Abstract

In this paper, according to the nuclear pressure steel A508-III, the effect of strength mis-matching on the fracture behavior was analyzed by fracture mechanics test and the crack tip stress field of three-point bend specimen was analyzed by using finite element analysis method (FEM). The fracture of heat-affected zone (HAZ) was emphasized especially. The results of FEM show that if the under-matching weld was used, the opening stress and stress triaxiality in the vicinity of crack tip would increase for weld-crack specimen, and would reduce for HAZ-crack specimen. This tendency was confirmed by the test results.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Fatigue and fracture mechanics · Metal Forming Simulation Techniques · Metallurgy and Material Forming

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (9)

Show source-provided references
1. Minami · J. Soc. Naval Architects Jpn. · 1997 · 182 · 64710.2534/jjasnaoe1968.1997.182_647 ↗
2. Minami · 1996
3. F. Minami, S. Hada, Analysis of strength mis-matching of fracture performance of welded joints, IIW Doc. X-1254-92.
4. Tang · 1994
5. Huo · 2000
6. Shan · Int. Fract. Mech. · 1992 · 41 · 62510.1016/0013-7944(92)90149-9 ↗
7. Chen · Int. Fract. Mech. · 1992 · 42 · 29910.1016/0013-7944(92)90220-9 ↗
8. BS7448: Part 2, British Standard Fracture Mechanics Toughness Tests, Method for determination of KIC, critical CTOD and critical J values of welds in metallic materials, 1997.
9. Sato · 1988