Creep strength degradation of ASME P23/T23 steels
Source abstract
Abstract
Abstract Creep behavior of ASME P23/T23 steels was investigated and analyzed, focusing on creep strength degradation in the long-term. Creep rupture strength at 898 and 923 K dropped in the long-term in both P23 and T23 steels. The stress exponent of minimum creep rate at 898 and 923 K was 7.8–13 for higher stresses and 3.9–5.3 for lower stresses in the P23/T23 steels. The change of stress exponent with stress levels was consistent with the drop in creep rupture strength in the long-term. The Monkman–Grant rule was confirmed in the range examined in P23 steel, while the data points deviated from the rule in the long-term in the case of T23 steel. The creep ductility of P23 steel was high over a wide stress and temperature range. On the other hand, in T23 steel, creep ductility at 898 and 923 K decreased as time to rupture increased, and then recovered again in the long-term. Fracture mode changed from transgranular to intergranular fracture in the long-term at 898 and 923 K. At 923 K, the rapid tertiary creep was observed under lower stresses in T23 steel, comparing with P23 steel.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: High Temperature Alloys and Creep · Nuclear Materials and Properties · Fatigue and fracture mechanics
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (21)
Show source-provided references
1. Masuyama · ISIJ Int. · 2001 · 41 · 61210.2355/isijinternational.41.612 ↗
2. Masuyama · Proc. Mater. Adv. Power Eng.: Part I · 1994 · 173
3. K. Kimura, Proceedings of the 2005 ASME Pressure Vessels and Piping Division Conference, 2005, PVP2005-71039.
4. K. Kimura, Proceedings of the 2006 ASME Pressure Vessels and Piping Division Conference, 2006, PVP2006-ICPVT11-93294.
5. Thermal Power Standard Code, Ministry of Economy, Trade and Industry (METI), Japanese Government, Tokyo, December 14, 2005.
6. Thermal Power Standard Code, Ministry of Economy, Trade and Industry (METI), Japanese Government, Tokyo, July 10, 2007.
7. Yoshizawa · CAMP-ISIJ · 2005 · 18 · 1549
8. Nakashiro · J. Soc. Mat. Sci. Jpn. · 1994 · 43 · 20310.2472/jsms.43.203 ↗
9. Viswanathan · Trans. ASME, J. Pressure Vessel Tech. · 1998 · 120 · 10510.1115/1.2842227 ↗
10. Kushima · Tetsu-to-Hagane · 1999 · 85 · 84110.2355/tetsutohagane1955.85.11_841 ↗
11. Kimura · Proc. Life Manage Maintenance Power Plants · 2004 · 2 · 465
12. K. Kimura, K. Sawada, K. Kubo, H. Kushima, Proceedings of the 2004 ASME/JSME Pressure Vessel and Piping Conference, 2004, PVP2004-2566.
13. Komai · Proc. 8th Liege Conf. Mater. Adv. Power Eng.: Part II · 2006 · 997
14. NIMS Creep Data Sheet, No. 54, National Institute for Materials Science, Tsukuba, Japan, 2008.
15. Iseda · Tetsu-to-Hagane · 1990 · 76 · 107610.2355/tetsutohagane1955.76.7_1076 ↗
16. Maruyama · J. Jpn. Inst. Metals · 1991 · 55 · 118910.2320/jinstmet1952.55.11_1189 ↗
17. Cadek · 1998
18. Pickering · 1978
19. Monkman · Proc. ASTM · 1956 · 56 · 595
20. Kushima · Proceedings of the 7th JIM International Symposium Aspects of High Temperature Deformation and Fracture in Crystalline Materials · 1993 · 609
21. Lee · Mater. Sci. Eng. A · 2006 · 428 · 27010.1016/j.msea.2006.05.010 ↗