Abstract Hydrogen embrittlement behavior of four heats of alloy 725 (H1, H2, H3, and H4) were characterized by measuring the crack growth rate response over a range of cathodic potentials. Significant grain boundary precipitation in two heats (H1 and H3) may have contributed to higher susceptibility, as evidenced by higher values of crack growth rate. The crack growth rate increased with increasing twin fraction. The crack morphology exhibited evidence of intergranular as well as slip band cracking. The crack growth rate response of the two heats that were less susceptible (H2 and H4) were evaluated in more detail over a range of applied potentials and stress intensity factors. Evidence of nano void formation at the intersection of dislocation slip bands, and grain boundaries suggests that hydrogen stabilized vacancies may play a role in the crack growth mechanism. Crack growth rate exhibited a strong response with applied potential varying by as much as 100 times in the potential range of −1050mV SCE to −850mV SCE. Over the range of K values evaluated, the crack growth rate increased by a factor of 3to 30 with applied K depending on the applied potential. The crack growth rate was related to the water adsorption on fresh metal surfaces of alloy 725 in the anticipated crack tip conditions. A crack tip strain rate based approach was applied to model the measured crack growth response.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Fatigue and fracture mechanics · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (74)
Show source-provided references
1. Hydrogen stress cracking of nickel alloy UNS N07725 — Part II: correlation between microstructure and hydrogen stress cracking resistance of Ni-Cr-Mo-Nb age hardened alloys
2. Hydrogen stress cracking of nickel alloy UNS N07725 — Part I: a field failure investigation and potential impact on future quality control
3. Hydrogen embrittlement failure of a precipitation hardened nickel alloy subsurface safety valve component installed in a North Sea seawater injection well
4. Effect of microstructure and processing on the hydrogen embrittlement of Ni-base superalloys
5. Environmentally assisted cracking of high strength nickel based alloys in HPHT applications
6. UNS N07725 nickel alloy connection failure
7. Foroni · 2018 · 193
8. Hydrogen embrittlement susceptibility of precipitation hardened Ni-alloys
9. High strength fasteners for subsea applications
10. Environmentally assisted cracking evaluation of a large UNS N07725 forging under cathodic protection conditions10.5006/0010-9312-68.5.449 ↗
11. The relationship between crack-tip strain and subcritical cracking thresholds for steels in high-pressure hydrogen gas10.1007/s11661-012-1400-5 ↗
12. Environmentally assisted cracking of high strength nickel based alloys
13. Environmentally assisted cracking of high strength nickel based alloys under cathodic protection
14. Measurement and modeling of hydrogen environment-assisted cracking in Monel K-50010.1007/s11661-014-2324-z ↗
15. Crystallographic character of grain boundaries resistant to hydrogen-assisted fracture in Ni-base alloy 72510.1038/s41467-018-05549-y ↗
16. The dual role of coherent twin boundaries in hydrogen embrittlement10.1038/ncomms7164 ↗
17. Grain-boundary engineering markedly reduces susceptibility to intergranular hydrogen embrittlement in metallic materials10.1016/j.actamat.2009.05.012 ↗
18. H. Hu, M. Zhao, S. Chen, and L. Rong, "Effect of grain boundary character distribution on hydrogen embrittlement in Fe–Ni based alloy," Mater. Sci. Eng., A, p. 139201, 2020/03/06/2020.10.1016/j.msea.2020.139201 ↗
19. 2015
20. Andresen · 1998
21. Bruemmer · 2011 · vol. 1
22. Bruemmer · 2012 · vol. 2
23. 2013
24. Hydrogen embrittlement of low alloy steels under cathodic polarization10.5006/3240 ↗
25. R. Thodla, A. Chandra, X. Li, C. D. Taylor, H. Ke, and N. Sridhar, "Hydrogen embrittlement of 718 under cathodic polarization," Corrosion Sci., vol. 165, p. 108361, 2020/04/01/2020.10.1016/j.corsci.2019.108361 ↗
26. Measurement of hydrogen embrittlement resistance of alloys 718 and custom age 625 Plus® using the rising step load technique
27. Hydrogen embrittlement study of three heats of UNS N07718 in subsea applications
28. Hydrogen-assisted failure in Ni-based superalloy 718 studied under in situ hydrogen charging: the role of localized deformation in crack propagation10.1016/j.actamat.2017.02.059 ↗
29. In-situ observation of hydrogen induced crack initiation in a nickel-based superalloy10.1016/j.scriptamat.2017.07.006 ↗
30. Hydrogen assisted crack initiation and propagation in a nickel-based superalloy10.1016/j.actamat.2016.05.003 ↗
31. Development of a novel test method to characterize material properties in corrosive environments for subsea HPHT design10.1115/1.4043512 ↗
32. Hydrogen-induced ductility loss of precipitation-strengthened Fe-Ni-Cr-based superalloy10.1016/j.msea.2018.10.040 ↗
33. Hydrogen-induced cracking behavior of twin boundary in γ′ phase strengthened Fe–Ni based austenitic alloys10.1016/j.msea.2012.10.069 ↗
34. Pronounced transition of crack initiation and propagation modes in the hydrogen-related failure of a Ni-based superalloy 718 under internal and external hydrogen conditions10.1016/j.corsci.2019.108186 ↗
35. First-principles investigation of hydrogen trapping and diffusion at grain boundaries in nickel10.1016/j.actamat.2015.07.031 ↗
36. Chemomechanical origin of hydrogen trapping at grain boundaries in fcc metals10.1103/PhysRevLett.116.075502 ↗
37. Atomistic study of hydrogen embrittlement of grain boundaries in nickel: I. Fracture10.1016/j.jmps.2017.01.020 ↗
38. Hydrogen embrittlement of steels: vacancy induced damage and nano-voiding mechanisms10.5006/2224 ↗
39. The effect of strain on the trapping of hydrogen at grain-boundary carbides in Ni-Cr-Fe alloys10.1007/s11661-001-0268-6 ↗
40. Evidence that carbide precipitation produces hydrogen traps in Ni-17Cr-8Fe alloys10.1016/S1359-6462(96)00440-X ↗
41. Dynamic deformation of hydrogen charged austenitic-ferritic steels: hydrogen trapping mechanisms, and simulations10.1016/j.jallcom.2017.10.142 ↗
42. Evaluation of hydrogen trapping mechanisms during performance of different hydrogen fugacity in a lean duplex stainless steel10.1016/j.jallcom.2015.07.029 ↗
43. Hydrogen transport in nickel-base alloys10.1007/BF02663432 ↗
44. Hydrogen diffusion and trapping in a precipitation-hardened nickel–copper–aluminum alloy Monel K-500 (UNS N05500)10.1016/j.actamat.2013.02.007 ↗
45. Hydrogen trapping phenomena in metals with B.C.C. and F.C.C. crystals structures by the desorption thermal analysis technique10.1016/0257-8972(86)90087-3 ↗
46. Deuterium concentration profiles in Fe-Ni-Co alloys electrochemically charged at room temperature10.1016/0001-6160(89)90286-1 ↗
47. The interaction mechanism of screw dislocations with coherent twin boundaries in different face-centred cubic metals10.1016/j.scriptamat.2005.11.072 ↗
48. Interactions between non-screw lattice dislocations and coherent twin boundaries in face-centered cubic metals10.1016/j.actamat.2007.11.020 ↗
49. Dislocation dynamics in a nickel-based superalloy via in-situ transmission scanning electron microscopy10.1016/j.actamat.2018.12.061 ↗
50. A combined grain scale elastic–plastic criterion for identification of fatigue crack initiation sites in a twin containing polycrystalline nickel-base superalloy10.1016/j.actamat.2015.09.050 ↗
51. Hydrogen embrittlement in nickel, visited by first principles modeling, cohesive zone simulation and nanomechanical testing10.1016/j.ijhydene.2015.06.069 ↗
52. Role of grain boundary character on oxygen and hydrogen segregation-induced embrittlement in polycrystalline Ni10.1007/s10853-016-0389-3 ↗
53. Hydrogen-induced intergranular failure in nickel revisited10.1016/j.actamat.2012.01.040 ↗
54. Experimental determination of the electrochemistry in corrosion fatigue cracks in structural steel in artificial seawater10.5006/1.3582026 ↗
55. Cathodic protection of crevices in BS 4360 50D structural steel in 3.5% NaCl and in seawater
56. The influence of strain on hydrogen entry and transport in a high strength steel in sodium chloride solution10.1149/1.2095978 ↗
57. Technical note: hydrogen evolution kinetics on a high-carbon steel and on tin in seawater10.5006/1.3584879 ↗
58. Predictions of surface electrochemistry of saturated and alkaline NH4Cl solutions interacting with Fe (110) from ab initio calculations10.5006/0411 ↗
59. Oxidation versus salt-film formation: competitive adsorption on a series of metals from first-principles10.1016/j.electacta.2018.02.150 ↗
60. Status of research on environmentally assisted cracking in LWR pressure vessel steels10.1115/1.3265576 ↗
61. Stress corrosion cracking of low-alloy steels in 288 C water
62. Ford · 1987
63. Current topics in corrosion: factors influencing stress corrosion crack growth kinetics10.5006/1.3583125 ↗
64. Strain rate effects in stress corrosion cracking10.5006/1.3585089 ↗
65. Quantitative prediction of environmentally assisted cracking10.5006/1.3292125 ↗
66. An alternative to the Shoji crack tip strain rate equation10.1016/j.corsci.2008.07.011 ↗
67. Film rupture model for aqueous stress corrosion cracking under constant and variable stress intensity factor10.1016/j.corsci.2008.08.052 ↗
68. A new parameter for characterizing corrosion fatigue crack growth10.1115/1.3225020 ↗
69. Formulating stress corrosion cracking growth rates by combination of crack tip mechanics and crack tip oxidation kinetics10.1016/j.corsci.2009.10.041 ↗
70. Evaluation of the Fracture Research Institute theoretical stress corrosion cracking model
71. The effect of isothermal heat treatment on hydrogen environment-assisted cracking susceptibility in Monel K-50010.1016/j.msea.2019.138249 ↗
72. Singular behaviour at the end of a tensile crack in a hardening material10.1016/0022-5096(68)90014-8 ↗
73. Accelerated test for evaluation of intergranular stress corrosion cracking initiation characteristics of non-sensitized 316 austenitic stainless steel in simulated pressure water reactor environment10.1016/j.corsci.2016.11.019 ↗
74. Refilming kinetics of scraped steel electrodes in simulated corrosion fatigue crack-tip environments10.1016/0010-938X(89)90046-2 ↗