Abstract

Abstract Specimens of a directionally solidified cast of a fully lamellar TiAl alloy were tensile tested using displacement-controlled procedure. Numbers of microcracks were measured for specimens after they were subjected to various preload–unload processes. Combined with detailed fracture surface observations, the following effects of microcrack-damage on fracture behavior of TiAl alloy are proposed—(1) Volumetric effect: the apparent plastic elongation incorporates both plastic strain and the elongation caused by microcracks. (2) Volumetric effect: microcracks produced in entire specimen volume decrease the apparent elastic modulus and produce a stress-softening sector of the load–displacement curve just before final fracture. (3) Facial effect: microcracks extended on a weakest cross-section decrease and determine the fracture load.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Intermetallics and Advanced Alloy Properties · Nuclear Materials and Properties · High-Velocity Impact and Material Behavior

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (21)

Show source-provided references
1. Chan · Metall. Trans. A · 1992 · 23A · 166310.1007/BF02804362 ↗
2. Chan · Metall. Mater. Trans. · 2000 · 31A · 7110.1007/s11661-000-0054-x ↗
3. Inui · Acta Mater. · 1992 · 40 · 309510.1016/0956-7151(92)90472-Q ↗
4. Chan · Metall Mater. Trans. A · 1997 · 28A · 7910.1007/s11661-997-0084-8 ↗
5. Campbell · Scripta Mater. · 1997 · 37 · 70710.1016/S1359-6462(97)00154-1 ↗
6. Arata · Int. J. Fract. · 2001 · 111 · 16310.1023/A:1012217617235 ↗
7. Arata · Mater. Sci. Eng. A · 2002 · 329–331 · 53210.1016/S0921-5093(01)01504-0 ↗
8. Bowen · Mater. Sci. Eng. A · 1995 · 192/193A · 44310.1016/0921-5093(95)80019-0 ↗
9. Mercer · Acta Mater. · 1997 · 46 · 438510.1016/S1359-6454(97)00060-8 ↗
10. Kad · Phil. Mag. A · 1995 · 71 · 56710.1080/01418619508244469 ↗
11. Frank · Intermetallics · 2003 · 11 · 33110.1016/S0966-9795(03)00004-9 ↗
12. Halford · J. Mater. Process. Technol. · 2004 · 153–154 · 61510.1016/j.jmatprotec.2004.04.109 ↗
13. Harding · Scripta Mater. · 1999 · 40 · 44510.1016/S1359-6462(98)00466-7 ↗
14. Zheng · J. Mater. Sci. · 2004 · 39 · 172110.1023/B:JMSC.0000016176.15217.51 ↗
15. Chen · Metall. Mater. Trans. · 2004 · 35A · 43910.1007/s11661-004-0355-6 ↗
16. Chan · Acta Mater. · 2004 · 52 · 460110.1016/j.actamat.2004.06.026 ↗
17. Cao · Mater. Sci. Eng. A · 2006 · 420 · 12210.1016/j.msea.2006.01.089 ↗
18. Cao · J. Zhang, Mater. Sci. Eng. A · 2007 · 465 · 18310.1016/j.msea.2007.02.026 ↗
19. R.Cao, H. Zhu, J.H. Chen, J. Zhang, Mater. Sci. Eng. A, submitted for publication.
20. Wu · Acta Mater. · 2001 · 49 · 169310.1016/S1359-6454(01)00092-1 ↗
21. Botten · Acta Mater. · 2001 · 49 · 168710.1016/S1359-6454(01)00091-X ↗