journal article·2000-02

Corrosion, oxidation and strength properties of Nicalon SiC fibre under loading

D.-Y. Song, N. Takeda, H. Kawamoto

Materials Science and Engineering: A· Volume 278· Issue 1-2
Publisher page

Abstract

Abstract Hot corrosion and oxidation behavior of Nicalon fibres in air under loading were investigated and compared. Degradation of Nicalon fibres exposed at temperatures over 900°C in the presence of Na 2 SO 4 was extremely severe compared with that in oxidation environment without Na 2 SO 4 . This is attributed to the rapid oxidation-dissolution of the fibres due to the formation of the liquid Na 2 SiO 3 . Room temperature strength of Nicalon fibre after oxidation decreased with increasing exposure temperature. Reduction of tensile strengths was most significant under the combined condition of exposure temperature and applied loading. This evident strength reduction is caused by the combination of applied load and the reaction between the inherent SiO 2 and free carbon in the fibre. Fracture surfaces of oxidized fibres exhibited mirror-hackle regions, whereas the fracture surfaces of fibres corroded were planar.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Concrete and Cement Materials Research · Silicon Carbide Semiconductor Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (12)

Show source-provided references
1. Gogotsi · J. Mater. Sci. Lett. · 1994 · 13 · 68010.1007/BF00271233 ↗
2. Pysher · J. Am. Ceram. Soc. · 1989 · 72[2] · 28410.1111/j.1151-2916.1989.tb06115.x ↗
3. Gogotsi · J. Mater. Sci. Lett. · 1994 · 13 · 39510.1007/BF00278008 ↗
4. Fareed · Am. Ceram. Soc. Bull. · 1987 · 66[2] · 353
5. Kim · J. Am. Ceram. Soc. · 1991 · 74[3] · 66610.1111/j.1151-2916.1991.tb04079.x ↗
6. Emig · J. Mater. Sci. · 1995 · 30 · 581310.1007/BF00356726 ↗
7. D.S. Fox, N.S. Jacobson, J.L. Smilalek, Hot Corrosion of Silicon Carbide and Silicon Nitride at 1000°C, Ceramic Transactions, Am. Ceram. Soc., 10 (1990) 227.
8. Jacobson · J. Am. Ceram. Soc. · 1985 · 68[8] · 43210.1111/j.1151-2916.1985.tb10170.x ↗
9. Mckee · J. Am. Ceram. Soc. · 1976 · 59[9–10] · 44110.1111/j.1151-2916.1976.tb09514.x ↗
10. Eckel · J. Am. Ceram. Soc. · 1989 · 72[3] · 45510.1111/j.1151-2916.1989.tb06152.x ↗
11. Sawyer · Ceram. Eng. Sci. Proc. · 1986 · 7[7–8] · 91410.1002/9780470320341.ch19 ↗
12. Simon · J. Mat. Sci. · 1984 · 19 · 365810.1007/BF02396938 ↗