Abstract

The enhanced strength-ductility synergy of Al12Si alloy manufactured via laser powder bed fusion (LPBF) was obtained through compositional regulation and post-fabrication plastic deformation. Microstructural characterizations showed that the typical synergy of multiple crystallised defects in brittle Si eutectic phase, including stacking faults (SFs), ultrafine nanotwins and 9R structure, co-contribute to the superb elongation of 23.7 % with the ultimate tensile strength of 189 MPa in as-LPBFed Al12Si alloy after hot-rolling deformation with a reduction rate of 70 %. In tandem with a trace of Mn and Fe additions, the UTS increases to 240 MPa with the El of 19.1 % under the same condition. Such an excellent strength-ductility synergy is mainly attributed to the formation of ultrafine α-Al12(Fe,Mn)3Si particles. This work offers a new perspective on the modification Al–Si alloys with the desired mechanical properties via LPBF and hot-rolling.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Additive Manufacturing and 3D Printing Technologies

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (41)

Show source-provided references
1. Achieving ultrahigh fatigue resistance in AlSi10Mg alloy by additive manufacturing10.1038/s41563-023-01651-9 ↗
2. High-strength Al-5Mg2Si-2Mg-2Fe alloy with extremely high Fe content for green industrial application through additive manufacturing, Virtual
3. From crack-prone to crack-free: eliminating cracks in additive manufacturing of high-strength Mg2Si-modified Al-Mg-Si alloys10.1016/j.jmst.2024.04.009 ↗
4. Additive manufacturing enabled synergetic strengthening of bimodal reinforcing particles for aluminum matrix composites
5. 3D printing of aluminium alloys: additive manufacturing of aluminium alloys using selective laser melting10.1016/j.pmatsci.2019.100578 ↗
6. A review of laser powder bed fusion additive manufacturing of aluminium alloys: microstructure and properties
7. Precipitation behavior and strengthening-toughening mechanism of additive friction stir-deposited Al-Mg-Si-Cu alloy
8. A high Fe-containing AlSi12 alloy fabricated by laser powder bed fusion10.1016/j.jmrt.2022.04.008 ↗
9. Laser powder-bed-fusion of Si3N4 reinforced AlSi10Mg composites: processing, mechanical properties and strengthening mechanisms10.1016/j.msea.2021.141874 ↗
10. Anomalous strengthening by supersaturated solid solutions of selectively laser melted Al–Si-based alloys
11. A selective laser melting and solution heat treatment refined Al–12Si alloy with a controllable ultrafine eutectic microstructure and 25% tensile ductility10.1016/j.actamat.2015.05.017 ↗
12. Effect of heat treatment on the microstructure and mechanical properties of an Al-5Mg2Si-2Mg alloy processed by laser powder bed fusion
13. Developing a high-strength Al-Mg-Si-Sc-Zr alloy for selective laser melting: crack-inhibiting and multiple strengthening mechanisms10.1016/j.actamat.2020.03.060 ↗
14. Overcoming the strength-ductility trade-off in additively manufactured AlSi10Mg alloy by ECAP processing10.1016/j.jallcom.2022.165817 ↗
15. Evaluation of the stress-strain relationship of constituent phases in AlSi10Mg alloy produced by selective laser melting using crystal plasticity FEM10.1016/j.jallcom.2017.04.264 ↗
16. Effect of eutectic Si on surface nanocrystallization of Al–Si alloys by surface mechanical attrition treatment10.1016/j.msea.2011.09.090 ↗
17. High temperature thermal and mechanical stability of high-strength nanotwinned Al alloys
18. Deformation twinning in nanocrystalline aluminum10.1126/science.1083727 ↗
19. Ultrastrong and ductile (CoCrNi)94Ti3Al3 medium-entropy alloys via introducing multi-scale heterogeneous structures10.1016/j.jmst.2022.06.048 ↗
20. Exceptional strength-ductility synergy of additively manufactured CoCrNi medium-entropy alloy achieved by lattice defects in heterogeneous microstructures10.1016/j.jmst.2022.03.024 ↗
21. Effects of intensive forced melt convection on the mechanical properties of Fe containing Al–Si based alloys10.1016/j.msea.2006.09.038 ↗
22. Enhancement in strength and thermal stability of selective laser melted Al–12Si by introducing titanium nanoparticles10.1016/j.msea.2022.143833 ↗
23. Simultaneous enhancements of strength and toughness in an Al-12Si alloy synthesized using selective laser melting10.1016/j.actamat.2016.06.009 ↗
24. Defining the tensile properties of Al-12Si parts produced by selective laser melting10.1016/j.actamat.2016.12.044 ↗
25. High as-cast strength die-cast AlSi9Cu2Mg alloy prepared by nanoparticle strengthening with industrially acceptable ductility10.1016/j.jallcom.2020.156873 ↗
26. On microstructure and work hardening behavior of laser powder bed fused Al-Cu-Mg-Ag-TiB2 and AlSi10Mg alloys
27. Review on the correlation between microstructure and mechanical performance for laser powder bed fusion AlSi10Mg
28. Additive manufactured versus cast AlSi10Mg Alloy: microstructure and micromechanics10.1016/j.rinma.2021.100178 ↗
29. Strengthening CoCrNi medium-entropy alloy by tuning lattice defects10.1016/j.scriptamat.2020.07.027 ↗
30. High strength-ductility Co23Cr23Ni23Mn31 medium-entropy alloy achieved via defect engineering
31. Heterogeneous precipitation behavior and stacking-fault-mediated deformation in a CoCrNi-based medium-entropy alloy10.1016/j.actamat.2017.07.029 ↗
32. Perspective on hetero-deformation induced (HDI) hardening and back stress10.1080/21663831.2019.1616331 ↗
33. The influences of temperature and microstructure on the tensile properties of a CoCrFeMnNi high-entropy alloy10.1016/j.actamat.2013.06.018 ↗
34. Effects of temperature on mechanical properties and deformation mechanisms of the equiatomic CrFeNi medium-entropy alloy10.1016/j.actamat.2020.11.012 ↗
35. Strengthening materials by engineering coherent internal boundaries at the nanoscale10.1126/science.1159610 ↗
36. Work hardening of polycrystalline Cu with nanoscale twins10.1016/j.scriptamat.2011.12.046 ↗
37. Dislocation structures of Σ3 {112} twin boundaries in face centered cubic metals
38. Mechanisms for nucleation and propagation of incoherent twins in a CoCrFeNiMo0.15 high-entropy alloy subject to cold rolling and annealing10.1016/j.intermet.2018.03.005 ↗
39. Structure characterization of special boundaries in Fe47Mn30Co10Cr10B3 dual-phase high-entropy alloy10.1016/j.jallcom.2020.157642 ↗
40. Interfacial nanophases stabilize nanotwins in high-entropy alloys10.1016/j.actamat.2019.12.010 ↗
41. Evaluation of the stress-strain relationship of constituent phases in AlSi10Mg alloy produced by selective laser melting using crystal plasticity FEM10.1016/j.jallcom.2017.04.264 ↗