Abstract

We present a detailed study of the thermal stability of activated junctions as a function of the post-annealing conditions. p+/n junctions were formed by implanting 500 eV boron (1 × 1015 cm−2) into Ge+ preamorphised Si followed by solid phase epitaxial growth (SPEG) at 650 °C. Post-annealing temperatures ranged from 250 to 950 °C, with times ranging from 3 to 1800 s. Four point probe (4PP), secondary ion mass spectrometry (SIMS) and transmission electron microscopy (TEM) analysis were then used to investigate the evolution of boron activation, boron diffusion and of the implantation induced extended defects. During isothermal anneals in the 750–900 °C range, it is found that the sheet resistance initially increases (deactivation) and then decreases (reactivation) with rates proportional to the temperature itself. TEM results elucidate the crucial role of the extended defects in the deactivation process. On the other hand, the combination of 4PP and SIMS measurements allows to separate the respective contribution of both cluster dissolution and dopant in-diffusion to the reactivation process.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Silicon and Solar Cell Technologies · Semiconductor materials and interfaces · Integrated Circuits and Semiconductor Failure Analysis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (20)

Show source-provided references
1. International Technology Roadmap for Semiconductors 2003 Edition, Semiconductor Industry Association, San Jose, CA, December 2003.
2. See the proceedings of the 7th International Workshop on the Fabrication of Ultra-Shallow Doping Profiles in Semiconductors (26 April–1 May 2003, Santa Cruz, CA, USA) published in J. Vac. Sci. Technol. B 22 (1) (2004) 288–476.
3. Lerch · Electrochem. Soc. Proc. · 2003 · 14 · 43
4. Lilak · Appl. Phys. Lett. · 2002 · 81 · 224410.1063/1.1508438 ↗
5. A. Mokhberi, P.B. Griffin, J.D. Plummer, Proceedings of SISPAD 2000 International Conference, IEEE, 2000, p. 163.
6. Shauly · J. Vac. Sci. Technol. B · 2004 · 22 · 59210.1116/1.1651548 ↗
7. Landi · Appl. Phys. A · 1987 · 44 · 13510.1007/BF00626414 ↗
8. Pawlak · Appl. Phys. Lett. · 2004 · 84 · 205510.1063/1.1682697 ↗
9. Jin · J. Vac. Sci. Technol. B · 2002 · 20 · 42210.1116/1.1424279 ↗
10. Aboy · Appl. Phys. Lett. · 2003 · 83 · 416610.1063/1.1628391 ↗
11. Mattoni · Phys. Rev. B · 2004 · 69 · 04520410.1103/PhysRevB.69.045204 ↗
12. S. Paul, W. Lerch, D.F. Downey, E.A. Arevalo, Workshop on Ultra-Shallow Junction Formation, USJ 2003, 27 April–1 May 2003, Santa Cruz, CA, 2003, p. 111.
13. Ehrke · J. Vac. Sci. Technol. B · 2004 · 22 · 110.1116/1.1633284 ↗
14. A. Armgliato, D. Nobili, P. Otoja, M. Servidori, S. Solmi, in: H.R Huff, E. Sirtl (Eds.), Electrochem. Soc. Proc. 77-2 Semiconductor Silicon, 1977, p. 638.
15. Olson · Mater. Res. Soc. Symp. Proc. · 1985 · 35 · 2510.1557/PROC-35-25 ↗
16. Olson · Mater. Sci. Rep. · 1988 · 3 · 110.1016/S0920-2307(88)80005-7 ↗
17. Thurber · Natl. Bureau Standards Special Publ. · 1981 · 400
18. Claverie · Appl. Phys. A · 2003 · 76 · 102510.1007/s00339-002-1944-0 ↗
19. Pichler · Mater. Res. Soc. Symp. Proc. · 2002 · 717 · C3.110.1557/PROC-717-C3.1 ↗
20. Colombeau · Appl. Phys. Lett. · 2001 · 78 · 94010.1063/1.1344566 ↗