journal article·2019-09

Microstructure and cracking behavior of hydroxide films formed on aluminum-alloy sheets prepared by steam coating

Hongmei Li, Naoki Takata, Makoto Kobashi, Ai Serizawa

Publisher page

Abstract

Abstract To elucidate the adhesion properties of anticorrosion hydroxide films formed on aluminum (Al)-alloy sheets prepared by the steam coating process, cracks that propagated inside the hydroxide film formed on Al–Mg–Si alloy (6061 grade) sheets were characterized. Continuous hydroxide films with different thicknesses of 0.7 μm and 1.4 μm formed at different temperatures of 180 °C and 200 °C, respectively. Microstructural characterizations revealed that these hydroxide films exhibited a dual-layer structure consisting of a polycrystalline γ-AlO(OH) layer (on the surface side) and a continuous amorphous layer (on the Al-alloy side). Bending tests caused numerous cracks inside the hydroxide films under tension and compression. On the tensile-strained surface, numerous vertical cracks penetrated through the hydroxide films, although their delamination was not observed. On the compressive-strained surface, local delamination of the upper γ-AlO(OH) layer occurred. However, cracks were not observed in the lower amorphous layer on the Al-alloy substrate deformed under compression. These results indicate that the dual-layer-structured hydroxide film prepared by steam coating exhibits remarkable adhesion to the Al-alloy substrate.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · Advanced ceramic materials synthesis · Metal and Thin Film Mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (31)

Show source-provided references
1. Variability in the tensile properties of squeeze-cast Al–Si–Cu–Mg alloy10.1016/j.msea.2007.11.014 ↗
2. A calorimetric study of precipitation in commercial aluminum alloy 606110.1007/BF00719697 ↗
3. Pre-precipitate clusters and precipitation processes in Al–Mg–Si alloy
4. The precipitation sequence in Al–Mg–Si alloys10.1016/S1359-6454(98)00059-7 ↗
5. Low-temperature oxidation10.1007/BF00603582 ↗
6. Theory of the oxidation of metals10.1088/0034-4885/12/1/308 ↗
7. The thickness of native oxides on aluminum alloys and single crystals10.1016/j.apsusc.2015.05.043 ↗
8. Microelectrochemical investigation of anodic oxide formation on the aluminum alloy AA202410.1016/j.electacta.2017.07.160 ↗
9. Salt spray corrosion and electrochemical corrosion properties of anodic oxide film on 7475 aluminum alloy10.1016/j.jallcom.2015.01.175 ↗
10. Electrodeposition of Ni-La2O3 composite on AA6061 alloy and its enhanced hardness, corrosion resistance and thermal stability10.1016/j.surfcoat.2017.06.011 ↗
11. Influence of surface pretreatments on the quality of trivalent chromium process coatings on aluminum alloy10.1016/j.apsusc.2017.06.246 ↗
12. Influence of prior corrosion on the high cycle fatigue behavior of microarc oxidation coated 6061-T6 aluminum alloy10.1016/j.ijfatigue.2011.03.016 ↗
13. Effect of micro arc oxidation coatings on corrosion resistance of 6061-Al alloy10.1007/s11665-008-9222-8 ↗
14. Increasing thickness and protective properties of PEO-coatings on aluminum alloy10.1016/j.surfcoat.2017.11.025 ↗
15. Corrosion resistance of Mg–Al layered double hydroxide container-containing magnesium hydroxide films formed directly on magnesium alloy by chemical-free steam coating10.1039/c3ta11015j ↗
16. Corrosion resistance of Mg(OH)2/Mg–Al layered double hydroxide composite film formed directly on combustion-resistant magnesium alloy AMCa602 by steam coating10.1016/j.corsci.2014.11.031 ↗
17. Formation mechanism of Mg-Al layered double hydroxide-containing magnesium hydroxide films prepared on Ca-added flame-resistant magnesium alloy by steam coating10.1016/j.surfcoat.2017.08.060 ↗
18. Formation of anticorrosive film for suppressing pitting corrosion on Al-Mg-Si alloy by steam coating10.3390/coatings8010023 ↗
19. ASM Handbook · 1991 · vol. 4 · 846
20. FIB preparation and STEM observation of specified area from two direction10.1017/S1431927605508353 ↗
21. Crystal structure of beta-Al4.5FeSi10.1107/S0108768193013096 ↗
22. Structure of some aluminium- iron- magnesium- manganese-silicon alloys
23. ASM Handbook · 2004 · vol. 9 · 748
24. Mechanism of aluminum hydroxide layer formation by surface modification of aluminum10.1016/j.apsusc.2010.01.011 ↗
25. Use of boehmite films for corrosion protection of aluminum10.5006/0010-9312-18.4.143 ↗
26. Anodizing of aluminum covered with hydroxide
27. The cracking and decohesion of thin films on ductile substrates10.1016/0001-6160(89)90018-7 ↗
28. Fracture mechanics analysis of coating/substrate systems10.1016/S0013-7944(99)00141-1 ↗
29. Crack spacing in brittle films on elastic substrates10.1111/j.1151-2916.1990.tb05290.x ↗
30. Cracking of thin films bonded to elastic plastic substrates10.1016/0022-5096(96)00042-7 ↗
31. Fracture toughness evaluation of thin Fe-Al intermetallic compound layer at reactive interface between dissimilar metals10.2320/matertrans.M2012425 ↗