The analysis of internal stresses on a welded joint in Grade 91 steel under creep test loading: Synchrotron X-ray diffraction measurements and modelling

Solenne Collomb, Xiaolei Chen, Jean-Philippe Tinnes, Thomas Schenk, Olivier Ferry, Svetlana Tsareva, Abdelkrim Redjaïmia, Alain Jacques

Abstract

The analysis and understanding of creep damage of Grade 91 steel welded joints is an important topic in the energy industry. Creep tests on welded joints were carried out at 600 • C, 100 MPa and then interrupted at 0%, 10%, 30%, 50%, 80% of the expected life and after failure. Creep damage is characterised by cavity bands located exclusively in the core of the sample in the InterCritical Heat Affected Zone (ICHAZ). These samples were tested using in situ synchrotron X-ray Diffraction (XRD) along the welded joint under creep conditions for the different creep times. The experimental results show a significant evolution of strain and creep damage characteristics on the welded joint, with a local maximum at the Heat Affected Zone (HAZ). Subsequently, a finite element creep strain analysis was performed for comparison with the experimental results.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: High Temperature Alloys and Creep · Microstructure and Mechanical Properties of Steels · Fatigue and fracture mechanics

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (19)

Show source-provided references
1. Recent advances in creep-resistant steels for power plant applications10.1007/BF02706455 ↗
2. Long term creep behaviour of welded joints of P91 steel at 650° C10.1016/j.msea.2012.10.013 ↗
3. Creep damage evaluation of 9Cr–1Mo–V–Nb steel welded joints showing Type IV fracture10.1016/j.ijpvp.2005.09.004 ↗
4. Evaluation of creep damage in heat affected zone of thick welded joint for Mod.9Cr–1Mo steel10.1016/j.ijpvp.2009.04.008 ↗
5. Evaluation of the creep cavitation behavior in Grade 91 steels10.1016/j.ijpvp.2016.02.018 ↗
6. Damage characterization of a P91 steel weldment under uniaxial and multiaxial creep10.1016/j.msea.2008.04.124 ↗
7. Creep fracture mechanism in welded joints of P91 steel10.1179/1743284713Y.0000000233 ↗
8. Damage assessment method of P91 steel welded tube under internal pressure creep based on void growth simulation10.1016/j.ijpvp.2010.08.009 ↗
9. The significance of weldment material mis-matching on stress redistribution and creep cracking of high temperature components10.1080/09603409.1998.11689607 ↗
10. Modelling high temperature creep flow, damage and fracture behaviour of 9Cr1Mo–NbV steel weldments10.3184/096034008X356998 ↗
11. Mechanical testing device for in situ experiments on reversibility of dislocation motion in silicon10.1016/S0168-583X(02)01698-1 ↗
12. PyFAI, a versatile library for azimuthal regrouping
13. Geandier · 2002
14. He · 2009
15. Quantitative texture analysis of small domains with synchrotron radiation X-rays10.1107/S0021889899004999 ↗
16. X-ray diffraction Debye Ring Analysis for STress measurement (DRAST): a new method to evaluate residual stresses10.1016/j.actamat.2003.09.041 ↗
17. Analysis of the creep behaviour of modified P91 (9Cr–1Mo–NbV) welds10.1016/S0261-3069(02)00026-2 ↗
18. Continuum damage mechanics modelling incorporating stress triaxiality effect on ductile damage initiation10.1111/ffe.13220 ↗
19. Characterization of welded joint in martensitic steel Grade 91 after interrupted creep test at 600 ° C10.1016/j.msea.2022.143851 ↗