Joining of SiC with Si infiltrated tape-cast TiB2–C interlayer: Effect of interlayer composition and thickness on the microstructure and mechanical properties
Source abstract
Abstract
Abstract Tape-cast TiB 2 –C interlayers with different compositions and thickness were used to bond SiC ceramics via reactive Si infiltration at 1450 °C in vacuum. This method result in strong bonding of SiC bodies by the formation of a dense TiB 2 –SiC–Si composite interlayer. Resultant SiC joints show homogeneous phase distribution within the interlayer while heterogeneous one at the interface. The grain growth behavior of reaction formed SiC and TiB 2 grains was observed and discussed in terms of the tape composition and the infiltration process. Average bending strength of SiC joints was measured to be from 360 MPa to 420 MPa and these joints usually fracture from SiC substrate.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties · Advanced materials and composites
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (21)
Show source-provided references
1. Meetham · J. Mater. Sci. · 1991 · 26 · 85310.1007/BF00576759 ↗
2. Cooke · J. Am. Ceram. Soc. · 1991 · 74 · 295910.1111/j.1151-2916.1991.tb04289.x ↗
3. Casady · Solid-State Electron. · 1996 · 39 · 140910.1016/0038-1101(96)00045-7 ↗
4. Heuer · J. Am. Ceram. Soc. · 1990 · 73 · 278910.1111/j.1151-2916.1990.tb06677.x ↗
5. Popper · 1960
6. P.P. Popper, Production of Dense Bodies of Silicon Carbide, U.S. Patent, 1966 p. 275.
7. K.M. Taylor, Cold molded dense silicon carbide articles and methods of making the same, U.S. Patent, 1965, p. 205.
8. Forrest · 1972
9. Chiang · Mater. Sci. Eng. A · 1991 · 144 · 6310.1016/0921-5093(91)90210-E ↗
10. Chakrabarti · Ceram. Int. · 1994 · 20 · 28310.1016/0272-8842(94)90042-6 ↗
11. Munro · J. Res. Natl. Inst. Stand. Technol. · 2000 · 105 · 70910.6028/jres.105.057 ↗
12. De Mestral · J. Mater. Sci. · 1991 · 26 · 554710.1007/BF02403957 ↗
13. Zhang · Ceram. Int. · 1996 · 22 · 14310.1016/0272-8842(95)00070-4 ↗
14. Tampieri · J. Mater. Sci. · 1993 · 28 · 64910.1007/BF01151240 ↗
15. Tian · J. Alloys Compd. · 2011 · 509 · 181910.1016/j.jallcom.2010.10.053 ↗
16. Panasyuk · Powder Metall. Met. Ceram. · 1979 · 18 · 48710.1007/BF00797254 ↗
17. Nikolopoulos · J. Mater. Sci. · 1992 · 27 · 13910.1007/BF02403656 ↗
18. Li · Mater. Lett. · 2008 · 62 · 313510.1016/j.matlet.2008.02.024 ↗
19. Einarsrud · J. Am. Ceram. Soc. · 1997 · 80 · 301310.1111/j.1151-2916.1997.tb03227.x ↗
20. Venkateswaran · J. Eur. Ceram. Soc. · 2006 · 26 · 243110.1016/j.jeurceramsoc.2005.05.011 ↗
21. Kondo · J. Ceram. Soc. Jpn. · 2010 · 118 · 910.2109/jcersj2.118.9 ↗