Microstructural study of the initiation and formation of immersion tin coating on copper
Source abstract
Abstract
The initiation and growth of immersion tin coating from hydrochloric acid based and methanesulphonic acid based baths on the inner surface of copper tube was studied by transmission electron microscopy (TEM) and scanning electron microscopy (SEM). The formation of immersion tin coating crystallites from hydrochloric acid based bath occurs semi-coherently with copper substrate. Tin crystallites grow actively both in vertical and horizontal directions yielding an equiaxial grain structure. The immersion tin deposition from methanesulphonic acid based bath proceeds by the formation of tin nanocrystals. These nanocrystals transform into columnar grains during the grain growth process. Differences in the coating formation characteristics between studied baths are reflected to the microstructural details and properties of coatings, such as surface morphology, porosity and adhesion.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · Copper Interconnects and Reliability · Corrosion Behavior and Inhibition
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (17)
Show source-provided references
1. 1993
2. United States Environmental Protecting Agency, Maximum Contaminant Levels Goals and National Primary Drinking Water Regulation for Lead and Copper, USA Federal Register, 1991, p. 26460.
3. The Council of European Union, Council Directive 98/83/EC, Official Journal. L 330 (1998) 32–54.
4. Pourbaix · 1966
5. Sidky · British Corrosion Journal · 1999 · 34 · 17110.1179/000705999101500815 ↗
6. Williams · 1996
7. Joint Committee of Powder Diffraction Standards, Card 4-673.
8. Edington · 1976
9. Barrett · 1966
10. Sard · Journal of the Electrochemical Society · 1970 · 117 · 86410.1149/1.2407658 ↗
11. Keränen · Surface and Coating Technology · 1996 · 82 · 2910.1016/0257-8972(95)02539-1 ↗
12. Edington · 1975
13. Wu · Transactions of the Institute of Metal Finishing · 1998 · 76 · 10810.1080/00202967.1998.11871206 ↗
14. Nakahara · Acta Metallurgica · 1983 · 31 · 71310.1016/0001-6160(83)90086-X ↗
15. Weil · Plating and Surface Finishing · 1997 · 84 · 28
16. Barker · Surface Technology · 1981 · 12 · 7710.1016/0376-4583(81)90138-2 ↗
17. Iacovangelo · Journal of the Electrochemical Society · 1991 · 138 · 97610.1149/1.2085756 ↗