Evaluation of the active mechanism for acidic SCC induced mechanical degradation: A methodological approach

T. De Seranno, T. Depover, A.R.D. Verliefde, K. Verbeken

Publisher page

Abstract

Abstract This work evaluates the mechanical degradation of Dual Phase steel due to acidic stress-corrosion cracking (SCC). The SCC susceptibility is studied by in-situ constant extension rate testing, followed by post-mortem fractographic evaluation, while the corrosion rate is determined by electrochemical measurements. Elevating the temperature results in a decrease in both strength and ductility. Organic acids addition further leads to a significant ductility loss, whereas oxygen removal yields a ductility gain. The corrosion rate shows a linear relationship with the H+ concentration. Between a pH of 4.2–7, anodic dissolution occurs, whereas hydrogen absorption takes place at lower pH, causing hydrogen-assisted stress-corrosion cracks.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Concrete Corrosion and Durability

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (95)

Show source-provided references
1. Steam turbine failure at hinkley point ‘A10.1243/PIME_PROC_1972_186_037_02 ↗
2. Low-pressure steam turbine disc cracking—an update10.1243/PIME_PROC_1985_199_007_02 ↗
3. Stress corrosion cracking of turbine disc steels: a study of mechanism, Electricité de France: direction Des Etudes et Recherches
4. Steam turbine operating conditions, chemistry of condensates, and environment assisted cracking – a critical review
5. Steam turbine corrosion and deposits problems and solutions
6. 2011
7. 2015
8. Ambasta · 2006
9. Dooley · Caustic Gouging, PowerPlant Chemistry · 2010 · 12 · 188
10. Stress corrosion cracking characterization of 3.5 NiCrMoV low pressure turbine rotor steels in NaOH and NaCI solutions10.5006/1.3580827 ↗
11. Twenty year experience in controlling corrosion in amine unit of badak LNG plant
12. Corrosion and materials selection for amine service
13. Carbonate SCC experiences in unusual locations
14. Alkaline carbonate SCC failures at a refinery10.1007/s11668-018-0391-y ↗
15. Mechanism of chloride stress corrosion cracking of austenitic stainless steels10.5006/0010-9312-25.11.462 ↗
16. The effect of chloride ions on stress corrosion cracking of type 304 and type 316 austenitic stainless steels in sulfuric acid solution10.1016/0010-938X(93)90023-A ↗
17. Effects of dissolved hydrogen and elastic and plastic deformation on active dissolution of pipeline steel in anaerobic groundwater of near-neutral pH10.1016/j.actamat.2008.08.035 ↗
18. Effect of CO2 and R-ratio on near-neutral pH stress corrosion cracking initiation under a disbonded coating of pipeline steel10.1016/j.corsci.2011.03.017 ↗
19. An experimental investigation of corrosion of X100 pipeline steel under uniaxial elastic stress in a near-neutral pH solution10.1016/j.corsci.2012.02.022 ↗
20. Effect of hydrogen-induced plasticity on the stress corrosion cracking of X70 pipeline steel in simulated soil environments10.1016/j.msea.2016.02.019 ↗
21. Hazards and threats to a pipeline system
22. Transgranular stress corrosion cracking of high-pressure pipelines in contact with solutions of near neutral pH10.5006/1.3294348 ↗
23. Mechanisms of high-pH and near-neutral-pH SCC of underground pipelines10.1115/1.1376716 ↗
24. Hydrogen-facilitated anodic dissolution-type stress corrosion cracking of pipeline steels in near-neutral pH solution10.5006/1.3283971 ↗
25. Thermodynamically modeling the interactions of hydrogen, stress and anodic dissolution at crack-tip during near-neutral pH SCC in pipelines10.1007/s10853-006-1375-y ↗
26. Local environment under simulated disbonded coating on steel pipelines in soil solution10.1016/j.corsci.2008.01.004 ↗
27. Micro-electrochemical characterization of corrosion of welded X70 pipeline steel in near-neutral pH solution10.1016/j.corsci.2009.04.030 ↗
28. 2004
29. Monitoring of first condensate corrosion (FCC) in industrial steam systems
30. Early condensate in a fossil power plant using organic treatment
31. Investigations into the composition of the water phase in steam turbines
32. Organic impurities and organic conditioning agents in the steam/water cycle: a power plant manufacturer's point of view
33. Palmer · 2008
34. 2013
35. Organic acid formation in steam–water cycles: influence of temperature, retention time, heating rate and O210.1016/j.applthermaleng.2014.01.019 ↗
36. Effects of temperature and pressure on the thermolysis of morpholine, ethanolamine, cyclohexylamine, dimethylamine, and 3-methoxypropylamine in superheated steam10.1021/ie504849v ↗
37. Organic matter composition more important than concentration in ion exchange demineralization of different water qualities for the production of steam10.1021/acs.iecr.7b05059 ↗
38. Organic matter and microbial cell density behavior during ion exchange demineralization of surface water for boiler feedwater10.1021/acs.iecr.9b02512 ↗
39. Latest advances in the understanding of acid dewpoint corrosion: corrosion and stress corrosion cracking in combustion gas condensates10.1108/00035590410533129 ↗
40. Stress corrosion cracking of a low alloy steel in high purity steam10.1016/S0010-938X(75)80029-1 ↗
41. Mechanical and metallurgical properties of retired 3.5NiCrMoV low pressure steam turbine discs10.1007/BF02833449 ↗
42. Prediction of failures of low-pressure steam turbine disks10.1115/1.2842321 ↗
43. Troubleshooting turbine steam path damage mechanisms
44. Dynamic tensile characteristics of TRIP-type and DP-type steel sheets for an auto-body10.1016/j.ijmecsci.2007.09.004 ↗
45. The influence of temperatures and strain rates on the mechanical behavior of dual phase steel in different conditions10.1016/j.jmrt.2014.11.001 ↗
46. Fractographic analysis of the role of hydrogen diffusion on the hydrogen embrittlement susceptibility of DP steel10.1016/j.msea.2015.09.124 ↗
47. Liu · 2017
48. Strain rate sensitivity of microstructural damage evolution in a dual-phase steel pre-charged with hydrogen10.1016/j.prostr.2018.12.118 ↗
49. An overview of dual-phase steels: advances in microstructure-oriented processing and micromechanically guided design10.1146/annurev-matsci-070214-021103 ↗
50. Mechanical degradation of Fe-C-X steels by acidic stress-corrosion cracking10.1016/j.corsci.2020.108509 ↗
51. Wastewater reclamation, recycling and reuse: past, present, and future10.2166/wst.1996.0656 ↗
52. Characterization of isolated fractions of dissolved organic matter from natural waters and a wastewater effluent10.1016/S0043-1354(00)00350-X ↗
53. The environmental benefits of water recycling and reuse10.2166/ws.2003.0041 ↗
54. 2017
55. Effect of hydrogen charging on the mechanical properties of advanced high strength steels10.1016/j.ijhydene.2013.12.190 ↗
56. Dependence of mechanical properties of high strength steel S690 on elevated temperatures10.1016/j.conbuildmat.2011.12.018 ↗
57. Effect of temperature on strength and elastic modulus of high-strength steel10.1061/(ASCE)MT.1943-5533.0000600 ↗
58. Temperature-dependent mechanical properties of an austenitic–ferritic stainless steel studied by in situ tensile loading in a scanning electron microscope (SEM)10.1016/j.msea.2013.04.060 ↗
59. Mechanical properties and design recommendations of very high strength steel S960 in fire10.1016/j.engstruct.2016.01.008 ↗
60. Environmental effects on the stress corrosion cracking susceptibility of 3.5NiCrMoV steels in high temperature water10.1016/j.corsci.2004.09.022 ↗
61. Conrad · 1963
62. Dislocation mechanics aspects of plastic instability and shear banding10.1016/0167-6636(94)90069-8 ↗
63. Meyers · 2009
64. Mechanical properties
65. Dislocation velocities, dislocation densities, and plastic flow in lithium fluoride crystals10.1063/1.1735121 ↗
66. Stress relaxation and the use of the johnston-gilman equation in the analysis of thermally activated flow10.1016/0036-9748(69)90206-3 ↗
67. The effect of acetic acid on the stress corrosion cracking of 3.5NiCrMoV turbine steels in high temperature water10.1016/j.corsci.2008.04.023 ↗
68. Strain rate dependence of tensile strength and ductility of nano and ultrafine grained coppers10.1016/j.msea.2017.11.083 ↗
69. 1993
70. Effect of pH and chloride concentration on the corrosion of duplex stainless steel
71. Electrolytic dissolution of binary alloys containing a noble metal10.1149/1.2426709 ↗
72. 1992
73. In-situ transmission electron microscopic observation of corrosion-enhanced dislocation emission and crack initiation of stress corrosion10.5006/1.3280556 ↗
74. Stress corrosion cracking (SCC) and hydrogen-assisted cracking in titanium alloys
75. Mechanistic and fractographic aspects of stress-corrosion cracking (SCC)
76. A new model for hydrogen-assisted cracking (hydrogen “embrittlement”)10.1007/BF02642048 ↗
77. Direct observations of enhanced dislocation mobility due to hydrogen10.1016/0036-9748(81)90249-0 ↗
78. An HVEM study of hydrogen effects on the deformation and fracture of nickel10.1016/0001-6160(86)90071-4 ↗
79. Hydrogen-enhanced localized plasticity—a mechanism for hydrogen-related fracture10.1016/0921-5093(94)90975-X ↗
80. Influence of hydrogen on the stacking-fault energy of an austenitic stainless steel10.4028/www.scientific.net/MSF.207-209.93 ↗
81. Hydrogen effects on the interaction between dislocations10.1016/S1359-6454(97)00349-2 ↗
82. The effects of hydrogen on the deformation and fracture of b-titanium10.1016/S1359-6454(01)00301-9 ↗
83. Hyun · 2012
84. Microstructural characterization of hydrogen induced cracking in TRIP-assisted steel by EBSD10.1016/j.matchar.2015.12.017 ↗
85. The detrimental effect of hydrogen at dislocations on the hydrogen embrittlement susceptibility of Fe-C-X alloys: an experimental proof of the HELP mechanism10.1016/j.ijhydene.2017.12.109 ↗
86. The effect of occluded hydrogen on the tensile strength of iron
87. A mechanistic theory of hydrogen embrittlement of steels10.1002/bbpc.19720760864 ↗
88. Equilibrium aspects of hydrogen-induced cracking of steels10.1016/0001-6160(74)90061-3 ↗
89. Hydrogen-induced cracking (HIC) of hardened and tempered steel fastener used in space application10.1007/s11668-009-9277-3 ↗
90. Hydrogen embrittlement (HE) phenomena and mechanisms
91. Hydrogen embrittlement susceptibility of a weld simulated X70 heat affected zone under H2 pressure10.1016/j.msea.2013.12.042 ↗
92. Numerical analysis of hydrogen transport near a blunting crack tip10.1016/0022-5096(89)90002-1 ↗
93. Determination of hydrogen diffusion parameters of ferritic steel from electrochemical permeation measurement under tensile loads10.1149/2.1021412jes ↗
94. The effect of hydrostatic stress on the hydrogen induced mechanical degradation of dual phase steel: a combined experimental and numerical approach10.1016/j.engfracmech.2019.106704 ↗
95. Influence of sample geometry and microstructure on the hydrogen induced cracking characteristics under uniaxial load10.1016/j.msea.2017.02.094 ↗