journal article·2018-12

Low-temperature consolidation of high-strength TiB2 ceramic composites via grain-boundary engineering using Ni-W alloy

Zdeněk Chlup, Ľuboš Bača, Hynek Hadraba, Ivo Kuběna, Pavla Roupcová, Zuzana Kováčová

Publisher page

Abstract

Abstract The concept of the consolidation of titanium diboride at relatively low temperature via formation of the solid solution was used in this research. A specially designed Ni-W alloy prepared by mechanical alloying method was used as the solid solution formation additive. The low amount of Ni-W alloy and TiB2 powder were mixed together and consequently consolidated in the temperature interval from 1300 °C to 1400 °C. The development of the microstructure and resulting mechanical behaviour of these composites were analysed in detail. The grain size of TiB2 below 3 micrometres was obtained for all processing temperatures. The highest processing temperature of 1400 °C resulted in the flexural strength on the level of 875 MPa and the elastic modulus being nearly 500 GPa. The fracture toughness was about 5 MPa m0.5. Formation of the solid solution was confirmed by XRD and TEM analysis. Due to the targeted change in chemical composition on grain boundaries and TiB2 lattice distortions by addition of transition metals with higher ionic radii a hypothesis about the preferential formation of solid solution layer on the surface of TiB2 grains taking into account their orientation was formulated.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced materials and composites · Aluminum Alloys Composites Properties · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (49)

Show source-provided references
1. Basu · 2011
2. Pressureless sintering of titanium diboride with nickel, nickel boride, and iron additives10.1111/j.1151-2916.1997.tb03227.x ↗
3. Simultaneous densification and phase decomposition of TiB2–WB2 solid solutions activated by cobalt boride addition10.1016/j.jeurceramsoc.2006.05.084 ↗
4. Pressureless sintering of TiB2-based ceramics with Ti–Fe additives: sintering mechanism and stability in liquid aluminum10.1002/adem.201200067 ↗
5. High temperature strength of TiB2 ceramics10.2109/jcersj.101.1074 ↗
6. Preparation and mechanical properties of TiB2 composites containing Ni and C10.2109/jcersj.99.78 ↗
7. Pressureless sintering and properties of titanium diboride ceramics containing chromium and iron10.1111/j.1151-2916.2001.tb00763.x ↗
8. Pressureless sintering of TiB2 with low concentration of Co binder to achieve enhanced mechanical properties10.1016/j.msea.2018.02.068 ↗
9. Densification and mechanical properties of titanium diboride with silicon nitride as a sintering aid10.1111/j.1151-2916.1999.tb02199.x ↗
10. High-strength TiB 2–TaC ceramic composites prepared using reactive spark plasma consolidation10.1016/j.ceramint.2015.09.065 ↗
11. Effects of ZrO2 Addition on the Mechanical Properties ofTiB2 HIP'ed Compacts
12. Microstructure and sintering mechanism of TiB2-ZrO2-SiC composite10.2109/jcersj.100.392 ↗
13. Effects of SiC addition on the mechanical properties and sinterability of TiB2-(2mol% Y2O3-ZrO2) composite10.2109/jcersj.100.691 ↗
14. Microstructure evolution and tribological properties of TiB2/Ni–Ta cermets10.1016/j.jeurceramsoc.2011.10.039 ↗
15. Effect of metallic dopants on the microstructure and mechanical properties of TiB210.1016/j.jeurceramsoc.2015.03.027 ↗
16. P. Franke, D. Neuschütz, Binary Systems. Part 4: Binary Systems from Mn-Mo to Y-Zr·Ni-W: Datasheet from Landolt-Börnstein – Group IV Physical Chemistry, Volume 19B4: "Binary Systems. Part 4: Binary Systems from Mn-Mo to Y-Zr", SpringerMaterials, Springer-Verlag Berlin Heidelberg 〈http://dx.doi.org/10.1007/10757285_38〉.10.1007/10757285_38 ↗
17. "EN 843-2," Advanced technical ceramics – Mechanical properties of monolithic ceramics at room temperature – Part 2: Determination of Young’s modulus, shear modulus and Poisson’s ratio, 2006.
18. "EN 843-1," Advanced technical ceramics. Mechanical properties of monolithic ceramics at room temperature. Determination of flexural strength, 2007.
19. Slice synthesis of a three dimensional “work of fracture” specimen10.1016/0013-7944(75)90059-4 ↗
20. The use of chevron-notched specimens for fracture-toughness determination of bearing steels
21. "EN 14425-3," Advanced technical ceramics – test methods for determination of fracture toughness of monolithic ceramics – Part 3: Chevron notched beam (CNB) method, 2010.
22. The Fe–Ni system: Thermodynamic modelling assisted by atomistic calculations10.1016/j.intermet.2010.02.026 ↗
23. A statistical approach to estimate the 3D size distribution of spheres from 2D size distributions10.1130/B25000.1 ↗
24. Influence of hot pressing sintering temperature and time on microstructure and mechanical properties of TiB2 ceramics10.1016/S0955-2219(01)00424-1 ↗
25. TEM characterization of dislocations in TiB2 particles after hypervelocity impact10.1016/j.micron.2014.06.007 ↗
26. Arrangement of dislocation networks in hot-pressed titanium diboride10.1016/0956-716X(95)00014-M ↗
27. Tensile deformation and microstructure of a nanocrystalline Ni–W alloy produced by electrodeposition10.1016/j.scriptamat.2003.09.056 ↗
28. On modifications of the well-known Hume-Rothery rules: amorphous alloys as model systems10.1016/j.jnoncrysol.2007.01.052 ↗
29. Atomic-size effect and solid solubility of multicomponent alloys10.1016/j.scriptamat.2014.09.010 ↗
30. XI. atomic and ionic radii.—II. Application to the theory of solid solubility in alloys10.1080/14786443808562109 ↗
31. Influences of binders on the mechanical properties of TiB2-TaB2 based cermets10.2497/jjspm.28.264 ↗
32. Solid solubility effect on properties of titanium diboride10.1111/j.1151-2916.1987.tb05630.x ↗
33. Mechanical properties of TiB2-CoB-metal boride alloys
34. Ceramic fracture during ballistic impact
35. Tough ceramics by microwave sintering of nanocrystalline titanium diboride ceramics10.1016/j.ceramint.2013.07.010 ↗
36. Densification and grain growth during microwave sintering of titanium diboride10.1016/j.scriptamat.2013.07.012 ↗
37. Temperature dependent hardness and strength properties of TiB2 with TiSi2 sinter-aid10.1016/j.jeurceramsoc.2008.11.018 ↗
38. Sintering and properties of titanium diboride made from powder synthesized in a plasma-arc heater10.1111/j.1151-2916.1984.tb19744.x ↗
39. Strength and toughness: the challenging case of TaC-based composites10.1016/j.compositesb.2014.11.043 ↗
40. Sintering and mechanical properties of titanium diboride with aluminum nitride as a sintering aid10.1016/S0955-2219(01)00403-4 ↗
41. Effect of residual nickel content on the grain size dependent mechanical properties of TiB210.1007/BF01672048 ↗
42. Strengthening and toughening of boride and carbide hard material composites10.1016/0025-5416(88)90485-5 ↗
43. Material properties of titanium diboride10.6028/jres.105.057 ↗
44. Rice · 2000
45. Densification behavior and mechanical properties of the spark plasma sintered monolithic TiB2 ceramics10.1016/j.msea.2010.05.086 ↗
46. Low-temperature densification of TiB2 ceramic by the spark plasma sintering process with Ti as a sintering aid10.1016/j.scriptamat.2011.10.030 ↗
47. Microstructure and mechanical properties of hot pressed submicron TiB2 powders10.1016/j.ceramint.2018.02.153 ↗
48. Effect of ZrB2 and SiC addition on TiB2-based ceramic composites prepared by spark plasma sintering10.1016/j.ijrmhm.2014.05.019 ↗
49. The deformation and ageing of mild steel: III discussion of results10.1088/0370-1301/64/9/303 ↗