Transformation-mismatch plasticity in sub-millimeter iron wires
Source abstract
Abstract
Abstract Wires of 99.5% pure iron with 406 and 508 μm diameter were subjected to a uniaxial tensile stress while being thermally cycled about the α–γ allotropic transformation temperature. The strain increments per cycle are proportional to the applied stress in the range 1–22 MPa, indicating that transformation-mismatch plasticity is the dominant deformation mechanism. The strain increments for the wires have the same magnitude as those reported for bulk iron samples, thus, indicating that the internal mismatch strains responsible for this deformation mechanism are undiminished in the wires, despite their high surface-to-volume ratio. Very high average strain rates (up to 3 × 10−3 s−1) were achieved through resistive heating and convective/radiative cooling of the thinnest wires.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Microstructure and Mechanical Properties of Steels · Microstructure and mechanical properties · Magnetic Properties and Applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (23)
Show source-provided references
1. Leblond · Int. J. Plastic. · 1989 · 5 · 55110.1016/0749-6419(89)90001-6 ↗
2. Olson · Metall. Trans. · 1975 · A 6 · 79110.1007/BF02672301 ↗
3. Diani · Int. J. Eng. Sci. · 1995 · 33 · 192110.1016/0020-7225(95)00045-Y ↗
4. Stringfellow · Acta Metall. Mater. · 1992 · 40 · 170310.1016/0956-7151(92)90114-T ↗
5. Greenwood · Proc. R. Soc. Lond. · 1965 · 283A · 40310.1098/rspa.1965.0029 ↗
6. Zwigl · Metall. Mater. Trans. · 1998 · 29 · 56510.1007/s11661-998-0138-6 ↗
7. Gautier · Acta Metall. · 1987 · 35 · 136710.1016/0001-6160(87)90019-8 ↗
8. T.G. Nieh, J. Wadsworth, O.D. Sherby, Superplasticity in Metals and Ceramics, Cambridge, 1997.10.1017/CBO9780511525230 ↗
9. Dunand · 1997 · 1821
10. Dunand · Mater. Sci. Eng. · 1997 · 230 · 2510.1016/S0921-5093(97)00033-6 ↗
11. Frary · Metall. Mater. Trans. A · 2002 · 33 · 166910.1007/s11661-002-0176-4 ↗
12. Engel · J. Mater. Proc. Technol. · 2002 · 125 · 3510.1016/S0924-0136(02)00415-6 ↗
13. Saotome · J. Mater. Proc. Technol. · 2001 · 119 · 30710.1016/S0924-0136(01)00957-8 ↗
14. Zamora · Mech. Mater. · 1983 · 2 · 19310.1016/0167-6636(83)90014-5 ↗
15. Dunand · Acta Mater. · 1996 · 44 · 106310.1016/1359-6454(95)00224-3 ↗
16. Gonzalez · J. Mater. Eng. Perform. · 2004 · 13 · 66510.1361/10599490421268 ↗
17. Schuh · J. Mater. Res. · 2001 · 16 · 86510.1557/JMR.2001.0115 ↗
18. Frost · 1982
19. Zwigl · Acta Mater. · 1997 · 45 · 528510.1016/S1359-6454(97)00186-9 ↗
20. Zwigl · Mater. Sci. Eng. · 1999 · 262 · 16610.1016/S0921-5093(98)00991-5 ↗
21. Schuh · Philos. Magn. · 2002 · 82 · 244110.1080/01418610208240045 ↗
22. Nishihara · J. Jpn. Inst. Metals · 1977 · 41 · 18810.2320/jinstmet1952.41.2_188 ↗
23. Iguchi · J. Jpn. Inst. Metals · 1974 · 38 · 72510.2320/jinstmet1952.38.8_725 ↗