Failure mechanisms in cobalt welded with a silver–copper filler
Source abstract
Abstract
Abstract Cobalt silver–copper (Co–AgCu) weldments approximate the stresses and failure mechanisms of beryllium aluminum–silicon (Be–AlSi) welds, which have strategic importance but are hazardous to study. Failure tests of these surrogate Co–AgCu welds, examined in tension and four-point bending, show that residual stresses and post-welding heat treatment have little or no effect on strength, whereas weld quality and geometry are extremely important. Scanning electron microscopy images reveal abundant defects in poor welds, which usually fail through propagation of preexisting cracks. Fracture surfaces show a variety of morphologies, ranging from dimples in the AgCu filler, to cleavage steps in the CoCu peritectic, and suspected intergranular fracture in the cobalt base. Spatially resolved acoustic spectroscopy reveals significant changes in microstructure near the base–filler interface, whereas wavelength dispersive analysis shows high Cu concentrations in this area.. Contrary to finite element predictions, these welds were found to be stronger during face bending than root bending, likely resulting from the increased number of cracks and imperfections in the Co base. These computations correctly predict that weld strength depends on geometry and that welds fail either in the cobalt base, or along the base–filler interface. Crack compliance measurements show that the largest residual stresses are located along this interface. However, these stresses are unlikely to influence failure due to their direction, whereas stresses in the weld root are too small to have observable effects on failure. The strength of Co–AgCu welds depends strongly on geometry, penetration, and weld quality, but little on residual stresses, and this conclusion is tentatively extended to Be–AlSi welds.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced Welding Techniques Analysis · Aluminum Alloys Composites Properties · Microstructure and mechanical properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (35)
Show source-provided references
1. Braze welding of cobalt with a silver–copper filler10.1016/j.jmrt.2014.11.002 ↗
2. Introduction to beryllium: uses, regulatory history and disease10.1080/10473220119088 ↗
3. 2003
4. ASM specialty handbook · 2000
5. Cobalt Monograph, Center D’Information du Cobalt, Brussels, 1960.
6. Cobalt Facts, Cobalt Development Institute, 2013.
7. K.B. Shedd, Minerals Yearbook, Cobalt (advance release) 2011, United States Geological Survey, 2013.
8. Campbell · 1996
9. Laser welding of a cobalt–chromium removable partial denture alloy10.1016/S0022-3913(98)70239-2 ↗
10. The tensile and shear strength of a base metal weld joint used in dentistry10.1177/00220345810600021101 ↗
11. 1998
12. E.R. Buchanan, An overview of hardfaced coatings for industrial use, in: Proceedings of the Third International Pump Symposium, College Station, Texas, May 1986 pp. 91–96
13. Stellite as a wear-resistant material10.1016/0041-2678(70)90058-8 ↗
14. Roth · 1994
15. Untracht · 1985
16. 2001
17. Donachie · 2002
18. Levy · 1994
19. Laughton · 2003
20. Cobalt-base high-temperature alloys10.1126/science.1121738 ↗
21. Alloying effects in polycrystalline γ' strengthened Co–Al–W base alloys10.1016/j.intermet.2013.10.022 ↗
22. Some expressions for the strain energy in a finite volume surrounding the root of blunt V-notches10.1007/s10704-005-3943-6 ↗
23. A review of the volume-based strain energy density approach applied to V-notches and welded structures10.1016/j.tafmec.2009.10.001 ↗
24. Recent developments in brittle and quasi-brittle failure assessment of engineering materials by means of local approaches10.1016/j.mser.2013.11.001 ↗
25. Spatially resolved acoustic spectroscopy for rapid imaging of material microstructure and grain orientation10.1088/0957-0233/25/5/055902 ↗
26. Determination of crystallographic orientation of large grain metals with surface acoustic waves10.1121/1.4731226 ↗
27. The effect of thermomechanical pretreatment on the allotropic transformation in cobalt10.1007/BF02666203 ↗
28. Casti Metals Blue Book · 2003
29. Standard Test Method for Guided Bend Test for Ductility of Welds, Designation: E190-92, ASTM International, 2008.
30. Citzaf-a package of correction programs for the quantitative electron microbeam X-ray analysis of thick polished materials, thin films, and particles
31. Bulk metastable cobalt in fcc crystal structure10.1016/j.jallcom.2013.05.115 ↗
32. Microstructural evolution and mechanical properties of a two-phase Cu–Ag alloy processed by high-pressure torsion to ultrahigh strains10.1016/j.actamat.2011.01.017 ↗
33. The slitting method10.1002/9781118402832.ch4 ↗
34. M.B. Prime, Experimental Procedure for Crack Compliance (Slitting) Measurements of Residual Stress, LA-UR-03-8629, Los Alamos National Laboratory, 2003.
35. Co-Cu (cobalt–copper)