journal article·1999-08

Microstructural and surface characterization of Ti–6Al–4V alloys after fretting fatigue

P.D Nicolaou, E.B Shell, T.E Matikas

Materials Science and Engineering: A· Volume 269· Issue 1-2
Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Mechanical stress and fatigue analysis · Electrical Contact Performance and Analysis · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (15)

Show source-provided references
1. Hills · 1994
2. Waterhouse · Int. Mater. Rev. · 1992 · 37 · 7710.1179/imr.1992.37.1.77 ↗
3. Sarkar · 1976
4. Bryggman · Wear · 1986 · 110 · 110.1016/0043-1648(86)90148-1 ↗
5. Hoeppner · Wear · 1981 · 70 · 15510.1016/0043-1648(81)90150-2 ↗
6. Zhou · Wear · 1995 · 181–183 · 53110.1016/0043-1648(94)07081-4 ↗
7. A.L. Hutson, T. Nicholas, Fretting fatigue of Ti–6Al–4V under flat-on-flat contact, Int. J. Fatigue (1998) submitted.10.1016/S0142-1123(99)00027-4 ↗
8. P.D. Nicolaou, T.E. Matikas, E.B. Shell, in: G.Y. Baaklini et al. (Eds.), SPIE 1999 International Symposium on Non-Destructive Evaluation Techniques for Aging Infrastructure and Manufacturing, 1999, in press.10.1016/S0921-5093(99)00138-0 ↗
9. Vingsbo · Wear · 1988 · 126 · 13110.1016/0043-1648(88)90134-2 ↗
10. Blanchard · Metall. Trans. A · 1991 · 22A · 153510.1007/BF02667367 ↗
11. Fayeulle · STLE Tribol. Trans. · 1993 · 36 · 26710.1080/10402009308983158 ↗
12. Lebedeva · Wear · 1991 · 148 · 20310.1016/0043-1648(91)90284-2 ↗
13. Bethune · Wear · 1965 · 8 · 2210.1016/0043-1648(65)90247-4 ↗
14. Fair · 1984 · 3
15. P.D. Nicolaou, T.E. Matikas, in: T.E. Matikas (Ed.), Development of Enabling Methodologies for Detection and Characterization of Early Stages of Damage in Aerospace Materials, 2nd Annual Report for DARPA-MURI, The University of Dayton, 1998, p. A18-1.