Investigation of precipitation and tensile properties of 7B04 under direct current and aging
Source abstract
Abstract
Abstract The mechanical properties and ageing precipitation behavior of 7B04 aluminum alloy aged with direct current (DC) intensity of 0–400 A at 110–130 °C were investigated by tensile test, conductivity measurement, scanning electron microscope (SEM), differential scanning calorimetry (DSC) and field emission spherical aberration correction transmission electron microscope (STEM). The conductivity, tensile strength and elongation of peak aged alloy with DC were all higher than those of peak aged alloy without DC. With increasing ageing temperature from 110 °C to 130 °C, the DC intensity that required for achieving peak strength reduced from 200 A to 100 A. The enthalpy value of the endothermic peak, the size and area fraction of GP zones, and η′ of peak aged alloy increased with the increase of DC intensity. The alloy aged with DC intensity of 100 A at 120 °C for 12 h had the highest tensile strength and favorable ductility.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Microstructure and mechanical properties · Electromagnetic Effects on Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (33)
Show source-provided references
1. Modification of solidification structure by pulse electric discharging10.1016/0956-716X(94)90465-0 ↗
2. Electroplasticity in metals and ceramics10.1016/S0921-5093(00)00786-3 ↗
3. The mechanical behavior of 5052-H32 aluminum alloys under a pulsed electric current10.1016/j.ijplas.2014.02.002 ↗
4. Effect of traveling magnetic field on separation and purification of Si from Al–Si melt during solidification10.1016/j.jcrysgro.2015.08.015 ↗
5. Phase distribution and phase structure control through a high gradient magnetic field during the solidification process10.1016/j.matdes.2008.03.012 ↗
6. Electric current effects upon the Sn/Cu and Sn/Ni interfacial reactions10.1007/s11664-998-0068-5 ↗
7. Annealing behavior of cold rolled aluminum alloy in a high magnetic field10.1016/j.scriptamat.2006.02.033 ↗
8. Magnetically enhanced recrystallization in an aluminum alloy10.1016/j.scriptamat.2006.08.018 ↗
9. Evolution of secondary phases and properties of 7B04 aluminum alloy during DC homogenization10.1016/S1003-6326(16)64122-5 ↗
10. Effects of D.C. current on the phase transformation in 7055 alloy during homogenization10.1016/j.matchar.2014.07.017 ↗
11. Structure and properties of alloys under the influence of electric field10.1007/BF00774754 ↗
12. External electric field applied during solution heat treatment of the Al-Mg-Si alloy AA602210.1023/B:JMSC.0000044886.66798.95 ↗
13. Effect of an electric field during solution treatment of 2091 Al-Li alloy10.1007/BF00240796 ↗
14. Effects of electric pulse current on the aging kinetics of 2219 aluminum alloy
15. Precipitation behavior of Al-Cu-Mg alloy during electric field-assisted aging10.1007/s11665-012-0212-5 ↗
16. Effect of current on fatigue life of 60Sn-40Pb solder10.1016/0956-716X(92)90697-D ↗
17. Microstructure and electric conductivity of Cu-Cr-Zr alloy aged with dc electric current10.1016/j.jallcom.2008.03.054 ↗
18. An electric current homogenization device and method for aluminum
19. A differential scanning calorimetry investigation of the effects zinc and copper on solid state reactions in Al-Zn-Mg-Cu alloys10.1016/0921-5093(91)90369-X ↗
20. The influence of zirconium on the early stages of aging of a ternary Al-Zn-Mg alloys10.1016/0956-7151(94)90406-5 ↗
21. Influence of predeformation and ageing in an Al-Zn-Mg alloy -I. Microstructure evolution and mechanical properties10.1016/S1359-6454(98)00293-6 ↗
22. Effect of processing way and aging treatment on properties and microstructures of 7B04 aluminum alloy10.1016/S1003-6326(08)60095-3 ↗
23. Characterization and modeling of precipitation kinetics in an Al-Zn-Mg alloy10.1016/S0921-5093(00)01247-8 ↗
24. GP zones in Al-Zn-Mg alloys and their role in artificial aging10.1016/S1359-6454(01)00251-8 ↗
25. Guinier-Preston zones in a high-purity Al-Zn-Mg alloy10.1080/09500839408240966 ↗
26. Secondary ageing in aluminium alloy 705010.1016/j.msea.2008.02.039 ↗
27. Early-stage precipitation in Al-Zn-Mg-Cu alloy (7050)10.1016/j.actamat.2004.06.025 ↗
28. The effect of direct electric current on precipitation in a bulk Al-4wt%Cu alloy10.1007/BF00542295 ↗
29. Effect of electric current on solid state phase transformations in metals10.1016/S0921-5093(00)00780-2 ↗
30. Electric current effects on Sn/Ag interfacial reactions10.1007/s11664-999-0217-5 ↗
31. Effects of current density on electropulsing-induced phase transformations in a Zn-Al based alloy10.1007/s00339-009-5100-y ↗
32. Conrad · 1989
33. Dislocations faster than the speed of sound10.1126/science.283.5404.965 ↗