The annular brittle cracking in notched samples of an HSLA-100 steel has been studied by crack interrupts. The average crack growth rate was found to be geometry and strain rate dependent. Suitable normalisation led to a generalised expression for crack growth rates that was strain rate and geometry independent. The crack growth rates were found to be directly proportional to a ‘critical product’ namely {KIcrack-tip·CHcrack-tip}. The crack initiation threshold for notched specimens showed an inverse exponential relationship with the notch tip hydrogen concentration. The crack tip hydrogen concentration was best represented by a hydrostatic stress equilibrated concentration for shallow notched specimens. Hydrogen deficiency in deep notches necessitated the use of a ‘frozen-in’ concentration approach for determining the crack tip hydrogen.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Nuclear Materials and Properties · High Temperature Alloys and Creep
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (39)
Show source-provided references
1. Beachem · Metall. Trans. · 1972 · 3 · 43710.1007/BF02642048 ↗
2. Tabata · Scripta Metall. · 1983 · 17 · 94710.1016/0036-9748(83)90268-5 ↗
3. Bond · Acta Metall. · 1987 · 35 · 228910.1016/0001-6160(87)90076-9 ↗
4. Troiano · Trans. Am. Soc. Metals · 1962 · 52 · 54
5. Hancock · Trans. Metal. Soc. AIME · 1966 · 236 · 513
6. Oriani · Acta Metall. · 1974 · 22 · 106510.1016/0001-6160(74)90061-3 ↗
7. Oriani · Metall. Trans. · 1980 · 11A · 180910.1007/BF02655096 ↗
8. Thomas · Mater. Sci. Eng. · 1992 · A159 · 20510.1016/0921-5093(92)90291-8 ↗
9. Esakul · Scripta Metall. · 1983 · 17 · 107910.1016/0036-9748(83)90457-X ↗
10. Dietzel · 1996 · 303
11. Piascik · 1996 · 409
12. Gerberich · 1996 · 539
13. Altstetter · 1996 · 599
14. Lopez · Metall. Trans. · 1996 · 27A · 360110.1007/BF02595451 ↗
15. Huang · Metall. Trans. · 1995 · 26A · 107910.1007/BF02670603 ↗
16. Moody · 1990 · 625
17. Yamaguchi · Corrosion · 1997 · 53 · 14710.5006/1.3280452 ↗
18. Krom · J. Mech. Phys. Solids · 1999 · 47 · 97110.1016/S0022-5096(98)00064-7 ↗
19. Sofronis · J. Mech. Phys. Solids · 1989 · 37 · 31710.1016/0022-5096(89)90002-1 ↗
20. Munn · Corrosion · 1990 · 46 · 28610.5006/1.3585104 ↗
21. Toribio · J. Mater. Sci. · 1993 · 28 · 228910.1007/BF01151655 ↗
22. Toribio · Corros. Sci. · 1992 · 33 · 138710.1016/0010-938X(92)90179-7 ↗
23. Kwon · Acta Metall. Mater. · 1990 · 38 · 159510.1016/0956-7151(90)90127-3 ↗
24. Brass · Corros. Sci. · 1996 · 38 · 56910.1016/0010-938X(95)00146-B ↗
25. Maier · Acta Metall. · 1987 · 35 · 87510.1016/0001-6160(87)90164-7 ↗
26. Sofronis · Acta Mater. · 1998 · 46 · 151910.1016/S1359-6454(97)00364-9 ↗
27. Devanathan · Proc. Roy. Soc. · 1962 · A270 · 9010.1098/rspa.1962.0205 ↗
28. Tada · 1985 · 27.1
29. Turnbull · Corros. Sci. · 1989 · 29 · 8910.1016/0010-938X(89)90082-6 ↗
30. Pound · Acta Mater. · 1998 · 46 · 573310.1016/S1359-6454(98)00247-X ↗
31. Crank · 1967 · 62
32. Bockris · Acta Metall. · 1971 · 19 · 120910.1016/0001-6160(71)90054-X ↗
33. Hirth · Metall. Trans. · 1980 · 11A · 86110.1007/BF02654700 ↗
34. Thompson · Metall. Trans. · 1979 · 10A · 119310.1007/BF02811666 ↗
35. Tien · Metall. Trans. · 1976 · 7A · 82110.1007/BF02644079 ↗
36. Nair · Metall. Trans. · 1983 · 14A · 38510.1007/BF02644216 ↗
37. Johnson · Metall. Trans. · 1976 · 7A · 154310.1007/BF02656397 ↗
38. Hashimoto · Metall. Trans. · 1988 · 19A · 279910.1007/BF02645814 ↗
39. Lecoester · Mater. Sci. Eng. · 1992 · A262 · 205