Cyclic deformation behavior in pure Cu with growth-in twins
Source abstract
Abstract
A polycrystalline pure copper sample with high density of growth-in twins was synthesized by means of electro-deposition technique. Symmetrical push-pull cyclic deformation was performed at constant axial plastic strain amplitude in the range of 1.1 x 10(-4) < epsilon(pl) <= 3.9 x 10(-3). At low strain amplitudes (epsilon(pl) = 1.1 x 10(-4) 2.1 x 10(-4)), the initial cyclic hardening of Cu sample was found to be similar to that of single crystal Cu, and secondary softening was found. At higher strain amplitudes (epsilon(pl) = 1.0 x 10(-3), 1.8 x 10(-3)), cyclic stress reached the saturation rapidly, neither secondary softening nor secondary hardening was found. Investigations of dislocation configurations show that twin boundaries play a crucial role in the plastic deformation at higher strain amplitudes for Cu. A special wall structure, i.e. persistent slip bands (PSB)-like structure, was found inside the twin lamellae, which may induce the saturation cyclic behavior in Cu. (c) 2005 Elsevier B.V. All rights reserved.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Microstructure and mechanical properties · Aluminum Alloys Composites Properties · Metal and Thin Film Mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (32)
Show source-provided references
1. Watanabe · J. Phys. · 1988 · 49 · 507
2. Watanabe · Mater. Forum. · 1988 · 11 · 284
3. Christian · Prog. Mater. Sci. · 1995 · 39 · 110.1016/0079-6425(94)00007-7 ↗
4. Paidar · Acta Metall. · 1986 · 34 · 227710.1016/0001-6160(86)90173-2 ↗
5. Lu · Science · 2004 · 16 · 42210.1126/science.1092905 ↗
6. Shen · Scri. Mater. · 2005 · 52 · 98910.1016/j.scriptamat.2005.01.033 ↗
7. Zhang · Acta Mater. · 2004 · 52 · 99510.1016/j.actamat.2003.10.033 ↗
8. Wang · J. Mater. Sci. Technol. · 1999 · 15 · 48910.1179/026708399101506643 ↗
9. Zhang · Mater. Sci. Eng. · 1999 · A 272 · 41010.1016/S0921-5093(99)00508-0 ↗
10. Heinz · Acta Metall. Mater. · 1990 · 38 · 193310.1016/0956-7151(90)90305-Z ↗
11. Sahin · Acta Metall. Mater. · 1991 · 39 · 244510.1016/0956-7151(91)90024-U ↗
12. Llanes · Mater. Sci. Eng. A · 1992 · 157 · 2110.1016/0921-5093(92)90094-H ↗
13. Wang · Metall. Trans. A · 1985 · 16 · 87310.1007/BF02814838 ↗
14. Gopalan · Mater. Sci. Eng. A · 1991 · 142 · 1110.1016/0921-5093(91)90749-D ↗
15. Llanes · Acta Metall. Mater. · 1993 · 41 · 266710.1016/0956-7151(93)90136-G ↗
16. Llanes · Mater. Sci. Eng. A · 1993 · 161 · 110.1016/0921-5093(93)90469-U ↗
17. Luoh · Mater. Sci. Eng. A · 1998 · 256 · 1810.1016/S0921-5093(98)00812-0 ↗
18. Form · Metal Sci. · 1980 · 1 · 1610.1179/030634580790438190 ↗
19. Abrams · Metallography · 1971 · 4 · 5910.1016/0026-0800(71)90005-X ↗
20. Polák · Mater. Sci. Eng. A · 1992 · 151 · 1910.1016/0921-5093(92)90177-3 ↗
21. Feltner · Acta Metall. · 1967 · 15 · 163310.1016/0001-6160(67)90138-1 ↗
22. Liu · Acta Metall. Mater. · 1994 · 42 · 163110.1016/0956-7151(94)90372-7 ↗
23. Mughrabi · Mater. Sci. Eng. · 1978 · 33 · 20710.1016/0025-5416(78)90174-X ↗
24. Polák · Mater. Sci. Eng. · 1990 · 63 · 18910.1016/0025-5416(84)90120-4 ↗
25. Basinski · Acta Mater. · 1980 · 28 · 19110.1016/0001-6160(80)90068-1 ↗
26. Rémy · Metall. Trans. A · 1981 · 12 · 38710.1007/BF02648536 ↗
27. Li · Trans. TMS-AIME · 1963 · 227 · 239
28. Li · Mater. Sci. Eng. A · 1999 · 269 · 16610.1016/S0921-5093(99)00154-9 ↗
29. Abel · Mater. Sci. Eng. · 1978 · 36 · 11710.1016/0025-5416(78)90201-X ↗
30. Polák · Mater. Sci. Eng. A · 1990 · 132 · 6710.1016/0921-5093(91)90362-Q ↗
31. Li · Phil. Mag. A · 2002 · 82 · 86710.1080/01418610208240007 ↗
32. Li · Phil. Mag. · 2004 · 84 · 332310.1080/14786430412331283055 ↗