Effect of addition of V and C on strain recovery characteristics in Fe–Mn–Si alloy
Source abstract
Abstract
Abstract Shape recoverable strain, recovery stress and low-temperature stress relaxation characteristics in an Fe–17Mn–5Si–10Cr–4Ni (0.08C) alloy and an Fe–17Mn–2Cr–5Si–2Ni–1V (0.23C) alloy have been studied by means of X-ray diffraction, transmission electron microscopy and measurement of recoverable strain and recovery stress. The amount of stress-induced ɛ martensite under tensile deformation at room temperature, recoverable strain and recovery stress are increased obviously with addition V and C in Fe–Mn–Si alloy, which is owing to the influence of addition V and C on strengthening austenitic matrix. Addition of V and C in Fe–Mn–Si alloy is evidently effective to reduce the degree of low-temperature stress relaxation, for the dispersed VC particles 50–180 nm in size precipitated during annealing restrain the stress induced martensitic transformation.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Microstructure and Mechanical Properties of Steels · Metal Alloys Wear and Properties · Metallurgy and Material Forming
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (6)
Show source-provided references
1. Kajiwara · Mater. Sci. Eng. A · 1999 · 273–275 · 6710.1016/S0921-5093(99)00290-7 ↗
2. Lin · Acta Metall. SINICA · 2002 · 38 · 825
3. Tszaki · Trans. Mater. Soc. Jpn. · 1994 · 18B · 961
4. Baruj · J. De Phys. IV: JP · 2003 · 112I · 37310.1051/jp4:2003904 ↗
5. Susan · Mater. Trans. · 2005 · 45 · 930
6. Wen · Science Forum · 2002 · 394–395 · 41910.4028/www.scientific.net/MSF.394-395.419 ↗