journal article·2000-06

Microscopic fracture mechanism of sintered high purity chromium

Y Matsumoto, S Ohta, N Aoki, M Morinaga

Materials Science and Engineering: A· Volume 285· Issue 1-2
Publisher page

Abstract

Abstract The microscopic fracture mechanism was examined experimentally for high purity chromium. With the specimens prepared by sintering and swaging, a series of tensile tests was carried out in various test conditions. The high purity chromium became more ductile as the test temperature increased, but the ductile-to-brittle transition temperature (DBTT) was not found clearly in the temperature range of 300–623 K. In addition, it was very brittle when tested in water, probably due to hydrogen embrittlement. From a fractographical analysis, it was shown that there were many micro-voids on the fracture surface, when the test temperature was less than 423 K. These micro-voids on a local region in the grain boundary seemed to grow up during deformation and to act as the initiation sites of intergranular fracture, and subsequently followed by transgranular cleavage fracture. The fracture strain increased with decreasing size of micro-voids, irrespective of the test conditions. The growth of the micro-voids was supposed to be one of the predominant factors for controlling the fracture of high purity sintered chromium.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Powder Metallurgy Techniques and Materials · Advanced materials and composites · Microstructure and mechanical properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (26)

Show source-provided references
1. Chromium
2. Maykuth · J. Electrochem. Soc. · 1955 · 102 · 31610.1149/1.2430054 ↗
3. E.P. Abrahamson II, N.J. Grant, Trans. ASM 50 (1958) 705.
4. Stephens · Trans. Met. Soc. AIME · 1968 · 242 · 1837
5. Filippi · Metall. Trans. · 1972 · 3 · 172710.1007/BF02642553 ↗
6. Weaver · J. Inst. Met. · 1960 · 89 · 385
7. Weaver · J. Appl. Phys. · 1960 · 31 · 62610.1063/1.1735654 ↗
8. Allen · Trans. ASM · 1963 · 56 · 387
9. Wain · J. Inst. Met. · 1954 · 83 · 133
10. Wain · J. Inst. Met. · 1957 · 86 · 281
11. Allen · Trans. Met. Soc. AIME · 1963 · 227 · 724
12. Marcinkowski · Acta Metall. · 1962 · 10 · 9510.1016/0001-6160(62)90055-X ↗
13. Hook · Trans. Met. Soc. AIME · 1963 · 227 · 151
14. Gilbert · J. Inst. Met. · 1963 · 92 · 351
15. Nambu · Scripta Metall. Mat. · 1995 · 32 · 40710.1016/S0956-716X(99)80073-9 ↗
16. Matsumoto · Scripta Mat. · 1996 · 35 · 168510.1016/1359-6462(96)00044-9 ↗
17. Matsumoto · Scripta Mat. · 1998 · 38 · 32110.1016/S1359-6462(97)00415-6 ↗
18. Morinaga · Scripta Mat. · 1997 · 37 · 69910.1016/S1359-6462(97)00152-8 ↗
19. Bullen · Phil. Mag. · 1964 · 9 · 80310.1080/14786436408211893 ↗
20. Plastic deformation and fracture of materials
21. Sameljuk · Int. J. Refract. Metals & Hard Mat. · 1996 · 14 · 24910.1016/0263-4368(95)00046-1 ↗
22. Vasilev · Scan. Electron Microsc. · 1986 · 111 · 917
23. Bourcier · Acta Metall. · 1986 · 34 · 244310.1016/0001-6160(86)90147-1 ↗
24. Ohmori · J. Japan Inst. Met. · 1988 · 52 · 22310.2320/jinstmet1952.52.2_223 ↗
25. Phase boundary effects on deformation of bcc metals at low temperatures
26. Sethi · Acta Met. · 1977 · 25 · 32110.1016/0001-6160(77)90151-1 ↗