journal article·2016-04

Low weight steel-magnesium composites achieved by powder compaction

Julien Nguyen, Frédéric Douville, Olivier Bouaziz, Xavier Sauvage

Publisher page

Abstract

Abstract Low weight steel-magnesium composites with various volume fractions of Mg were achieved by a multi-step co-extrusion process. Hollow tubes filed with Mg powders were extruded, annealed, cut and restacked in hollow tubes before subsequent extrusion. This way, fully dense composites with various architectures and length scales were achieved. Microstructure observations revealed that both phases undergo an axisymmetric deformation in the early stage of the process. At higher extrusion ratio, Mg/Fe interfaces become wavy and irregular which is attributed to a strong crystallographic texture. In the as-extruded states, the composites exhibit peculiar elastic to plastic transition with an unusually high strain hardening. Tensile tests performed after annealing prove that this behavior is directly linked to large internal stresses.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Aluminum Alloys Composites Properties · Magnesium Alloys: Properties and Applications · Microstructure and mechanical properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (31)

Show source-provided references
1. Deformation of sandwich sheet materials in uniaxial tension10.1007/BF02686411 ↗
2. Processing, microstructure and properties of a Mg/Al bimetal macrocomposite10.1177/0021998308098369 ↗
3. Solidification processed Mg/Al bimetal macrocomposite: microstructure and mechanical properties10.1016/j.jallcom.2007.07.050 ↗
4. Improving compressive failure strain and work of fracture of magnesium by integrating it with millimeter length scale aluminum10.1177/0021998308092198 ↗
5. Effects of intermetallic phases on the bond strength of diffusion-bonded joints between titanium and 304 stainless steel using nickel interlayer10.1007/s11661-007-9273-8 ↗
6. Ductibilty enhancement in AZ31 magnesium alloy by controlling its grain structure10.1016/S1359-6462(01)00996-4 ↗
7. Massalski · 1996 · 1
8. Deformation processed metal–metal composites10.1002/(SICI)1527-2648(200002)2:1/2<11::AID-ADEM11>3.0.CO;2-Z ↗
9. The room temperature ductility of fine grain magnesium
10. Metallic composites processed via extreme deformation: towards the limits of strength in bulk Materials10.1557/mrs2010.703 ↗
11. Steel-magnesium composite wire obtained by repeated co-extrusion
12. A new processing technique for copper-graphite multifilamentary nanocomposite wire: microstructures and electrical properties10.1016/j.jmatprotec.2006.06.019 ↗
13. Nanostructured multifilamentary carbon-copper composites: fabrication, microstructural characterization, and properties
14. Established and emerging materials for use as high-field magnet conductors10.1002/adem.200400014 ↗
15. Evidence of internal Bauschinger test in nanocomposite wires during in situ macroscopic tensile cycling under synchrotron beam10.1063/1.2748325 ↗
16. Ultra-high strength in situ composites formed by large plastic straining: structure and mechanical properties modelling
17. Microstructural Changes during deformation of [011] fiber-textured metals
18. Solid state amorphization in cold drawn Cu/Nb wires10.1016/S1359-6454(00)00338-4 ↗
19. Atomic scale characterization of deformation-induced interfacial mixing in a Cu/V nanocomposite wire10.1016/j.scriptamat.2009.06.007 ↗
20. A new criterion for elasto-plastic transition in nanomaterials: application to size and composite effects on Cu–Nb nanocomposite wires10.1016/j.actamat.2009.03.021 ↗
21. Kainer · 2006
22. The structure and properties of drawn pearlite10.1016/0001-6160(66)90296-3 ↗
23. Thermal stability and mechanical properties of ultrafine grained low carbon steel10.1016/S0921-5093(00)01220-X ↗
24. Novel ultra-high straining process for bulk materials-development of the accumulative roll-bonding (ARB) process10.1016/S1359-6454(98)00365-6 ↗
25. Influence of residual stresses in the performance of cold-drawn pearlitic wires10.1023/B:JMSC.0000031470.31354.b5 ↗
26. Properties of severe plastically deformed Mg alloys10.1016/j.msea.2005.04.035 ↗
27. Twinning and the ductility of magnesium alloys Part I: “Tension” twins10.1016/j.msea.2006.12.037 ↗
28. Transition of deformation behavior in an ultrafine grained magnesium alloy10.1016/j.msea.2012.04.017 ↗
29. The deformation and ageing of mild steel10.1088/0370-1301/64/6/305 ↗
30. Dynamic strain ageing as a strengthening mechanism10.1016/0025-5416(72)90070-5 ↗
31. On the effect of Lüders bands on the bending of steel tubes. Part I: experiments10.1016/j.ijsolstr.2011.06.024 ↗