Abstract Melt-spun amorphous Fe 73 Si 16 B 7 Nb 3 Cu 1 (numbers indicate at.%) alloy strip was pulverized to make flake-shaped fine powders. The powders were ball-milled to control the powder shape and to mix with polyimide-based binder of 0.5–3 wt.%, followed by cold compaction to form toroid-shaped bonded powder-metallurgical magnets. The powder cores were heat-treated to crystallize the amorphous structure and to control the nano-grain structure. Well-coated polymer binder on the powder surface decreased the coercivity and the core loss with the insulation of each powder. The analyses by differential scanning calorimetry, magnetization cores and transmission electron microscopy revealed that the best magnetic properties of powder cores was obtained after annealing for 1 h at 550–600 °C. The annealing condition to obtain the aimed grain size of 10–20 nm should be optimized considering the stored energy generated during the powder-forming process.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metallic Glasses and Amorphous Alloys · Magnetic Properties of Alloys · Electromagnetic wave absorption materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (7)
Show source-provided references
1. Yoshizawa · J. Appl. Phys. · 1988 · 64 · 604410.1063/1.342149 ↗
2. Petzold · J. Magn. Mag. Mater. · 2002 · 242–245 · 8410.1016/S0304-8853(01)01206-9 ↗
3. Wojcik · J. Magn. Mag. Mater. · 2000 · 215–216 · 50310.1016/S0304-8853(00)00204-3 ↗
4. Derebasi · J. Magn. Mag. Mater. · 2000 · 215–216 · 61110.1016/S0304-8853(00)00240-7 ↗
5. Herzer · IEEE Trans. Magn. · 1989 · 25 · 332710.1109/20.42292 ↗
6. Herzer · IEEE Trans. Magn. · 1990 · 26 · 139710.1109/20.104389 ↗
7. Herzer · 1991 · 130