Abstract In order to prepare embedded planar decoupling capacitors with high capacitance density, we attempted to fabricate BaTiO 3 thin films on Cu substrates at room temperature by employing aerosol deposition method (ADM). Their thickness range was 0.2–1.5 μm. From the measurement of the magnitude and phase of their impedance by a vertical type, it was confirmed that BaTiO 3 thin films acted like conductors or dielectrics in the thickness range of 0.8–1.0 μm. In this thickness range, we supposed that their high leakage currents resulted in the problems of interfaces between BaTiO 3 thin films and Cu substrates or the quality of BaTiO 3 films themselves. So, the magnitude and phase of impedance of BaTiO 3 thin films deposited on glass substrates and Cu substrates to remove the problems of interfaces were measured by a horizontal type. As a result, all BaTiO 3 thin films deposited on glass substrates became dielectrics. However, some BaTiO 3 thin films with below 0.8 μm deposited on Cu substrates acted like conductors in this thickness range. Consequently, it could be suggested that the major causes were problems of interfaces between BaTiO 3 thin films and Cu substrates.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Semiconductor materials and devices · Dielectric materials and actuators · Copper Interconnects and Reliability

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (13)

Show source-provided references
1. Shahparnia · IEEE Trans. Electromagn. Compat. · 2004 · 46–4 · 58010.1109/TEMC.2004.837671 ↗
2. Balaraman · 2004 · 282
3. Imanaka · J. Eur. Ceram. Soc. · 2007 · 27 · 278910.1016/j.jeurceramsoc.2006.11.055 ↗
4. Wan · 2005 · 1617
5. Tsurumi · J. Kor. Ceram. Soc. · 2003 · 40 · 71510.4191/KCERS.2003.40.8.715 ↗
6. Nam · Jpn. J. Appl. Phys. · 2004 · 43 · 541410.1143/JJAP.43.5414 ↗
7. Lahti · 2005 · A25
8. Akedo · Mater. Res. Soc. Symp. Proc. · 2003 · 77910.1557/PROC-779-W7.10/U8.10 ↗
9. Abdullah · IEEE Trans. Electr. Insul. · 1990 · 25 · 60510.1109/14.55739 ↗
10. Nam · Trans. Mater. Res. Soc. Jpn. · 2004 · 29 · 1215
11. Akedo · J. Am. Ceram. Soc. · 2006 · 89 · 183410.1111/j.1551-2916.2006.01030.x ↗
12. Akedo · J. Therm. Spray Technol. · 2008 · 17 · 18110.1007/s11666-008-9163-7 ↗
13. Hatono · Jpn. J. Appl. Phys. · 2007 · 46 · 691510.1143/JJAP.46.6915 ↗