journal article·2001-07

Failure paths of the Cu-based leadframe/EMC joints

H.Y Lee

Materials Science and Engineering: A· Volume 311· Issue 1-2
Publisher page

Abstract

Abstract Copper-based leadframe sheets were oxidized in a black-oxide forming solution and molded with epoxy molding compound (EMC) to measure the fracture toughness of leadframe/EMC interface using sandwiched double-cantilever beam (SDCB) specimens and sandwiched Brazil-nut (SBN) specimens. Results showed that the pebble-like Cu2O precipitates on the leadframe had almost no adhesion to the EMC, while the opposite was true for the acicular CuO precipitates. Under the mixed-mode loading condition, the fracture toughness increased parabolically with mode mixity. For phase angle (ψ)
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Electronic Packaging and Soldering Technologies · Material Properties and Processing · Mechanical Behavior of Composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (17)

Show source-provided references
1. Chai · 1999
2. Wong · 1998
3. Kitano · 1988
4. Ganesan · IEEE Trans. · 1993 · 16 · 940
5. Cui · 1998
6. Moon · 1998
7. Yun · J. Mater. Sci. · 1992 · 27 · 581110.1007/BF01119743 ↗
8. Evans · J. Adhesion · 1978 · 9 · 26710.1080/00218467808075120 ↗
9. Ashworth · J. Electrochem. Soc. · 1977 · 124 · 50610.1149/1.2133338 ↗
10. Strehblow · Electrochimica Acta · 1980 · 55 · 83910.1016/0013-4686(80)90036-5 ↗
11. Oh · J. Am. Ceram. Soc. · 1987 · 70 · C352
12. Atkinson · Int. J. Fract. · 1982 · 18 · 27910.1007/BF00015688 ↗
13. Suo · Mater. Sci. Eng. · 1989 · A107 · 13510.1016/0921-5093(89)90382-1 ↗
14. Wang · Acta Metall. Mater. · 1990 · 38 · 127910.1016/0956-7151(90)90200-Z ↗
15. Lee · Mater. Sci. Eng. · 2000 · A277 · 15410.1016/S0921-5093(99)00536-5 ↗
16. Liechti · J. Appl. Mech. · 1992 · 59 · 29510.1115/1.2899520 ↗
17. Evans · Acta Metall. Mater. · 1989 · 37 · 324910.1016/0001-6160(89)90197-1 ↗