Eu-doped barium strontium silicate phosphor particles prepared from spray solution containing NH4Cl flux by spray pyrolysis
Source abstract
Abstract
Abstract Eu-doped barium strontium silicate phosphor particles with high photoluminescence intensity under long wavelength ultraviolet were prepared from the spray solution containing NH 4 Cl flux by spray pyrolysis. It was found that the addition of NH 4 Cl to the spray solution makes it possible to greatly improve the photoluminescence intensity of Ba 1.488 Sr 0.5 SiO 4 :Eu 0.012 phosphor particles under long wavelength ultraviolet of 410 nm. The highest photoluminescence intensity, which was achieved when the NH 4 Cl content was 5 wt.%, was about 150% of Ba 1.488 Sr 0.5 SiO 4 :Eu 0.012 particles prepared from the spray solution without flux material at the post-treatment temperature of 1050 °C. The particle size of Ba 1.488 Sr 0.5 SiO 4 :Eu 0.012 phosphor particles were enlarged by using the NH 4 Cl flux in the spray solution because of the large grain growth which was identified from the sharpening of the XRD peaks. Adding the NH 4 Cl flux into the spray solution was found to lower the optimal post-treatment temperature at which the Ba 1.488 Sr 0.5 SiO 4 :Eu 0.012 phosphor particles are fully crystallized and have the maximum photoluminescence intensity. The phosphor particles prepared from spray solution containing 5 wt.% NH 4 Cl flux had the maximum photoluminescence intensity at post-treatment temperature of 1100 °C.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Luminescence Properties of Advanced Materials · Perovskite Materials and Applications · Gas Sensing Nanomaterials and Sensors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (13)
Show source-provided references
1. Strategies Unlimited, Visible LED market review and forecast, 1999.
2. Barry · J. Electrochem. Soc. · 1968 · 115 · 118110.1149/1.2410935 ↗
3. Bender · J. Non-Cryst. Solids · 2002 · 298 · 9910.1016/S0022-3093(02)00943-2 ↗
4. Peng · J. Mater. Chem. · 2003 · 13 · 120210.1039/b211624c ↗
5. Poort · J. Alloys. Comp. · 1997 · 260 · 9310.1016/S0925-8388(97)00140-0 ↗
6. Poort · J. Alloys. Comp. · 1996 · 241 · 7510.1016/0925-8388(96)02324-9 ↗
7. Kang · J. Electrochem. Soc. · 1999 · 146 · 122710.1149/1.1391750 ↗
8. Kang · J. Mater. Res. · 1999 · 14 · 261110.1557/JMR.1999.0349 ↗
9. Kang · Adv. Mater. · 2000 · 12 · 45110.1002/(SICI)1521-4095(200003)12:6<451::AID-ADMA451>3.0.CO;2-S ↗
10. M.J. Hampden-Smith, T.T. Kodas, J. Caruso, U.S. Patent (2001) 6,180,029 B1.
11. Vanheusden · J. Lumin. · 1997 · 75 · 1110.1016/S0022-2313(96)00096-8 ↗
12. Barry · J. Electrochem. Soc. · 1968 · 115 · 73410.1149/1.2411413 ↗
13. Kim · Solid State Comm. · 2005 · 133 · 18710.1016/j.ssc.2004.10.017 ↗