journal article·2004-01

High temperature oxidation behaviour of Fe–Al–C alloys: an overview

V.Shankar Rao

Materials Science and Engineering: A· Volume 364· Issue 1-2
Publisher page

Abstract

Abstract Carbide containing dual phase iron aluminide offers two-fold benefits; it posses high temperature strength and high resistance to probability of hydrogen embrittlement compared to single-phase iron aluminide. In this paper, we summarise the recent developments related to the oxidation behaviour of Fe–Al–C alloys. Emphasis is placed on the each variables of the system C, Al and temperature, and tried to differentiate the oxidation behaviour between Fe 3 Al/α and Fe 3 AlC phases while reviewing the oxidation resistance of Fe–Al–C alloys.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Intermetallics and Advanced Alloy Properties · High-Temperature Coating Behaviors · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (33)

Show source-provided references
1. Stoloff · Mater. Sci. Eng. A · 1998 · 258 · 110.1016/S0921-5093(98)00909-5 ↗
2. C.T. Liu, J.O. Stiegler, F.H. Fores, Ordered intermetallics, in: Metals Handbook ASM, vol. 2, Metals Park, OH, 1990, p. 913.10.31399/asm.hb.v02.a0001102 ↗
3. McKamey · J. Mater. Res. · 1991 · 6 · 177910.1557/JMR.1991.1779 ↗
4. Baligidad · ISIJ, Int. · 1996 · 36 · 145310.2355/isijinternational.36.1453 ↗
5. Baligidad · Scripta Metall. · 1997 · 36 · 66710.1016/S1359-6462(96)00441-1 ↗
6. Baligidad · Mater. Sci. Eng. · 1999 · A265 · 30110.1016/S0921-5093(98)01146-0 ↗
7. Baligidad · Mater. Sci. Eng. · 2000 · A283 · 21110.1016/S0921-5093(99)00796-0 ↗
8. Shankar Rao · Corros. Sci. · 2002 · 44 · 52110.1016/S0010-938X(01)00084-1 ↗
9. Sen · Scripta Mater. · 2001 · 44 · 61910.1016/S1359-6462(00)00602-3 ↗
10. Parvathavarthini · Intermetallics · 2002 · 10 · 32910.1016/S0966-9795(01)00140-6 ↗
11. V. Shankar Rao, V.S. Raja, R.G. Baligidad, R. Raman, Corros. Eng. Sci. Tech. 38 (2003) October issue, in press.
12. Kolluru · Mater. Sci. Eng. A · 2002 · 328 · 5810.1016/S0921-5093(01)01667-7 ↗
13. Pang · Intermetallics · 2000 · 8 · 69310.1016/S0966-9795(99)00145-4 ↗
14. Radhakrishna · Scripta Metall. · 2001 · 45 · 107710.1016/S1359-6462(01)01142-3 ↗
15. Shankar Rao · Intermetallics · 2002 · 10 · 7310.1016/S0966-9795(01)00106-6 ↗
16. Shankar Rao · Oxid. Met. · 2002 · 57 · 44910.1023/A:1015348320981 ↗
17. Tortorelli · Mater. Sci. Eng. · 1998 · A258 · 11510.1016/S0921-5093(98)00924-1 ↗
18. Banovi · Oxid. Met. · 2000 · 54 · 33910.1023/A:1004658530596 ↗
19. Prescott · Oxid. Met. · 1992 · 38 · 7310.1007/BF00665045 ↗
20. Gesmundo · Oxid. Met. · 1995 · 44 · 21110.1007/BF01046728 ↗
21. Caplan · Oxid. Met. · 1979 · 13 · 25510.1007/BF00603670 ↗
22. Boggs · J. Electrochem. Soc. · 1971 · 118 · 90610.1149/1.2408222 ↗
23. Kao · J. Mater. Sci. · 1987 · 22 · 320310.1007/BF01161183 ↗
24. Shankar Rao · Corros. Sci. · 2003 · 45 · 271710.1016/S0010-938X(03)00119-7 ↗
25. Shankar Rao · Corrosion · 2003 · 59 · 57510.5006/1.3277588 ↗
26. Xu · Corros. Sci. · 2001 · 43 · 67110.1016/S0010-938X(00)00104-9 ↗
27. Shankar Rao · High Temp. Mater. Process. · 2002 · 21 · 14310.1515/HTMP.2002.21.3.143 ↗
28. Boggs · Oxid. Met. · 1976 · 10 · 27710.1007/BF00618248 ↗
29. Kao · J. Mater. Sci. · 1988 · 23 · 194310.1007/BF01115754 ↗
30. P. Villars, A. Prince, H. Okamoto, Handbook of Ternary Alloy Phase Diagrams, ASM International vol. 3 (1994) p. 2871.
31. Shankar Rao · Intermetallics · 2003 · 11 · 71310.1016/S0966-9795(02)00194-2 ↗
32. Shankar Rao · Intermetallics · 2003 · 11 · 11910.1016/S0966-9795(02)00194-2 ↗
33. Das · Mater. Sci. Eng. A · 2002 · 338 · 2410.1016/S0921-5093(02)00072-2 ↗