Abstract The vacuum degassing behavior of Zr 55 Al 10 Ni 5 Cu 30 , Ni 59 Zr 15 Ti 13 Si 3 Sn 2 Nb 7 Al 1 , and Cu 54 Ni 6 Zr 22 Ti 18 (numbers indicate at.%) metallic glass powders has been investigated and compared with that of Al alloy powder. It was found that the alloy composition influenced the gas desorption behavior with heating in vacuo . Zr 55 Al 10 Ni 5 Cu 30 and Ni 59 Zr 15 Ti 13 Si 3 Sn 2 Nb 7 Al 1 metallic glass powders exhibited little H 2 gas desorption from powder surfaces during vacuum degassing. Because Zr in the Zr-based and Ni-based amorphous alloy powders produced a native zirconium oxide layer, the surface of the Zr 55 Al 10 Ni 5 Cu 30 and Ni 59 Zr 15 Ti 13 Si 3 Sn 2 Nb 7 Al 1 amorphous alloys had no influence on adsorbed H 2 O. Cu 54 Ni 6 Zr 22 Ti 18 metallic glass powder was the most affected by atmospheric H 2 O among the metallic glass powders examined in this study. The adsorbed H 2 O and Cu metal may react with each other with the formation of Cu 2 O and liberation of H 2 during vacuum degassing. In order to obtain sound P/M final products with Cu-based P/M alloys, oxygen-free copper powders should be used in well-controlled atmospheres with low H 2 O partial pressures.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metallic Glasses and Amorphous Alloys · Glass properties and applications · Phase-change materials and chalcogenides
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (22)
Show source-provided references
1. Nishiyama · Mater. Trans. JIM · 1997 · 38 · 46410.2320/matertrans1989.38.464 ↗
2. Inoue · Mater. Trans. JIM · 1993 · 34 · 35110.2320/matertrans1989.34.351 ↗
3. Inoue · Mater. Trans. JIM · 1991 · 32 · 60910.2320/matertrans1989.32.609 ↗
4. Inoue · Acta Mater. · 2001 · 29 · 264510.1016/S1359-6454(01)00181-1 ↗
5. Lin · J. Appl. Phys. · 1995 · 78 · 651410.1063/1.360537 ↗
6. Zhang · Mater. Trans. JIM · 1991 · 32 · 100510.2320/matertrans1989.32.1005 ↗
7. Peker · Appl. Phys. Lett. · 1993 · 63 · 234210.1063/1.110520 ↗
8. Lu · Acta Mater. · 2002 · 50 · 350110.1016/S1359-6454(02)00166-0 ↗
9. Nishi · Phys. Rev. B · 2004 · 70 · 17420410.1103/PhysRevB.70.174204 ↗
10. Yamasaki · Appl. Phys. Lett. · 2004 · 84 · 465310.1063/1.1759768 ↗
11. Yamasaki · Scr. Mater. · 2005 · 53 · 6310.1016/j.scriptamat.2005.03.021 ↗
12. Yamasaki · Mater. Trans. · 2004 · 45 · 133510.2320/matertrans.45.1335 ↗
13. Yamasaki · Mater. Trans. · 2006 · 47 · 190210.2320/matertrans.47.1902 ↗
14. Lee · Mater. Sci. Forum · 2005 · 475–479 · 341910.4028/www.scientific.net/MSF.475-479.3419 ↗
15. Kawamura · Scr. Metall. · 1993 · 29 · 2510.1016/0956-716X(93)90248-Q ↗
16. Kai · Intermetallics · 2002 · 10 · 126510.1016/S0966-9795(02)00163-2 ↗
17. Hsieh · Intermetallics · 2004 · 12 · 108910.1016/j.intermet.2004.04.024 ↗
18. Jayaraj · Corros. Sci. · 2006 · 48 · 95010.1016/j.corsci.2005.04.006 ↗
19. Asami · Corros. Sci. · 1997 · 39 · 9510.1016/S0010-938X(96)00108-4 ↗
20. Sato · J. Am. Ceram. Soc. · 1985 · 68 · 35610.1111/j.1151-2916.1985.tb15239.x ↗
21. Sato · J. Am. Ceram. Soc. · 1985 · 68 · c32010.1111/j.1151-2916.1985.tb15233.x ↗
22. Carter · Eng. Fail. Anal. · 2001 · 8 · 11310.1016/S1350-6307(99)00040-0 ↗