nano ZnO particles were deposited on En8 steel using an alkaline electroless process. Friction – wear test was carried out on NiP/SSP/ZnO composite coatings and comparison was made with NiP and NiP/SSP composite coating using pin on disc apparatus. Wear track was characterized using SEM and non-contact surface profilometer. Hardness is measured using Vickers micro hardness tester. There is a decrease in the hardness of NiP/SSP/ZnO coating due to the incorporation of nano ZnO particles. Significant improvement in friction and wear resistance was observed for NiP/SSP/ZnO (0.25 g/l) coatings in contrast to NiP and NiP/SSP coating.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Electrodeposition and Electroless Coatings · Lubricants and Their Additives · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (27)

Show source-provided references
1. Discussion on the feasibility of using proteinized/deproteinized crab shell particles for coating applications: synthesis and characterization10.1016/j.jece.2016.08.031 ↗
2. Electroless nickel – phosphorus coating on crab shell particles and its characterization10.1016/j.jssc.2017.02.001 ↗
3. Nano-structured biogenic calcite: a thermal and chemical approach to folia in oyster shell10.1016/j.micron.2007.03.006 ↗
4. Electrolyte conductivity through the shell of the eastern oyster using a four-electrode measurement10.1149/1.3230623 ↗
5. Wear characteristics of electroless NiP/bio-composite coatings on En8 steel10.1016/j.jmapro.2015.08.002 ↗
6. The role of calcinated sea shell particles on friction-wear behavior of electroless NiP coating: fabrication and characterization10.1016/j.surfcoat.2016.07.053 ↗
7. The effect of heat treatment on the structure and abrasive wear resistance of autocatalytic NiP and NiP–SiC coatings10.1016/S0257-8972(01)01492-X ↗
8. Effect of SiO2 and PTFE additives on dry sliding of NiPelectroless coating10.1016/j.triboint.2012.12.012 ↗
9. Nickel coating on peptide nanotubes by electroless plating10.1016/j.tsf.2011.08.114 ↗
10. Friction and wear of electroless NiP and NiP + PTFE coatings10.1016/j.wear.2005.02.052 ↗
11. Structural, optical and electrical properties of zinc oxide thin films deposited by sol-gel spin coating technique10.1016/j.ijleo.2017.01.014 ↗
12. Incorporation of nano zinc oxide for improvement of electroless nickel plating10.1016/j.apsusc.2006.02.063 ↗
13. Influence of fly ash on corrosion resistance and chloride ion permeability of concrete10.1016/j.conbuildmat.2011.12.106 ↗
14. The effect of carbon nanotubes on the corrosion and tribological behavior of electroless Ni–P–CNT composite coating10.1016/j.apsusc.2011.10.067 ↗
15. Electroless nickel, alloy, composite and nano coatings – a critical review10.1016/j.jallcom.2013.03.107 ↗
16. Phase composition, microstructure and microhardness of electroless nickel composite coating co-deposited with SiC on cast aluminium LM24 alloy substrate10.1016/j.surfcoat.2013.08.063 ↗
17. The role of surface texture on friction and transfer layer formation during repeated sliding of Al–4Mg against steel10.1016/j.wear.2011.01.076 ↗
18. Development of nickel–phosphorus coatings containing micro particles of talc phyllosilicates10.1016/j.matchemphys.2012.09.049 ↗
19. Effect of pickling processes on the microstructure and properties of electroless Ni–P coating on Mg–7.5Li–2Zn–1Y alloy10.1016/j.pnsc.2014.10.014 ↗
20. Electroless deposition and characterization of high phosphorus Ni–P–Si3N4 composite coatings10.1016/S1452-3981(23)17109-4 ↗
21. Development of electroless NiP-PTFE-SiC composite coating10.1016/S0257-8972(02)00899-X ↗
22. Surface Modification and Mechanisms: Friction, Stress, and Reaction Engineering edited by George E. Totten, Hong Liang.
23. Tribology of electroless nickel coatings – a review10.1016/j.matdes.2010.11.013 ↗
24. Influence of heat treatment on tribological properties of electroless Ni–P and Ni–P–Al2O3 coatings on Al–Si casting alloy10.1016/j.apsusc.2009.11.057 ↗
25. Electroless deposition of Ni–P–B4C composite coating on AZ91D magnesium alloy and investigation on its wear and corrosion resistance10.1016/j.matdes.2009.12.042 ↗
26. Electroless NiP micro- and nano-composite coatings10.1016/j.surfcoat.2005.11.127 ↗
27. Sarika Sharma, Sulaxna Sharma, Awanish Sharma, and Vijaya Agarwala, Co-deposition of Synthesized ZnO Nanoparticles into Ni-P Matrix Using Electroless Technique and Their Corrosion Study, 25 (2016) 4383–4393.