Thermo-magnetic processing of ductile cast iron
Source abstract
Abstract
Abstract In this investigation, austempered ductile cast iron (ADI) with a fully ferritic microstructure was produced by a novel thermo magnetic austempering process. This novel process consists of austempering of ductile cast iron in a high magnetic field of 20 T. Unalloyed ductile cast iron samples were initially austenitized at 927 °C (1700 °F) for 2 h and then quenched in a salt bath to an austempering temperature of 260 °C (500 °F). The samples were austempered at this temperature for 0.5 h in the presence of a strong external magnetic field of 20 T around the salt bath chamber and test samples. This resulted in a fully ferritic microstructure. The microstructure and mechanical properties of the resulting material have been characterized and compared with conventionally processed austempered ductile cast iron at the same temperature (260 °C) without magnetic field.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Microstructure and Mechanical Properties of Steels · Metal Alloys Wear and Properties · Metallurgy and Material Forming
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (38)
Show source-provided references
1. Dodd · Mod. Cast. · 1978 · 68 · 60
2. Gundlach · AFS Trans. · 1983 · 94 · 377
3. Harding · Br. Foundryman · 1986 · 79 · 489
4. Schmidt · Z. Metal. · 1987 · 78 · 871
5. Johansson · AFS Trans. · 1977 · 85 · 117
6. Putatunda · Mater. Character. · 1993 · 30 · 22110.1016/1044-5803(93)90069-8 ↗
7. Shanmugam · J. Mater. Sci. · 1994 · 29 · 493310.1007/BF00356546 ↗
8. Bartosiewicz · 1991 · 135
9. Bartosiewicz · 1990 · 323
10. Rao · Metal. Mater. Trans. A · 1997 · 28 · 145710.1007/s11661-997-0208-1 ↗
11. Rao · Mater. Sci. Technol. · 1998 · 14 · 125710.1179/mst.1998.14.12.1257 ↗
12. Rao · Metal. Mater. Trans. A · 1998 · 29 · 300510.1007/s11661-998-0208-9 ↗
13. Putatunda · J. Test. Eval. · 1995 · 23 · 32510.1520/JTE11401J ↗
14. Doong · Fatigue Fract. Eng. Mater. Struct. · 1989 · 12 · 15510.1111/j.1460-2695.1989.tb00520.x ↗
15. Janowak · AFS Trans. · 1985 · 88 · 123
16. Putatunda · Mater. Sci. Eng. A · 2001 · 315 · 7010.1016/S0921-5093(01)01210-2 ↗
17. Putatunda · Mater. Des. · 2004 · 25 · 21910.1016/j.matdes.2003.09.021 ↗
18. Putatunda · ASM Int. · 1996 · 24 · 103
19. Moore · J. Heat Treat. · 1985 · 4 · 710.1007/BF02835485 ↗
20. Reed Hill · 1973
21. Smith · 1981
22. R.B. Gundlach, J.D. Mullins, Improving the properties of Austempered Ductile Iron, SAE Technical Paper Series 2002-01-139, SAE World Congress, Detroit, Michigan, 2002.10.4271/2002-01-1307 ↗
23. Enomoto · Metall. Mater. Trans. A · 2001 · 32 · 44510.1007/s11661-001-0061-6 ↗
24. Shifflet · Metall. Trans. A · 1978 · l9 · 99910.1007/BF02649845 ↗
25. Joo · Mater. Lett. · 2000 · l43 · 22510.1016/S0167-577X(99)00263-3 ↗
26. Dinsdale · J. Phase Stability · 1991 · 15 · 317
27. Bozorth · 1986
28. Cullity · 1972
29. ASTM E-8: Standard Test Method for Tensile Testing of Metallic Materials, Annual book of ASTM Standards, vol. 3.01, ASTM, 1993, pp. 542–566.
30. ASTM E-399: Standard Test Method for Plane Strain Fracture Toughness Tests in Metallic Materials, Annual Book of ASTM Standards, vol. 3.01, ASTM, 1995, pp. 647–678.
31. Rundman · AFS Trans. · 1982 · 90 · 499
32. Cullity · 1974
33. Roberts · Trans. AIME · 1953 · 197 · 203
34. Choi · Scripta Mater. · 2000 · 43 · 22110.1016/S1359-6462(00)00394-8 ↗
35. Enomoto · Metall. Mater. Trans. A · 2001 · 32 · 44510.1007/s11661-001-0061-6 ↗
36. Liu · J. Mater. Res. · 2001 · 16 · 228010.1557/JMR.2001.0313 ↗
37. Ludtka · Scripta Mater. · 2004 · 51 · 17110.1016/j.scriptamat.2004.03.029 ↗
38. Jaramillo · Scripta Mater. · 2005 · 52 · 46110.1016/j.scriptamat.2004.11.015 ↗