Complete recovery of high temperature oxidation resistance in carbon fiber reinforced SiC composites by a recoating repair methodology
Source abstract
Abstract
Abstract The current work reports on the oxidation behavior and residual flexural strength of carbon fiber–reinforced silicon carbide composites (C/SiC) after induction of thermal crack damage by heat treatment (HT) at 1900 °C and the effect, therein, of a repair process involving recoating by SiC. As-prepared, heat-treated and heat-treated/recoated specimens, were subjected to static oxidation tests in air at a temperature range of 500–1500 °C for 10 h and then tested in three-point bending. It was found that composite weight of heat-treated samples decreased dramatically with increasing oxidation temperature with weight loss values of ~30% being systematically observed for oxidation temperatures above 800 °C. On the other hand, as-prepared and heat-treated/SiC-recoated specimens reached almost their original weight after oxidation. The residual flexural strength of C/SiC composites with thermally-induced crack damage decreased significantly compared to as-prepared specimens, while SiC recoating was found to efficiently enable strength enhancement. Microstructural analysis showed that HT was associated with increased population and dimensions of micro-cracks on the C/SiC surface while SiC recoating enabled repair of HT-induced thermal crack damage hence leading to oxidation resistance recovery of the material.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (13)
Show source-provided references
1. Naslain · Compos. Sci. Technol. · 2004 · 64 · 15510.1016/S0266-3538(03)00230-6 ↗
2. Schmidt · Acta Astronaut. · 2004 · 55 · 40910.1016/j.actaastro.2004.05.052 ↗
3. Cheng · Carbon · 2000 · 38 · 210310.1016/S0008-6223(00)00068-3 ↗
4. Yin · Compos. Sci. Technol. · 2001 · 61 · 97710.1016/S0266-3538(00)00190-1 ↗
5. Mei · Carbon · 2010 · 48 · 300710.1016/j.carbon.2010.01.056 ↗
6. Zhang · J. Am. Ceram. Soc. · 2008 · 91 · 29110.1111/j.1551-2916.2007.02007.x ↗
7. Luan · Compos. Sci. Technol. · 2010 · 70 · 67810.1016/j.compscitech.2009.12.025 ↗
8. Halbig · J. Am. Ceram. Soc. · 2008 · 91 · 51910.1111/j.1551-2916.2007.02170.x ↗
9. Mei · Carbon · 2013 · 54 · 4210.1016/j.carbon.2012.11.001 ↗
10. Dong · 2007
11. R.J. Archacki Jr., H.I. Ringermacher, W.A. Veronesi, Nondestructive Testing: Transient Depth Thermography, US Patent 5711603A, 1998.
12. Naslain · J. Mater. Sci. · 2004 · 39 · 730310.1023/B:JMSC.0000048745.18938.d5 ↗
13. Konstantinos · Compos. Interface · 2012 · 19 · 52310.1080/15685543.2012.762730 ↗