journal article·1993-01

Stage I stress corrosion cracking behavior

R.H. Jones, E.P. Simonen

Publisher page

Abstract

No abstract is available for this record. The assistant can identify its topic from the title, but cannot infer the study’s results.

Source: Not provided · Quality: missing

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Welding Techniques and Residual Stresses

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (26)

Show source-provided references
1. Danielson · Corrosion Science · 1991 · 32 · 110.1016/0010-938X(91)90060-3 ↗
2. Corrosion of nickel-base alloys10.1007/BF02833343 ↗
3. Ford · 1984 · 117
4. Speidel · 1982 · 1
5. Newman · Metall. Trans. A · 1982 · 13 · 201510.1007/BF02645947 ↗
6. Chung · 1984
7. Speidel · 1985 · 443
8. Singbeil · Metall. Trans. A · 1982 · 13 · 109110.1007/BF02643407 ↗
9. Lee · 1979 · 232
10. Jones · Metall. Trans. A · 1989 · 20 · 63710.1007/BF02667582 ↗
11. Jones · Corrosion · 1989 · 45 · 49410.5006/1.3582049 ↗
12. Jones · Corrosion · 1991 · 47 · 54210.5006/1.3585291 ↗
13. Stress corrosion cracking threshold testing—Scc growth behavior of alloy X-750 and type 304 stainless steel under slow rising load
14. Jones · Acta Metall. Mater. · 1990 · 38 · 170310.1016/0956-7151(90)90013-7 ↗
15. Hydrogen-induced crack growth in a Ni-base superalloy10.1016/0036-9748(80)90099-X ↗
16. Andresen · Mater. Sci. Eng. · 1988 · A103 · 16710.1016/0025-5416(88)90564-2 ↗
17. Ford · 1982
18. Newman · Corrosion Sci. · 1981 · 21 · 48710.1016/0010-938X(81)90078-0 ↗
19. Vermilyea · 1973 · 208
20. Macdonald · Corrosion Sci. · 1991 · 32 · 5110.1016/0010-938X(91)90063-U ↗
21. Freiman · J. Geophys. Res. · 1984 · 89 · 407210.1029/JB089iB06p04072 ↗
22. Tester · J. Electrochem. Soc. · 1978 · 122 · 143810.1149/1.2134039 ↗
23. Transport properties of salt firms on nickel in 0.5N HCl10.1149/1.2095974 ↗
24. Elastic-plastic analysis of growing cracks
25. Quasi-static steady crack growth in small-scale yielding
26. Jones · 1986 · 41