journal article·2006-10

Localized corrosion of Alloy C22 nuclear waste canister material under limiting conditions

S.G. Lee, A.A. Solomon

Materials Science and Engineering: A· Volume 434· Issue 1-2
Publisher page

Abstract

Abstract Localized corrosion behavior of Alloy C22 in simulated Yucca Mountain (YM) repository environments was studied at the highest achievable but realistic temperatures under boiling and dripping scenarios. Temperatures measured in concentrated boiling solutions of KCl and NaNO3 were found to be stable at 140 °C, although transient boiling before dryout was observed at temperatures as high as 160 °C, as the electrolyte became progressively more concentrated. Experiments that simulated a dripping scenario with simulated J13 well water confirmed the existence of concentrated solutions stable at 142 ± 3 °C under controlled drip conditions leading to pit initiation in Alloy C22 after only a few hours. The polarization experiments conducted at 140 °C in a solution with 0.5 mol L−1 chloride concentration showed that the critical potential for localized corrosion was 250 mV (versus Ag/AgCl). Potentiostatic tests confirmed that active metal dissolution occurred only in the crevice region at this potential. The crevice corrosion of Alloy C22 required an incubation time to develop a critical crevice solution, and it was triggered by severe local chemistry (enrichment of Cl− and H+) aided by the high temperature.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Nuclear Materials and Properties · Corrosion Behavior and Inhibition

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (29)

Show source-provided references
1. CRWMS M&O 2000, General Corrosion and Localized Corrosion of Waste Package Outer Barrier, ANL-EBS-MD-000003 REV 00, 2000.
2. CRWMS M&O 2001, MIS-MGR-RL-000001 REV 00, 2001.
3. CRWMS M&O 2002, Peer Review of the Waste Package Material Performance, Final Report, February 28, 2002.
4. CRWMS 2003, DE-AC28-01RW12101, 2003.
5. CRWMS M&O 2000, ANL-EBS-MD-000001 REV 00, 2000.
6. Hynes International, HASTELLOY C-22 ALLOY, H-2019E.
7. Rousseau · Am. Scientist · 1992 · 80 · 54
8. NRC BULLETIN 2002-01, Reactor Pressure Vessel Head Degradation and Reactor Coolant Pressure Boundary Integrity, March 18, 2002.
9. NRC INFORMATION NOTICE 2004-21, Additional Adverse Effect of Boric Acid Leakage: Potential Impact on Postaccident Coolant pH, November 24, 2004.
10. Magar · Corrosion · 1976 · 32 · 37410.5006/0010-9312-32.9.374 ↗
11. Indig · Corrosion · 1990 · 46 · 68010.5006/1.3585168 ↗
12. Kehler · Corrosion · 2001 · 57 · 104210.5006/1.3281677 ↗
13. Streicher · Corrosion · 1963 · 19 · 272t10.5006/0010-9312-19.8.272 ↗
14. Streicher · Corrosion · 1976 · 32 · 7910.5006/0010-9312-32.3.79 ↗
15. J.R. Scully, J.L. Hudson, T. Lunt, B. Kehler, Charlottesville, University of Virginia, TIC: 246630, Virginia, 1999, p. 1.
16. Heubner · Corrosion · 1989 · 45 · 24910.5006/1.3577851 ↗
17. Pawel · Corrosion · 1993 · 49 · 92910.5006/1.3316019 ↗
18. D.C. Agarwal et al., http://www.corrosionlab.com/papers/alloy-rad-waste.htm.
19. Priyantha · J. Electroanal. Chem. · 2004 · 572 · 40910.1016/j.jelechem.2004.06.031 ↗
20. Macdonald · J. Electroanal. Chem. · 2004 · 572 · 42110.1016/j.jelechem.2004.05.032 ↗
21. Ilevbare · Corros. Sci. · 2001 · 43 · 48510.1016/S0010-938X(00)00086-X ↗
22. Virtanen · Corros. Sci. · 2001 · 43 · 116510.1016/S0010-938X(00)00121-9 ↗
23. Zhao · Corros. Sci. · 2002 · 44 · 211910.1016/S0010-938X(02)00017-3 ↗
24. Jain · 1985 · 337
25. K.A. Gruss, G.A. Cragnolino, D. Dunn, N. Sridhar, Corrosion 98, Paper No. 149, 1998.
26. Lloyd · J. Electrochem. Soc. · 2003 · 150 · B12010.1149/1.1554914 ↗
27. Pickering · J. Electrochem. Soc. · 2003 · 150 · k110.1149/1.1565142 ↗
28. Shaw · Corros. Sci. · 1991 · 32 · 70710.1016/0010-938X(91)90085-4 ↗
29. Newman · Corrosion · 2001 · 57 · 103010.5006/1.3281676 ↗