journal article·2004-09

Geometrical effect of pyramidal indenters on the elastoplastic contact behaviors of ceramics and metals

Junqiu Zhang, Mototsugu Sakai

Materials Science and Engineering: A· Volume 381· Issue 1-2
Publisher page

Abstract

Abstract Depth-sensing indentation measurements were performed using the three trihedral pyramid indenters with the specific inclined face angles β B ( β B =11.4°, 24.7° (Berkovich) and 43.7°), three tetrahedral pyramid indenters with β V ( β V =10°, 22° (Vickers) and 40°) and a Knoop indenter ( β K =25.2°). The materials tested ranged from ductile metals to brittle ceramics, including soda-lime glass, Si 3 N 4 , MgO, copper/zinc alloy, and high-carbon chromium bearing steels. The loading paths were conformed to the quadratic relations of P = k 1 h 2 , and the unloading paths were well approximated with P = k 2 ( h − h r ) 2 , in terms of the indentation load P , penetration depth h , and the residual depth h r of impression. All of the indentation-related parameters were calculated from the loading/unloading P – h hysteresis curves, and then correlated well with the nondimensional plastic strain E ′ tan β C / H (elastic modulus E ′, true hardness H and the inclined face angle β C of equivalent cone indenter). The concept of “equivalent cone” provided an efficient analytical method, by which all of the indentation behaviors for the Vickers-type, Berkovich-type and the Knoop indenters were described in a unified manner. The quadratic approximation for the unloading path combined with the concept of “effective shape of indenter” was successfully utilized to estimate the elastic modulus E ′ of the materials indented.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Metal and Thin Film Mechanics · Advanced ceramic materials synthesis · Advanced Surface Polishing Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (36)

Show source-provided references
1. Sakai · Acta Metall. Mater. · 1993 · 41 · 175110.1016/0956-7151(93)90194-W ↗
2. Oliver · J. Mater. Res. · 1992 · 7 · 156410.1557/JMR.1992.1564 ↗
3. Sakai · J. Mater. Res. · 1999 · 14 · 147110.1557/JMR.1999.0198 ↗
4. Sakai · J. Mater. Res. · 1999 · 14 · 363010.1557/JMR.1999.0490 ↗
5. Sakai · J. Mater. Res. · 2002 · 17 · 216110.1557/JMR.2002.0318 ↗
6. Wilde · Materialprüfung · 2000 · 42 · 468
7. Pharr · MRS Bull. · 1992 · 17 · 2810.1557/S0883769400041634 ↗
8. Sakai · J. Non-Cryst. Solids · 2001 · 282 · 23610.1016/S0022-3093(01)00316-7 ↗
9. Schulze · Int. J. Solids Struct. · 2000 · 37 · 104510.1016/S0020-7683(98)00285-6 ↗
10. Chen · J. Mater. Res. · 2001 · 16 · 297410.1557/JMR.2001.0408 ↗
11. Sanchez · Acta Mater. · 1999 · 47 · 440510.1016/S1359-6454(99)00254-2 ↗
12. Malzbender · Thin Solid Films · 2000 · 372 · 13410.1016/S0040-6090(00)01025-7 ↗
13. Amitay-Sadovsky · Polymer · 1998 · 39 · 238710.1016/S0032-3861(97)00550-8 ↗
14. Mukhopadhyay · J. Eur. Ceram. Soc. · 1990 · 6 · 30310.1016/0955-2219(90)90021-7 ↗
15. Li · J. Am. Ceram. Soc. · 1989 · 72 · 90410.1111/j.1151-2916.1989.tb06242.x ↗
16. Bolse · J. Test Eval. · 1995 · 23 · 2710.1520/JTE10395J ↗
17. Gong · Mater. Lett. · 2002 · 56 · 94110.1016/S0167-577X(02)00641-9 ↗
18. Chen · J. Mater. Res. · 1994 · 9 · 131410.1557/JMR.1994.1314 ↗
19. Rother · Materialwiss Werkstofftechnik · 1995 · 26 · 47710.1002/mawe.19950260904 ↗
20. Rother · J. Mater. Res. · 1998 · 13 · 207110.1557/JMR.1998.0291 ↗
21. Rother · Materialwiss Werkstofftechnik · 1996 · 27 · 48710.1002/mawe.19960271008 ↗
22. JIS standard B-7735, Vickers hardness test—calibration of the reference blocks, Japanese Standard Association, 1997.
23. JIS standard G-4805, High carbon chromium bearing steels, Japanese Standard Association, Tokyo, Japan, 1999.
24. JIS standard H-3100, Copper and copper alloy sheets, plates and strips, Japanese Standard Association, 1992.
25. ISO standard 426-1, Wrought copper–zinc alloys—chemical composition and forms of wrought products—Part 1: non-leaded special copper–zinc alloys, International Standardization Organization, 1983.
26. ISO/DIS standard 683-17, Heat-treated steels, alloy steels and free-cutting steels—Part 17: ball and roller bearing steels, International Standardization Organization, Geneva, Switzerland, 1997.
27. J.L. Loubet, J.M. Georges, G. Meille, in: P.J. Blay, B.R. Lawn (Eds.), Microindentation Techniques in Materials Science and Engineering, ASTM STP889, Philadelphia, PA, 1986, p. 72.10.1520/STP32952S ↗
28. P.J. Blau, The Lab Handbook of Microindentation Hardness Testing, Section 4.1, Blue Rock Technical Publications, Oak Ridge, TN, 2000.
29. Riester · Thin Solid Films · 2000 · 377 · 63510.1016/S0040-6090(00)01298-0 ↗
30. Lawn · J. Mater. Sci. · 1981 · 16 · 274510.1007/BF02402837 ↗
31. Marshall · J. Am. Ceram. Soc. · 1982 · 65 · C17510.1111/j.1151-2916.1982.tb10357.x ↗
32. K.L. Johnson, Contact Mechanics, Chapters 3–6, Cambridge University Press, Cambridge, 1985.10.1017/CBO9781139171731 ↗
33. Sakai · J. Mater. Res. · 2003 · 18 · 208710.1557/JMR.2003.0293 ↗
34. Sakai · J. Mater. Res. · 2003 · 18 · 163110.1557/JMR.2003.0224 ↗
35. Sakai · Acta Mater. · 2004 · 52 · 235910.1016/j.actamat.2004.01.027 ↗
36. Pharr · J. Mater. Res. · 2002 · 17 · 266010.1557/JMR.2002.0386 ↗