Sub-transus transformation-driven softening in Ti-6Al-2Sn-4Zr-2Mo alloy additively manufactured using laser powder bed fusion
Source abstract
Abstract
In the present work, the high-temperature phase stability and the correlated flow stress softening of Ti-6 %Al-2 %Sn-4 %Zr-2 %Mo alloy (Ti-6242) fabricated through the laser powder bed fusion process were studied. Toward this end, a set of hot compression tests were conducted at 700, 800, 900 and 1000 °C under the strain rate of 0.001s-1. A distinct observation was the occurrence of a significant strength drop and notable flow softening after reaching the maximum stress at all thermomechanical conditions. The peak stress was significantly dropped (∼490 MPa) with increasing temperature from 700 °C to 800 °C, proposing activation of a new emerging softening mechanism. The α′ martensitic starting microstructure extensively started to decompose at around 800 °C, leading to the formation of α and β grains, where the β phase fraction was considerably increased by approaching the β transus temperature. The reverse transformation of the martensite served as an effective softening mechanism, owing to the fact that the α and β phases represent higher capability for strain accommodation. At 900 °C and 1000 °C, the penetration of β phases through the α lamellae and the occurrence of α-globularization was clearly evident, contributing to the flow softening at elevated temperatures. A preferred texture towards the <2-1-10> and <0001> orientations was also recognized in the microstructure deformed at 800 °C and 900 °C, which proposed the contribution of texture weakening as an additional factor in flow softening.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Titanium Alloys Microstructure and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (33)
Show source-provided references
1. Effect of content and configuration of equiaxed α and lamellar α on deformation mechanism and tensile properties of a near-α titanium alloy10.1016/j.msea.2023.145192 ↗
2. Effect of heat-treatment on microstructure and mechanical properties of Ti alloys: an overview10.1016/j.matpr.2020.02.541 ↗
3. Enhanced strength of dual-phase Ti6242 alloy via a heterogeneous microstructure10.1016/j.matdes.2023.111972 ↗
4. Feasibility analysis of obtaining tri-modal microstructure by multi-pass conventional forging combined with dual heat treatment for near-α titanium alloy with different initial microstructures
5. Achieving an ideal combination of strength and plasticity in additive manufactured Ti–6.5 Al–2Zr–1Mo–1V alloy through the development of tri-modal microstructure10.1016/j.msea.2022.142944 ↗
6. Three-dimensional morphology of tri-modal microstructure and evolution mechanisms of constitute phases in dual heat treated near-α titanium alloy10.1016/j.matchar.2022.111761 ↗
7. Comparative analyses of the tensile and damage tolerance properties of tri-modal microstructure to widmanstätten and bimodal microstructures of TA15 titanium alloy10.1016/j.jallcom.2019.02.300 ↗
8. Pillai · 2023
9. High-temperature mechanical performance of directed energy deposited Ti6242S alloy10.1016/j.msea.2022.143526 ↗
10. An investigation on the processing conditions of Ti-6Al-2Sn-4Zr-2Mo by electron beam powder bed fusion: microstructure, defect distribution, mechanical properties and dimensional accuracy
11. Comparative study of Ti-6.5 Al-2Zr-1Mo-1V (TA15) alloy fabricated by selective laser melting and laser metal deposition10.1016/j.optlastec.2024.111052 ↗
12. Martensite decomposition during post-heat treatments and the aging response of near-α Ti–6Al–2Sn–4Zr–2Mo (Ti-6242) titanium alloy processed by selective laser melting (SLM)10.1142/S2424913020500186 ↗
13. Transformation softening in three titanium alloys10.1016/j.matdes.2016.10.039 ↗
14. Temperature sensitivity of mechanical properties and microstructure during moderate temperature deformation of selective laser melted Ti-6Al-4V alloy10.1016/j.matchar.2020.110342 ↗
15. Stress–strain behavior of a selective laser melted Ti-6Al-4V at strain rates of 0.001–1/s and temperatures 20–1000° C10.1016/j.jmatprotec.2021.117141 ↗
16. Flow softening during hot working of Ti-6Al-4V with a lamellar colony microstructure10.1016/S1359-6462(99)00061-5 ↗
17. Heat treatment effect on the microstructure and elevated temperature tensile property of the Ti6242S alloy fabricated via laser powder bed fusion10.1016/j.jallcom.2022.166656 ↗
18. Effect of annealing temperature on microstructure and high-temperature tensile behaviour of Ti-6242S alloy produced by laser powder bed fusion10.1080/26889277.2021.1997341 ↗
19. Comparing the cold, warm, and hot deformation flow behavior of selective laser‐melted and electron‐beam‐melted Ti–6Al–2Sn–4Zr–2Mo alloy10.1002/adem.202301046 ↗
20. Standard practice for compression tests of metallic materials at elevated temperatures with conventional or rapid heating rates and strain rates
21. Effects of direct aging on near-alpha Ti–6Al–2Sn–4Zr–2Mo (Ti-6242) titanium alloy fabricated by selective laser melting (SLM)10.1016/j.msea.2020.139533 ↗
22. Selective laser melting of a near‐α Ti6242S alloy for high‐performance automotive parts10.1002/adem.202001194 ↗
23. Critical strain for dynamic recrystallization in variable strain rate hot deformation10.2355/isijinternational.43.692 ↗
24. High-temperature flow characterization and microstructural evolution of Ti6242 alloy: yield drop phenomenon10.1016/j.msea.2016.07.043 ↗
25. Effect of cyclic heat treatment on microstructure and mechanical properties of laser aided additive manufacturing Ti–6Al–2Sn–4Zr–2Mo alloy10.1016/j.apmate.2021.09.002 ↗
26. Compressive/Tensile deformation behavior and the correlated microstructure evolution of Ti–6Al–4V titanium alloy at warm temperatures10.1016/j.jmrt.2020.12.110 ↗
27. On the warm temperature strain accommodation mechanisms of Ti–6Al–4V alloy holding different starting microstructures10.1016/j.jmrt.2021.06.077 ↗
28. Tailoring the microstructure and mechanical property of laser powder bed fusion fabricated Ti–6Al–2Sn–4Zr–2Mo via heat treatment10.1016/j.jallcom.2021.162648 ↗
29. 2004
30. Effect of heat treatment on the crystallographic orientation evolution in a near-α titanium alloy Ti6010.1016/j.actamat.2017.04.007 ↗
31. Crystal orientation, crystallographic texture and phase evolution in the Ti–45Al–2Cr–5Nb alloy processed by selective laser melting10.1016/j.matchar.2016.01.012 ↗
32. Comparatively evaluating the room and high temperature mechanical properties of AlSi10Mg alloy produced by selective laser melting10.1016/j.jmrt.2022.10.162 ↗
33. Flow softening and recrystallization accompanied flow in AZ61 magnesium alloy during thermomechanical processing10.1016/j.heliyon.2024.e37625 ↗