Oxidation of two-phase Cu–50 Cr alloy at low oxygen pressure
Source abstract
Abstract
Abstract Oxidation behaviour of a cast two-phase Cu–50 Cr alloy and a nano-crystalline two-phase Cu–50 Cr alloy coating were studied at 1073 K at an oxygen partial pressure of 10 −8 Pa. Microstructural observations clearly showed that at the initial oxidation stage, discrete Cr 2 O 3 scales were formed only on the β-phase (Cr) areas of the cast Cu–50 Cr alloy, however, surface diffusion of Cr would assist the lateral growth of these discrete Cr 2 O 3 scales from the β-phase regions, a continuous Cr 2 O 3 scale could be developed to cover the whole sample surface if the oxidation time is long enough (the Cr content should also be high enough). Formation and growth of oxide scales on the nano-crystalline two-phase Cu–50 Cr alloy coating were quite different. A continuous Cr 2 O 3 scale could form and cover the whole surface after only 15 min oxidation, indicating that a phase grain size reduction could promote the formation of a protective scale on the surface through enhanced diffusion along grain boundaries and shortened lateral surface diffusion distance. Based on these morphological results, a physical model describing the role of Cr surface diffusion in the scaling behaviour of two-phase alloys was proposed.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Advanced materials and composites · Nuclear Materials and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (27)
Show source-provided references
1. Meier · Mater. Sci. Eng. · 1989 · A120 · 110.1016/0921-5093(89)90712-0 ↗
2. Wagner · Z. Elektrochem. · 1959 · 63 · 772
3. Wagner · J. Electrochem. Soc. · 1952 · 10 · 36910.1149/1.2779605 ↗
4. Gesmundo · Oxid. Met. · 1993 · 40 · 37310.1007/BF00664498 ↗
5. Gesmundo · Oxid. Met. · 1994 · 43 · 37910.1007/BF01047037 ↗
6. Gesmundo · Oxid. Met. · 1994 · 42 · 40910.1007/BF01046758 ↗
7. Gesmundo · Oxid. Met. · 1994 · 42 · 46510.1007/BF01046761 ↗
8. Fu · Corros. Sci. · 2003 · 45 · 55910.1016/S0010-938X(02)00141-5 ↗
9. Niu · Oxid. Met. · 1997 · 48 · 35710.1007/BF02153456 ↗
10. Gesmundo · Oxid. Met. · 1998 · 49 · 14710.1023/A:1018809819937 ↗
11. Chiang · Surf. Coat. Technol. · 1996 · 78 · 24310.1016/0257-8972(95)02421-2 ↗
12. Li · Mater. Sci. Eng. · 2001 · A315 · 24510.1016/S0921-5093(01)01187-X ↗
13. Niu · Corros. Sci. · 2000 · 42 · 16510.1016/S0010-938X(99)00051-7 ↗
14. Niu · Corros. Sci. · 2000 · 42 · 79910.1016/S0010-938X(99)00115-8 ↗
15. Niu · J. Alloys Compd. · 2001 · 317–318 · 57310.1016/S0925-8388(00)01390-6 ↗
16. Liu · Acta Metall. Mater. · 1998 · 46 · 169110.1016/S1359-6454(97)00346-7 ↗
17. He · Mater. Sci. Eng. · 2002 · A334 · 17910.1016/S0921-5093(01)01805-6 ↗
18. Li · Scripta Mater. · 2001 · 45 · 109910.1016/S1359-6462(01)01146-0 ↗
19. Gao · Adv. Mater. · 2001 · 13 · 100110.1002/1521-4095(200107)13:12/13<1001::AID-ADMA1001>3.0.CO;2-V ↗
20. Gao · Mater. Sci. Forum · 2001 · 369–372 · 57910.4028/www.scientific.net/MSF.369-372.579 ↗
21. Y.D. He, H.Y. Yao, Z.W. Li, H.B. Qi, Chinese Patent, 98101027.X (1998).
22. Li · Oxid. Met. · 2000 · 54 · 4710.1023/A:1004646511882 ↗
23. Li · Oxid. Met. · 2000 · 53 · 57710.1023/A:1004641328140 ↗
24. Gao · Intermetallics · 2002 · 10 · 26310.1016/S0966-9795(01)00132-7 ↗
25. Li · High Temp. Mater. Processes · 2002 · 21 · 3510.1515/HTMP.2002.21.1-2.35 ↗
26. He · Oxid. Met. · 2000 · 53 · 32310.1023/A:1004593204901 ↗
27. Kofstad · 1988