Abstract
Abstract The structural and hydrogen sorption properties of the ZrNi 5− x Co x ( x =0,1,2 and 3) system have been studied. The alloys were characterized by X-ray diffraction patterns and by pressure-composition-temperature (PCT) diagrams at temperatures ranging from 448 to 523 K. It was found that compositions with 0≤ x ≤2 were solid solutions of AuBe 5 type structure, whereas the ZrNi 2 Co 3 alloy showed a two-phase structure. Substitution of Ni by Co increases the unit cell volume of the monophase alloys by 0.84% per one substituted atom in formula unit. Hydrogen uptake increases the cell volume of the host alloy by up to 2.3%. In the studied conditions of temperature (448 to 523 K) and pressure (0.05 to 2.5 MPa) the PCT diagrams do not exhibit any plateau of hydrogen equilibrium pressure. The hydrogen capacity increases with increasing Co substitution. The largest hydrogen solubility has been found for the ZrNi 2 Co 3 alloy (1.3 hydrogen atoms per formula unit).
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Hydrogen Storage and Materials · Rare-earth and actinide compounds · Magnetic Properties of Alloys
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (22)
Show source-provided references
1. Uchida · Z. Phys. Chem. Neue Folge · 1989 · 164 · 127510.1524/zpch.1989.164.Part_2.1275 ↗
2. Block · J. Alloys Compounds · 1997 · 253–254 · 52910.1016/S0925-8388(96)03070-8 ↗
3. Luo · J. Alloys Compounds · 1995 · 231 · 46710.1016/0925-8388(95)01871-9 ↗
4. Witham · J. Alloys Compounds · 1997 · 253–254 · 57410.1016/S0925-8388(96)02931-3 ↗
5. Rożdżyńska-Kiełbik · J. Alloys Compounds · 2000 · 298 · 23710.1016/S0925-8388(99)00616-7 ↗
6. Takeshita · J. Solid State Chem. · 1978 · 23 · 27110.1016/0022-4596(78)90074-9 ↗
7. Osumi · J. Less-Common Met. · 1979 · 66 · 6710.1016/0022-5088(79)90196-6 ↗
8. Huang · 1979 · 1613
9. Iwasieczko · 1998 · 389
10. Sorgic · J. Alloys Compounds · 1995 · 221 · 16910.1016/0925-8388(94)01421-3 ↗
11. van Mal · J. Less-Common Met. · 1974 · 35 · 6510.1016/0022-5088(74)90146-5 ↗
12. Bernauer · J. Less-Common Met. · 1987 · 131 · 21310.1016/0022-5088(87)90521-2 ↗
13. Bala · J. Appl. Electrochem. · 1993 · 23 · 101710.1007/BF00266123 ↗
14. Matsumoto · J. Less-Common Met. · 1982 · 88 · 44310.1016/0022-5088(82)90255-7 ↗
15. Lee · J. Alloys Compounds · 1999 · 291 · 25410.1016/S0925-8388(99)00262-5 ↗
16. Une · J. Less-Common Met. · 1978 · 57 · 9310.1016/0022-5088(78)90165-0 ↗
17. Fromm · Z. Phys. Chem. Neue Folge · 1986 · 147 · 6110.1524/zpch.1986.147.1_2.061 ↗
18. Efron · J. Less-Common Met. · 1989 · 153 · 2310.1016/0022-5088(89)90529-8 ↗
19. Jacob · Z. Phys. Chem. · 1993 · 181 · 28910.1524/zpch.1993.181.Part_1_2.289 ↗
20. K.N. Semenenko, E.E. Fokina, V.N. Fokin, S.L. Troitskaya, V.V. Burnasheva, Otkrytiya Izobret. Prom. Obraztsy, Tovarnye Znaki, 34 (1982) 102, Russian Patent C01B006–02.
21. Villars · 1985 · 2566
22. Methodes d'essais liees a la fragilisation par l'hydrogene