Abstract
The cyclic oxidation and acoustic emission (AE) tests were carried out for studying cracking behavior of oxide scales formed on Ti3SiC2-based ceramic at 1100 degreesC. A duplex oxide scale with an outer layer of pure TiO2 and an inner layer of a mixture of TiO2 and SiO2 was formed. The oxide scale did not spall from substrate during the cyclic oxidation at 1100 degreesC for 360 times. However, a great number of micro-cracks penetrating whole inner oxide layer were detected. AE test showed that the oxide scale did not crack during the isothermal oxidation at 1100 degreesC for 1 h, however, the scale cracked during the cooling stage. Comparing the growth rate and thickness between the oxide layers formed during the isothermal oxidation and cyclic oxidation, respectively, indicated that cracks in the inner oxide layer served as paths mainly for outward diffusion of titanium and for inward diffusion of oxygen, resulting in increased growth rate of the outer oxide layer. Because of entire and compact TiO2 consisted of outer oxide layer, and low thermal stress resulting from small mismatch of thermal expansion coefficients between the oxides and the substrate, Ti3SiC2 exhibited excellent cyclic oxidation resistance at 1100 degreesC for 360 cycles. (C) 2003 Elsevier B.V. All rights reserved.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: MXene and MAX Phase Materials · Advanced ceramic materials synthesis · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (20)
Show source-provided references
1. Barsoum · J. Am. Ceram. Soc. · 1996 · 79 · 195310.1111/j.1151-2916.1996.tb08018.x ↗
2. Sun · Phil. Mag. Lett. · 2000 · 80 · 28910.1080/095008300176056 ↗
3. Barsoum · J. Electrochem. Soc. · 1997 · 144 · 250810.1149/1.1837846 ↗
4. Racault · J. Mater. Sci. · 1994 · 29 · 338410.1007/BF00352037 ↗
5. Tong · J. Mater. Sci. · 1995 · 30 · 308710.1007/BF01209221 ↗
6. Feng · J. Mater. Res. · 1999 · 14 · 92510.1557/JMR.1999.0124 ↗
7. Radhakrishnan · J. Alloys Compd. · 1999 · 286 · 8510.1016/S0925-8388(99)00003-1 ↗
8. Sun · Corros. Sci. · 2001 · 43 · 109510.1016/S0010-938X(00)00142-6 ↗
9. Sun · Acta Mater. · 2001 · 49 · 434710.1016/S1359-6454(01)00247-6 ↗
10. Zhou · Mater. Res. Innovat. · 1998 · 2 · 14210.1007/s100190050076 ↗
11. Monceau · Oxid. Met. · 1998 · 50 · 44710.1023/A:1018860909826 ↗
12. Pieraggi · J. Electrochem. Soc. · 1993 · 140 · 284410.1149/1.2220920 ↗
13. Sun · Oxid. Met. · 2002 · 57 · 37910.1023/A:1015363119164 ↗
14. Barsoum · J. Phys. Chem. Solids · 1999 · 60 · 42910.1016/S0022-3697(98)00313-8 ↗
15. W.D. Kingery, H.K. Bowen, D.R. Uhlmann, Introduction to Ceramics, 2nd ed., Thermal Properties, Wiley, New York, 1975, pp. 594–595 (Chapter 12).
16. Turner · J. Res. Natl. Bur. Stand. · 1946 · 37 · 23910.6028/jres.037.015 ↗
17. Birks · 1983
18. Liu · Mater. Res. Innovat. · 2002 · 6 · 22610.1007/s10019-002-0201-7 ↗
19. Christensen · Acta Mater. · 1997 · 45 · 176110.1016/S1359-6454(96)00258-3 ↗
20. Birnie · Corros. Sci. · 1992 · 33 · 110.1016/0010-938X(92)90014-T ↗