Abstract The thermal fatigue testings of γ-TiAl were performed in 200–700 °C and 200–900 °C, and that of thermal cycling with dead-load were conducted in the same temperature ranges with different tensile dead-load. After the samples were subjected to a predetermined thermal cycling, the dynamic elastic modulus and electrical resistance were measured at room temperature. The relative change of modulus D E and that of electrical resistance D R were employed to evaluate damage. In the shorter thermal fatigue, the damage increased intensely. Then, the damage increased very slowly as cycling increased and approached a constant subsequently. The negative increase of D E occurred after thermal cycling with dead-load in initial stage. Nevertheless, The D R did not increase negatively like D E . The fine and dark γ phase increased and the size of lamellar colony reduced obviously after testing, and the damage appeared taking the form of micro-pores, micro-cracks, etc. In addition, the damage mechanisms were also discussed.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Intermetallics and Advanced Alloy Properties · Semiconductor materials and interfaces · MXene and MAX Phase Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (21)

Show source-provided references
1. Kim · JOM · 1989 · 41 · 2410.1007/BF03220267 ↗
2. Dennis · JOM · 1991 · 43 · 4010.1007/BF03221103 ↗
3. Liu · Intermetallics · 1998 · 6 · 65310.1016/S0966-9795(98)00062-4 ↗
4. Kim · Mater. Sci. Eng. A · 1995 · 192/193 · 51910.1016/0921-5093(94)03271-8 ↗
5. William · Scripta Metall. Mater. · 1995 · 33 · 24510.1016/0956-716X(95)00138-L ↗
6. Christ · Mater. Sci. Eng. A · 2001 · 625 · A319
7. Roth · Scripta Mater. · 2006 · 54 · 13710.1016/j.scriptamat.2005.09.049 ↗
8. Sun · Int. J. Fatigue · 2004 · 26 · 45710.1016/j.ijfatigue.2003.10.004 ↗
9. Goldsby · Mater. Sci. Eng. A · 2000 · 279 · 26610.1016/S0921-5093(99)00630-9 ↗
10. Lee · Mater. Sci. Eng. A · 1992 · 154 · 110.1016/0921-5093(92)90356-6 ↗
11. Wang · Int. Mater. Rev. · 1994 · 39 · 22810.1179/imr.1994.39.6.228 ↗
12. Kaya · J. Eur. Ceram. Soc. · 2002 · 22 · 44710.1016/S0955-2219(01)00320-X ↗
13. Lemaitre · Eng. Fract. Mech. · 1987 · 28 · 64310.1016/0013-7944(87)90059-2 ↗
14. Mishin · Acta Mater. · 2000 · 48 · 58910.1016/S1359-6454(99)00400-0 ↗
15. Pouly · Scripta Metall. Mater. · 1993 · 29 · 152910.1016/0956-716X(93)90272-T ↗
16. Murry · 1987
17. Chawla · Metall. Mater. Trans. · 2004 · 35A · 3710.1007/s11661-004-0106-8 ↗
18. Watts · J. Phys. F · 1988 · 119710.1088/0305-4608/18/6/022 ↗
19. Chung · Mater. Sci. Eng. R · 2003 · 42 · 110.1016/S0927-796X(03)00037-8 ↗
20. Pin · 1992
21. Venkata · J. Eur. Ceram. Soc. · 1998 · 18 · 207310.1016/S0955-2219(98)00159-9 ↗