A degradation mode of a carbon steel during thermal cycling under a simulated combustion environment
Source abstract
Abstract
The degradation of A210C carbon steel has been investigated at 560 °C under a simulated coal-firing combustion environment. The simulation was performed by direct introduction into the chamber of flue gas from a freeboard of a coal-fired fluidized-bed combustor (FBC) and meanwhile by covering part of samples using ash deposits collected from the FBC freeboard wall. It shows that oxidation is significantly increased, when the steel is covered with ash deposits. During thermal cycling, the accelerated metal recession in the presence of deposits can be interpreted using a proposed degradation mode, which follows a sequence of scale wrinkling, buckling, and finally spalling. The effect of ash deposits on the steel degradation is also discussed.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metallurgical Processes and Thermodynamics · High-Temperature Coating Behaviors · High-Velocity Impact and Material Behavior
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (17)
Show source-provided references
1. E.A. Rogers, J.C. Holder, A.J. Minchener, A.J. Page, R.D. Lanauze, G.G. Thurlow, Materials problems in fluidized-bed combustion systems, May 1980, EPRI report No. CS-1449.
2. Stringer · J. Mater. Energy Sys. · 1986 · 8 · 31910.1007/BF02833595 ↗
3. A.J. Minchener, A.V. Levy, in: Proc. Conf. on Corrosion–Erosion–Wear of Materials at Elevated Temperature. NACE, Houston, TX, 1987, p. 152.
4. K. Nakagawa, in: Proc. High Temp. Corros. (III), Les Embiez, France, May 1992, J. De Physique. 4 (colloque C9) (1993) 787.
5. Bakker · J. Mat. Perf. · 1985 · 1 · 9
6. Natesan · Corrosion · 1985 · 41 · 65510.5006/1.3582999 ↗
7. H.J. Grabke, Meadowcroft (Eds.), Guideline for Methods of Testing and Research in High-Temperature Corrosion. European Federation of Corrosion Publication Number 14, Institute of Materials, 1995.
8. Stott · Mat. High Temp. · 1997 · 14 · 4310.1080/09603409.1997.11689535 ↗
9. Nicholls · Mat. High Temp. · 1997 · 14 · 21910.1080/09603409.1997.11689555 ↗
10. Liu · Corrosion · 2000 · 56 · 29810.5006/1.3287658 ↗
11. X. Peng, K.L. Liu, P. Hack, W.P. Pan, J.T. Riley, D.L. Reuss (Eds.), Technical Meeting of Central States Section on Combustion Fundaments and Applications. Indianapolis, Indiana, USA, April 16–18, 2000, p. 80.
12. Suo · Mech. Phys. Solids · 1995 · 43 · 82910.1016/0022-5096(95)00014-A ↗
13. Golightly · Oxid. Met. · 1976 · 10 · 16310.1007/BF00612158 ↗
14. Rhines · Metall. Trans. · 1970 · 1 · 170110.1007/BF02642020 ↗
15. Tolpygo · Acta Mater. · 1998 · 46 · 516710.1016/S1359-6454(98)00134-7 ↗
16. Wang · Acta Mater. · 1999 · 47 · 69910.1016/S1359-6454(98)00328-0 ↗
17. Evans · Internal Mat. Rev. · 1995 · 40 · 110.1179/imr.1995.40.1.1 ↗